Evaluation of mode III interlaminar fracture toughness of laminated composites

被引:0
|
作者
Ogihara, S. [1 ]
Matsuda, K. [1 ]
机构
[1] Tokyo Univ Sci, Dept Mech Engn, Noda, Chiba 2788510, Japan
关键词
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Mode III interlaminar fracture toughness in CFRP is evaluated experimentally by using the Edge Crack Torsion (ECT) test. A material system used is T700S/2500 carbon/epoxy system. Laminate configuration is [90/(+45/-45)(3)/(-45/+45)(3)/90](s) with a delamination introduced by a 25 mu m-thick kapton film at the mid-plane along one edge. The specimen size is 90mm long, 40mm wide and 4.2mm thick. The film lengths were 0, 5, 10 and 15 mm. A natural crack is produced with a wedge from the film edge. The resulting crack lengths are from 8mm to 18mm. Two data reduction methods are used to calculate mode III interlaminar fracture toughness G(IIIC) at the maximum load and load at onset of nonlinearity. Soft X-ray radiograph is used to observe delamination propagation. Three-dimensional finite element analysis is performed to calculate the distribution of mode I, mode II, and mode III energy release rate along the delamination front. The validity of the experimental method is also discussed.
引用
收藏
页码:355 / +
页数:2
相关论文
共 50 条
  • [31] MODE II INTERLAMINAR FRACTURE TOUGHNESS OF FLAX AND GLASS EPOXY HYBRID COMPOSITES
    Bougherara, Habiba
    Ekeoseye, Wilfred Stephen
    7TH INTERNATIONAL CONFERENCE INTEGRITY-RELIABILITY-FAILURE (IRF2020), 2020, : 245 - 246
  • [32] Novel Test Method for Mixed Mode II and III Interlaminar Fracture Toughness
    Suemasu, Hiroshi
    Kondo, Atsushi
    Gozu, Katsuhisa
    Aoki, Yuichiro
    ADVANCED COMPOSITE MATERIALS, 2010, 19 (04) : 349 - 361
  • [33] On mode I/II interlaminar fracture toughness of double-sided-loop 2D woven laminated composites
    Shao, Mingyang
    Zhou, Guangming
    Chen, Mudan
    Xing, Dandan
    Hu, Fangtian
    Kuang, Ning
    Cai, Deng'an
    COMPOSITE STRUCTURES, 2022, 286
  • [34] Effect of interleaved non-woven carbon tissue on interlaminar fracture toughness of laminated composites: Part I - Mode II
    Lee, SH
    Noguchi, H
    Kim, YB
    Cheong, SK
    JOURNAL OF COMPOSITE MATERIALS, 2002, 36 (18) : 2153 - 2168
  • [35] Computation analysis of interlaminar fracture of laminated composites
    F.-G. Buchnolz
    R. Rikards
    H. Wang
    International Journal of Fracture, 1997, 86 : 37 - 57
  • [36] Computational analysis of interlaminar fracture of laminated composites
    Buchholz, FG
    Rikards, R
    Wang, H
    INTERNATIONAL JOURNAL OF FRACTURE, 1997, 86 (1-2) : 37 - 57
  • [37] Interlaminar toughness and characteristic morphology of laminated graphite composites interlaminar-toughened
    Yi, Xiaosu
    Xu, Yahong
    Cheng, Qunfeng
    Fang, Zhengping
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2008, 22 (04): : 337 - 346
  • [38] Mode I interlaminar fracture toughness of composite
    Jiao, Guiqiong
    Gao, Jian
    Deng, Qiang
    Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica, 1994, 11 (01): : 113 - 118
  • [39] ANALYSIS OF STITCHED LAMINATED ENF SPECIMENS FOR INTERLAMINAR MODE-II FRACTURE-TOUGHNESS
    JAIN, LK
    MAI, YW
    INTERNATIONAL JOURNAL OF FRACTURE, 1994, 68 (03) : 219 - 244
  • [40] Fracture toughness characteristics of laminated composites
    Bolotin, VV
    Bolotina, KS
    Radin, VP
    Shchugorev, VN
    MECHANICS OF COMPOSITE MATERIALS, 1996, 32 (01) : 14 - 20