In vitro degradation of porous poly(propylene fumarate)/poly(DL-lactic-co-glycolic acid) composite scaffolds

被引:90
|
作者
Hedberg, EL
Shih, CK
Lemoine, JJ
Timmer, MD
Liebschner, MAK
Jansen, JA
Mikos, AG
机构
[1] Rice Univ, Dept Bioengn, Houston, TX 77251 USA
[2] Univ Nijmegen, Med Ctr, Dept Biomat, NL-6500 HB Nijmegen, Netherlands
关键词
composite polymer; injectable scaffold; degradation; bone-tissue engineering;
D O I
10.1016/j.biomaterials.2004.09.012
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
This study investigated the in vitro degradation of porous poly(propylene fumarate) (PPF-based) composites incorporating microparticles of blends of poly(DL-lactic-eo-glycolic acid) (PLGA) and poly(ethylene glycol) (PEG) during a 26-week period in pH 7.4 phosphate-buffered saline at 37 degreesC. Using a fractional factorial design, four formulations of composite scaffolds were fabricated with varying PEG content of the microparticles, microparticle mass fraction of the composite material, and initial leachable porogen content of the scaffold formulations. PPF scaffolds without microparticles were fabricated with varying leachable porogen content for use as controls. The effects of including PLGA/PEG microparticles in PPF scaffolds and the influence of alterations in the composite formulation on scaffold mass, geometry, water absorption, mechanical properties and porosity were examined for cylindrical specimens with lengths of 13 mm and diameters of 6.5 mm. The composite scaffold composition affected the extent of loss of polymer mass, scaffold length, and diameter, with the greatest loss of polymer mass equal to 15+/-5% over 26 weeks. No formulation, however, exhibited any variation in compressive modulus or peak compressive strength over time. Additionally, sample porosity, as determined by both mercury porosimetry and micro-computed tomography did not change during the period of this study. These results demonstrate that microparticle carriers can be incorporated into PPF scaffolds for localized delivery of bioactive molecules without altering scaffold mechanical or structural properties up to 26 weeks in vitro. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:3215 / 3225
页数:11
相关论文
共 50 条
  • [1] In vivo degradation of porous poly(propylene fumarate)/poly(DL-lactic-co-glycolic acid) composite scaffolds
    Hedberg, EL
    Kroese-Deutman, HC
    Shih, CK
    Crowther, RS
    Carney, DH
    Mikos, AG
    Jansen, JA
    [J]. BIOMATERIALS, 2005, 26 (22) : 4616 - 4623
  • [2] In vitro and in vivo degradation of porous poly(DL-lactic-co-glycolic acid) foams
    Lu, L
    Peter, SJ
    Lyman, MD
    Lai, HL
    Leite, SM
    Tamada, JA
    Uyama, S
    Vacanti, JP
    Langer, R
    Mikos, AG
    [J]. BIOMATERIALS, 2000, 21 (18) : 1837 - 1845
  • [3] Degradation and miscibility of poly(DL-lactic acid)/poly(glycolic acid) composite films: Effect of poly(DL-lactic-co-glycolic acid)
    Ma, Zhigang
    Zhao, Na
    Xiong, Chengdong
    [J]. BULLETIN OF MATERIALS SCIENCE, 2012, 35 (04) : 575 - 578
  • [4] Degradation and miscibility of poly(DL-lactic acid)/poly(glycolic acid) composite films: Effect of poly(DL-lactic-co-glycolic acid)
    ZHIGANG MA
    NA ZHAO
    CHENGDONG XIONG
    [J]. Bulletin of Materials Science, 2012, 35 : 575 - 578
  • [5] In vitro degradation of thin poly(DL-lactic-co-glycolic acid) films
    Depts. of Chem. Eng. and Bioeng., Rice University, 6100 Main Street, Houston, TX 77005-1892, United States
    不详
    [J]. J Biomed Mater Res, 2 (236-244):
  • [6] In vitro degradation of thin poly(DL-lactic-co-glycolic acid) films
    Lu, L
    Garcia, CA
    Mikos, AG
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1999, 46 (02): : 236 - 244
  • [7] Porous poly(DL-lactic-co-glycolic acid)/calcium phosphate cement composite for reconstruction of bone defects
    Ruhe, P. Quinten
    Hedberg-Dirk, Elizabeth L.
    Padron, Nestor Torio
    Spauwen, Paul H. M.
    Jansen, John A.
    Mikos, Antonios G.
    [J]. TISSUE ENGINEERING, 2006, 12 (04): : 789 - 800
  • [8] Peptide degradation during preparation and in vitro release testing of poly(L-lactic acid) and poly(DL-lactic-co-glycolic acid) microparticles
    Witschi, C
    Doelker, E
    [J]. INTERNATIONAL JOURNAL OF PHARMACEUTICS, 1998, 171 (01) : 1 - 18
  • [9] Biocompatibility and degradation of poly(DL-lactic-co-glycolic acid)/calcium phosphate cement composites
    Ruhé, PQ
    Hedberg, EL
    Padron, NT
    Spauwen, PHM
    Jansen, JA
    Mikos, AG
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2005, 74A (04) : 533 - 544
  • [10] Three-dimensional porous poly(propylene fumarate)-co-poly(lactic-co-glycolic acid) scaffolds for tissue engineering
    Wu, Wei
    Liu, Xifeng
    Zhou, Zifei
    Miller, A. Lee, II
    Lu, Lichun
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2018, 106 (09) : 2507 - 2517