Potential change and corrosion behavior of two Al-Mg-Si alloys with different Si content under MgCl2 drops in 33% relative humidity

被引:4
|
作者
Li, J-F. [1 ,2 ]
Tan, X. [1 ]
机构
[1] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Peoples R China
[2] Minist Educ, Key Lab Nonferrous Met Mat Sci & Engn, Changsha 410083, Peoples R China
来源
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION | 2014年 / 65卷 / 11期
关键词
THIN ELECTROLYTE LAYERS; ATMOSPHERIC CORROSION; PITTING CORROSION; GALVANIZED STEEL; ELECTROCHEMICAL IMPEDANCE; LOCALIZED CORROSION; INITIAL-STAGE; METALS; DEPENDENCE; MECHANISM;
D O I
10.1002/maco.201307020
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The Volta potential change and corrosion behaviors of alloys Al-0.63Mg-0.28Si and Al-0.52Mg-0.63Si under MgCl2 drops with the initial concentration of 0.1-1.0 M in environments with relative humidity (RH) 33% were studied using a Kelvin probe (KP). For the alloy Al-0.63Mg-0.28Si, the Volta potential curve was mainly featured with many potential transients in the form of a sudden drop followed by an immediate recovery along the potential baseline at a higher potential value of -0.35 to -0.5 V-SHE, which were associated with initiation and repassivation of metastable pits with diameter less than 3 mu m. For the alloy Al-0.52Mg-0.63Si containing excess Si particles, the potential curve was featured with potential change in the form of slow increase followed by a sudden drop along the potential baseline at a lower potential value of about -0.7 V-SHE. The sudden potential drop and stabilizing at the lower potential level were associated with corrosion initiation and growth, respectively. In the case of lower initial concentration and higher Si content leading to excess Si particles, the corrosion rating was higher. However, the excess Si particles showed a greater impact than the initial concentration.
引用
收藏
页码:1062 / 1072
页数:11
相关论文
共 50 条
  • [41] DIFFERENT FORMS OF TEMPERING DEFECT ELIMINATION IN SUPERSATURATION DURING AGING OF 2 ALLOYS AL-CU AND AL-MG-SI
    MIRAILLE, JP
    WYON, G
    BRICHET, C
    FRADE, G
    SCRIPTA METALLURGICA, 1972, 6 (09): : 891 - &
  • [42] Corrosion behavior of Al-Mg2Si alloys with/without addition of Al-P master alloy
    Li, Zedi
    Li, Chong
    Gao, Zhiming
    Liu, Yongchang
    Liu, Xiangfa
    Guo, Qianying
    Yu, Liming
    Li, Huijun
    MATERIALS CHARACTERIZATION, 2015, 110 : 170 - 174
  • [43] Influence of Different Aqueous Media on the Corrosion Behavior of B4C-Modified Lightweight Al-Mg-Si Matrix Composites
    Kumar, Neeraj
    Sharma, Ashutosh
    Manoj, Manoranjan Kumar
    MATERIALS, 2022, 15 (23)
  • [44] Compressive creep aging behavior and microstructure evolution in extruded Al-Mg-Si alloy under different temperature and stress levels
    Zhang, Jiayi
    Fan, Jie
    Chen, Li
    Li, Youhao
    MATERIALS TODAY COMMUNICATIONS, 2022, 33
  • [45] Effect of Rolling on the Electrochemical Corrosion Behavior of Spray Deposited Al-6Si Alloys with Different Pb Content
    Mittal, Rashmi
    Moon, Abhijeet Premkumar
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (17) : 7969 - 7979
  • [46] Effect of Rolling on the Electrochemical Corrosion Behavior of Spray Deposited Al-6Si Alloys with Different Pb Content
    Rashmi Mittal
    Abhijeet Premkumar Moon
    Journal of Materials Engineering and Performance, 2023, 32 : 7969 - 7979
  • [47] Aging-Induced Hardening of Transition-Metal-Containing Al-Mg-Si Alloys Subjected to Deformation under Different Conditions
    Bochvar, N. R.
    Rokhlin, L. L.
    Tarytina, I. E.
    Leonova, N. P.
    RUSSIAN METALLURGY, 2019, 2019 (05): : 524 - 530
  • [48] Nanocluster formation and two-step aging behavior in Al-Mg-Si(-xCu: X=0-4 mass%) alloys
    Kim, InSu
    Song, MinYoung
    Kim, JaeHwang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 857
  • [49] Thermal Stability and Transition Behavior of Nanoclusters during Two-Step Aging at 250°C in Al-Mg-Si(-Cu) Alloys
    Kim, JaeHwang
    Kim, SeongNyeong
    Kobayashi, Equo
    Sato, Tatsuo
    MATERIALS TRANSACTIONS, 2014, 55 (05) : 768 - 773
  • [50] Investigations of Al-Mg-Si Alloys Containing 0,8% Mg2Si with Different Amounts of Excess Si, Treated by T-HA (T8) Cycles.
    Giarda, Andrea
    Buratti, Massimo
    Di Russo, Ettore
    Alluminio, 1976, 45 (7-8): : 387 - 399