Thermally induced sp2 clustering in tetrahedral amorphous carbon (ta-C) films

被引:47
|
作者
Orwa, JO
Andrienko, I
Peng, JL
Prawer, S
Zhang, YB
Lau, SP
机构
[1] Univ Melbourne, Sch Phys, Microanalyt Res Ctr, Parkville, Vic 3010, Australia
[2] Nanyang Technol Univ, Sch Elect & Elect Engn, Singapore 639798, Singapore
关键词
D O I
10.1063/1.1808918
中图分类号
O59 [应用物理学];
学科分类号
摘要
Tetrahedral amorphous carbon films with 70%-88% sp(3) content are studied by atomic force microscopy (AFM), transmission electron microscopy (TEM), and Raman spectroscopy as a function of annealing temperature in the range 25-1100 degreesC. Using a high-resolution AFM current imaging, we directly image the formation and growth of conducting graphitic (sp(2)-bonded) nanoclusters in the ta-C films. Overall results from all the techniques used show that the structural and electronic changes in the films depend sensitively on the initial sp(3) content. Cross-sectional TEM confirms that the clusters appear not only at the surface of the films but in the bulk as well. The growth and, perhaps, the partial orientation of the sp(2)-bonded nanoclusters in the size range of 1-3 nm is accompanied by a large reduction in the film stress, which decreases sharply in the temperature range 500-600 degreesC. (C) 2004 American Institute of Physics.
引用
收藏
页码:6286 / 6297
页数:12
相关论文
共 50 条
  • [21] High temperature tribological behavior of tetrahedral amorphous carbon (ta-C) and fluorinated ta-C coatings against aluminum alloys
    Bhowmick, S.
    Banerji, A.
    Khan, M. Z. U.
    Lukitsch, M. J.
    Alpas, A. T.
    SURFACE & COATINGS TECHNOLOGY, 2015, 284 : 14 - 25
  • [22] Influence of ion energy and substrate temperature on the optical and electronic properties of tetrahedral amorphous carbon (ta-C) films
    Chhowalla, M
    Robertson, J
    Chen, CW
    Silva, SRP
    Davis, CA
    Amaratunga, GAJ
    Milne, WI
    JOURNAL OF APPLIED PHYSICS, 1997, 81 (01) : 139 - 145
  • [23] Effect of test atmosphere on the tribological behaviour of the tetrahedral amorphous carbon (ta-C) and fluorinated ta-C (ta-C-F) coatings against steel
    Khan, M. Z. U.
    Bhowmick, S.
    Lukitsch, M. J.
    Alpas, A. T.
    SURFACE & COATINGS TECHNOLOGY, 2017, 332 : 382 - 390
  • [24] Corrosion behaviour of tetrahedral amorphous carbon (ta-C) filled titania nano tubes
    Mohan, L.
    Viswanathan, S.
    Anandan, C.
    Rajendran, N.
    RSC ADVANCES, 2015, 5 (113): : 93131 - 93138
  • [25] Wear Mechanism of Superhard Tetrahedral Amorphous Carbon (ta-C) Coatings for Biomedical Applications
    Rothammer, Benedict
    Schwendner, Michael
    Bartz, Marcel
    Wartzack, Sandro
    Boehm, Thomas
    Krauss, Sebastian
    Merle, Benoit
    Schroeder, Stefan
    Uhler, Maximilian
    Kretzer, Jan Philippe
    Weihnacht, Volker
    Marian, Max
    ADVANCED MATERIALS INTERFACES, 2023, 10 (07)
  • [26] Strongly adhering and thick highly tetrahedral amorphous carbon (ta-C) thin films via surface modification by implantation
    Chhowalla, M
    Amaratunga, GAJ
    JOURNAL OF MATERIALS RESEARCH, 2001, 16 (01) : 5 - 8
  • [27] XPS and Raman Spectral Analysis of Nitrogenated Tetrahedral Amorphous Carbon (ta-C : N) Films with Different Nitrogen Content
    Chen Wang-shou
    Zhu Jia-qi
    Han Jie-cai
    Tian Gui
    Tan Man-lin
    SPECTROSCOPY AND SPECTRAL ANALYSIS, 2009, 29 (01) : 268 - 272
  • [28] XPS and Raman spectral analysis of nitrogenated tetrahedral amorphous carbon (ta-C:N) films with different nitrogen content
    Chen, Wang-Shou
    Zhu, Jia-Qi
    Han, Jie-Cai
    Tian, Gui
    Tan, Man-Lin
    Guang Pu Xue Yu Guang Pu Fen Xi/Spectroscopy and Spectral Analysis, 2009, 29 (01): : 268 - 272
  • [29] Determination of the sp3/sp2 ratio in tetrahedral amorphous carbon films by effective medium approximation
    Chen, ZY
    Yu, YH
    Zhao, JP
    Wang, X
    Liu, XH
    Shi, TS
    JOURNAL OF APPLIED PHYSICS, 1998, 83 (03) : 1281 - 1285
  • [30] Hydrogen-free tetrahedral carbon (ta-C) films preparation and tribological characterisation
    Tay, BK
    Shi, X
    Flynn, DI
    Sun, Z
    SURFACE MODIFICATION TECHNOLOGIES X, 1997, : 487 - 498