Microstructure and mechanical properties of LMD-SLM hybrid forming Ti6A14V alloy

被引:68
|
作者
Liu, Qi [1 ]
Wang, Yudai [1 ]
Zheng, Hang [1 ,2 ]
Tang, Kang [1 ,3 ]
Ding, Li [1 ]
Li, Huaixue [1 ]
Gong, Shuili [1 ]
机构
[1] AVIC Beijing Aeronaut Mfg Technol Res Inst, Sci & Technol Power Beam Proc Lab, Beijing Key Lab High Power Beam Addit Mfg Technol, Aeronaut Key Lab Addit Mfg Technol, Beijing 100024, Peoples R China
[2] Beihang Univ, Sch Mech Engn & Automat, Beijing 100191, Peoples R China
[3] China Univ Petr, Sch Mech Engn, Qingdao 266000, Peoples R China
基金
中国国家自然科学基金;
关键词
Laser melting deposition; Selective laser melting; Ti6Al4V; Hybrid forming; Mechanical properties; LASER; BEHAVIOR; FABRICATION; COMPONENTS; POWDER; NANOCOMPOSITES; PERFORMANCE; DEPOSITION; EVOLUTION; DENSITY;
D O I
10.1016/j.msea.2016.02.069
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Laser melting deposition (LMD) and selective laser melting (SLM) are two major metal additive manufacturing technologies that explore the near-net shaping of large components and net shaping of small complex structures. In order to achieve subscale complex structures, researchers proposed LMD-SLM hybrid manufacturing processes. Ti6Al4V is an alpha-beta dual-phase, moderate strength titanium alloy that is widely used in the fields of medicine, aeronautics, and astronautics. In this study, thin (1.5-2.5 mm) horizontal, vertical SLM plate and rolled plate are used as substrate materials for the LMD process to analyze tensile properties, microhardness, microstructure, and internal defects. The results show that the LMD process forms a hybrid with the aforementioned plates. The relative density of hybrid-forming area can reach 99.5%, because of the existence of the pores with diameter < 20 mu m. Tensile strength and elongation of the hybrid thus produced can reach respectively 918 MPa and 11%, and fractures are located in the LMD zone. Internal layer fracture of the LMD zone increases elongation, whereas layer interface fracture decreases it. The laser deposition process epitaxially generates coarse columnar crystals, and laser remelting reduces the microhardness of the SLM substrate in the 2- to 3-mm-thick grain-increased heat-affected zone (HAZ). The microhardness distributions of the LMD zone, HAZ, and substrate material are found to be 344, 343, and 375 (horizontal SLM); 346, 334, and 386 (vertical SLM); and 351, 328, and 340 HV (rolled plate), respectively. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:24 / 33
页数:10
相关论文
共 50 条
  • [41] Finish machining of Ti6A14V SLM components under consideration of thin walls and support structure removal
    Hintze, Wolfgang
    von Wenserski, Robert
    Junghans, Sebastian
    Moeller, Carsten
    48TH SME NORTH AMERICAN MANUFACTURING RESEARCH CONFERENCE, NAMRC 48, 2020, 48 : 485 - 491
  • [42] FRICTION AND WEAR BEHAVIORS OF Ti6A14V ALLOY TREATED BY PLASMA Ni ALLOYING
    Wang, Zhenxia
    Cai, Wenlan
    Wu, Hairui
    Lin, Naiming
    Yao, Xiaohong
    He, Zhiyong
    Liu, Xiaoping
    SURFACE REVIEW AND LETTERS, 2018, 25 (05)
  • [43] MODELING OF DYNAMIC RECRYSTALLIZATION OF Ti6A14V ALLOY USING A CELLULAR AUTOMATON APPROACH
    J.W.Zhao~(1)*) H.Din~(1)) W.J.Zhao~(1)) F.R.Cao~(1)) H.L.Hou~(2)) Z.Q.Li~(2)) 1)School of Materials and Metallurgy
    Acta Metallurgica Sinica(English Letters), 2008, (04) : 260 - 268
  • [44] Bacteria adherence property of molybdenum nitride modified layer on Ti6A14V alloy
    Fan Ai-lan
    Tian Lin-hai
    Qin Lin
    Tang Bin
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2007, 17 : S889 - S891
  • [45] Nanoindentation Measurement of Creep Stress Exponent of Ti6A14V Alloy at Room Temperature
    Meng Longhui
    Yang Yinfei
    He Ning
    RARE METAL MATERIALS AND ENGINEERING, 2016, 45 (03) : 617 - 622
  • [46] Heat-treated microstructure and mechanical properties of laser solid forming Ti-6Al-4V alloy
    Shuangyin Zhang
    Xin Lin
    Jing Chen
    Weidong Huang
    Rare Metals, 2009, 28 : 537 - 544
  • [47] Heat-treated microstructure and mechanical properties of laser solid forming Ti-6Al-4V alloy
    ZHANG Shuangyin
    Rare Metals, 2009, 28 (06) : 537 - 544
  • [48] Heat-treated microstructure and mechanical properties of laser solid forming Ti-6Al-4V alloy
    Zhang Shuangyin
    Lin Xin
    Chen Jing
    Huang Weidong
    RARE METALS, 2009, 28 (06) : 537 - 544
  • [49] Corrosion-wear behavior of molybdenum nitride layer on Ti6A14V alloy
    Qin Lin
    Zhan Ke
    Fan Ailan
    Tang Bin
    RARE METAL MATERIALS AND ENGINEERING, 2008, 37 (04) : 725 - 728
  • [50] Microarc oxidation coatings formed on Ti6A14V in Na2SiO3 system solution:: Microstructure, mechanical and tribological properties
    Wang, Y. M.
    Jiang, B. L.
    Lei, T. Q.
    Guo, L. X.
    SURFACE & COATINGS TECHNOLOGY, 2006, 201 (1-2): : 82 - 89