Four year performance of dentine-bonded all-ceramic crowns

被引:12
|
作者
Burke, F. J. T. [1 ]
机构
[1] Univ Birmingham, Sch Dent, Primary Dent Care Res Grp, Birmingham B4 6NN, W Midlands, England
关键词
D O I
10.1038/bdj.2007.176
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Aim This paper reports a prospective evaluation of 59 dentine-bonded crowns placed in a dental school environment for patients, a majority of whom were suffering from tooth substance loss. Results Forty-eight crowns (83%) were available for examination, with their mean age since placement being 3.9 years. The mean age of the patients in whom the crowns were placed was 37.5 years. Three crowns had failed due to porcelain fractures, an overall failure rate of 6%. Two of the failures were minimal cracks of which the patient was unaware, and one, in an upper premolar tooth, because of crown fracture. No secondary caries was noted, incidence of pulp symptoms or pulp death was nil, and margins were rated as `excellent' in 42 crowns (86%). Conclusion The dentine bonded crowns assessed in this study showed excellent retention and low incidence of fracture at four years. This technique would appear to be suitable for a variety of clinical indications, including treatment of tooth substance loss, although the results presented in this study are relatively short term in relation to the anticipated life of restorations.
引用
收藏
页码:269 / 273
页数:5
相关论文
共 50 条
  • [41] Clinically relevant fracture testing of all-ceramic crowns
    Oilo, Marit
    Kvam, Ketil
    Tibballs, John E.
    Gjerdet, Nils Roar
    DENTAL MATERIALS, 2013, 29 (08) : 815 - 823
  • [42] Influence of luting agent on the microleakage of all-ceramic crowns
    Toman, Muhittin
    Toksavul, Suna
    Artunc, Celal
    Turkun, Murat
    Schmage, Petra
    Nergiz, Ibrahim
    JOURNAL OF ADHESIVE DENTISTRY, 2007, 9 (01): : 39 - 47
  • [43] Fracture resistance of all-ceramic molar-crowns
    Behr, M
    Rosentritt, M
    Hofmann, E
    Latzel, D
    Handel, G
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B247 - B247
  • [44] Fracture resistence of implant all-ceramic crowns.
    Suzuki, RM
    Mezzomo, E
    Teixeira, ER
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B181 - B181
  • [45] All-ceramic crowns and preparation characteristics:: A mathematic approach
    Oilo, G
    Törnquist, A
    Durling, D
    Andersson, M
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2003, 16 (03) : 301 - 306
  • [46] THE FIT OF MOLDED ALL-CERAMIC, TWIN FOIL, AND CONVENTIONAL CERAMIC CROWNS
    BRUKL, CE
    PHILP, GK
    JOURNAL OF PROSTHETIC DENTISTRY, 1987, 58 (04): : 408 - 413
  • [47] COMPARISON OF THE FRACTURE STRENGTHS OF CERAMOMETAL CROWNS VERSUS SEVERAL ALL-CERAMIC CROWNS
    MILLER, A
    LONG, J
    MILLER, B
    COLE, J
    JOURNAL OF PROSTHETIC DENTISTRY, 1992, 68 (01): : 38 - 41
  • [48] Fractographic analyses of all-ceramic crowns: A study of 27 clinically fractured crowns
    Oilo, Marit
    Gjerdet, Nils Roar
    DENTAL MATERIALS, 2013, 29 (06) : E78 - E84
  • [49] Standards of teeth preparations for anterior resin bonded all-ceramic crowns in private dental practice in Jordan
    Al-Dwairi, Ziad Nawaf
    Al-Hiyasat, Ahmad Saleh
    Aboud, Haitham
    JOURNAL OF APPLIED ORAL SCIENCE, 2011, 19 (04) : 370 - 377