摘要
This paper employs simple rolling process plus annealing to refine the grain size of magnesium alloy ZK60. This goal is effectively achieved, obtaining grains as fine as similar to 3.7 mu m. Such a specimen shows an elongation of 642%, and its ultimate fracture surface exhibits intergranular separation and significant grain growth. Additionally, the effects of the specimen's geometry and tensile test axis with respect to the rolling direction on superplastic elongation is studied, which has not been done before.
引用
收藏
页码:421 / 425
页数:5
相关论文
共 50 条
  • [31] Homogenizing research on ZK60 magnesium alloy ingot
    Peng, Jian
    Zhang, Ding-Fei
    Yang, Chun-Mei
    Ding, Pei-Dao
    Cailiao Gongcheng/Journal of Materials Engineering, 2004, (08): : 32 - 35
  • [32] Impression creep behavior of magnesium alloy ZK60
    Liao, Huimin
    Zeng, Ming
    Chen, Hong
    MATERIALS TESTING, 2018, 60 (01) : 68 - 72
  • [33] Analysis of the hot deformation of ZK60 magnesium alloy
    Hadadzadeh, Amir
    Wells, Mary A.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2017, 5 (04) : 369 - 387
  • [34] Superplasticity in a ZK60 magnesium alloy at low temperatures
    Watanabe, H
    Mukai, T
    Higashi, K
    SCRIPTA MATERIALIA, 1999, 40 (04) : 477 - 484
  • [35] Low temperature superplasticity in a ZK60 magnesium alloy
    Watanabe, H
    Mukai, T
    Kohzu, M
    Tanabe, S
    Higashi, K
    MATERIALS TRANSACTIONS JIM, 1999, 40 (08): : 809 - 814
  • [36] Pseudo-Superplastic Characteristics of ZK60 Alloy with Fibrous Microstructure
    Wang, Cheng-Yu
    Wang, Jian-Yih
    Saufan, Akhmd
    Fu, Yen-Pei
    MATERIALS TRANSACTIONS, 2018, 59 (04) : 674 - 678
  • [37] Low temperature superplasticity of a fine-grained ZK60 magnesium alloy processed by equal-channel-angular extrusion
    Watanabe, H
    Mukai, T
    Ishikawa, K
    Higashi, K
    SCRIPTA MATERIALIA, 2002, 46 (12) : 851 - 856
  • [38] Inter-granular liquid phase aiding grain boundary sliding in superplastic deformation of fine-grained ZK60 Mg alloy
    Lee Shyong
    Chiang Chih-te
    Chu Chun-lin
    Hsu Chang-chuan
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 : S576 - S579
  • [39] Inter-granular liquid phase aiding grain boundary sliding in superplastic deformation of fine-grained ZK60 Mg alloy
    LEE Shyong
    CHIANG Chih-te
    HSU Chang-chuan
    TransactionsofNonferrousMetalsSocietyofChina, 2010, 20(S2) (S2) : 576 - 579
  • [40] Inter-granular liquid phase aiding grain boundary sliding in superplastic deformation of fine-grained ZK60 Mg alloy
    Lee S.
    Chiang C.-T.
    Chu C.-L.
    Hsu C.-C.
    Transactions of Nonferrous Metals Society of China (English Edition), 2010, 20 (SUPPL. 2): : s576 - s579