Study on Electrochemical Corrosion Behavior of Co Base Super-alloys in Chloride Solution

被引:2
|
作者
Zhu, Jiao-jiao [1 ]
Fen, Li [2 ]
Guan, Jian-jun [1 ]
Gao, Peng [1 ]
Shi, Xiao-ai [3 ]
机构
[1] Liaoning Petrochem Univ, Sch Mech Engn, Fushun 113001, Liaoning, Peoples R China
[2] Shengyang Polytech Coll, Sch Elect Engn, Shenyang 110045, Peoples R China
[3] Eighth Construct Co CNPC Ltd, Fushun 113006, Peoples R China
来源
关键词
Co base super-alloys; Heat treatment; Electrochemistry; pitting corrosion; TEMPERATURE; STEEL;
D O I
10.20964/2021.06.22
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The Co base super-alloys after heat treatment were studied, and its corrosion resistance in chlorine solution was evaluated by electrochemical methods. The surface morphology of Co base super-alloys was observed by Scanning Electron Microscope (SEM) before and after corrosion property tests. Potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) were used to study electrochemical corrosion behavior of Co base super-alloys in chlorine solution. The results show that the typical 11 phase is found after the heat treatment of the Co base super-alloys, and the 11 phase appears as a light gray blocky morphology. The results of potentiodynamic polarization and EIS experiments show that the Co base super-alloys have the characteristics of a typical passivation metal. The potentiodynamic polarization experiment results show that the passivation range is -0.3V to 0.4V. The observation of the surface morphology shows that the 11 phase of the Co base super-alloys has severe pitting corrosion. The corrosion not only expands along the substrate around the 11 phase to form a groove, but also the corrosion holes continue to penetrate into the substrate and present a spiral shape.
引用
收藏
页码:1 / 10
页数:10
相关论文
共 50 条
  • [31] PRECIPITATION HARDENING MECHANISM IN NI-BASE WROUGHT SUPER-ALLOYS
    SHIMANUKI, Y
    TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1981, 22 (01): : 17 - 24
  • [32] An electrochemical investigation and corrosion performance of some aluminum alloys in chloride solution
    Elboujdaini, M
    Shehata, MT
    Ghali, E
    ANALYSIS OF IN-SERVICE FAILURES AND ADVANCES IN MICROSTRUCTURAL CHARACTERIZATION, 1999, 26 : 91 - 97
  • [33] HIGH-TEMPERATURE CORROSION OF SUPER-ALLOYS IN CHLORINE CONTAMINATED ENVIRONMENTS
    OH, JM
    MCNALLAN, MJ
    LAI, GY
    ROTHMAN, MF
    JOURNAL OF METALS, 1982, 35 (12): : A76 - A76
  • [34] FEATURES OF ALLOYING OF NI-BASE SUPER-ALLOYS AT THE DIRECTED CRYSTALLIZATION
    KISHKIN, ST
    STROGANOV, GB
    LOGUNOV, AV
    GLEZER, GM
    MOROZOVA, GI
    MOROZOVA, SG
    SOBOLEV, GI
    DOKLADY AKADEMII NAUK SSSR, 1983, 268 (04): : 865 - 867
  • [35] DEVELOPMENT OF COBALT-FREE NICKEL-BASE SUPER-ALLOYS
    KOIZUMI, Y
    YAMAZAKI, M
    HARADA, H
    TRANSACTIONS OF NATIONAL RESEARCH INSTITUTE FOR METALS, 1980, 22 (03): : 144 - 150
  • [36] ELECTROCHEMICAL AND CORROSION FATIGUE BEHAVIOR OF FEALMN ALLOYS IN NACL SOLUTION
    DUH, JB
    TSAI, WT
    LEE, JT
    CORROSION, 1988, 44 (11) : 810 - 818
  • [37] NICKEL-BASE SUPER-ALLOYS BY ALLOY DESIGN .8. THE CREEP-RUPTURE STRENGTH OF NICKEL-BASE SUPER-ALLOYS WITH VARIED CONCENTRATION OF TA, W AND MO
    KUSUNOKI, K
    MATSUBAYASHI, K
    SAKUMA, N
    NAKAZAWA, S
    YAMAZAKI, M
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1983, 23 (03) : B107 - B107
  • [38] Electrochemical Study of Corrosion Behavior of Wrought Stellite Alloys in Sodium Chloride and Green Death Solutions
    X. Z. Zhang
    R. Liu
    K. Y. Chen
    M. X. Yao
    R. Collier
    Journal of Materials Engineering and Performance, 2015, 24 : 3579 - 3587
  • [39] Electrochemical Study of Corrosion Behavior of Wrought Stellite Alloys in Sodium Chloride and Green Death Solutions
    Zhang, X. Z.
    Liu, R.
    Chen, K. Y.
    Yao, M. X.
    Collier, R.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (09) : 3579 - 3587
  • [40] AGE-HARDENING MECHANISM IN NI-BASE WROUGHT SUPER-ALLOYS
    SHIMANUKI, Y
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1979, 43 (03) : 203 - 208