Catalytic reforming of methane with carbon dioxide on reduced perovskite-type oxides

被引:2
|
作者
Wu, YY
Motoi, S
Sugiyama, K
Matsuda, T
Yoshida, Y
机构
[1] Saitama Univ, Fac Engn, Dept Appl Chem, Urawa, Saitama 3388570, Japan
[2] Toyo Univ, Fac Engn, Dept Appl Chem, Kawagoe, Saitama 3508585, Japan
关键词
D O I
10.1246/nikkashi.2000.613
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The reforming reactions of CH4 with CO2 diluted with He were carried out over the cobalt catalysts prepared from the perovskite structural oxides, LnCoO(3) (Ln = La, Pr, Nd, Sm, Eu, Gd, Er, Tb) and the relationship between the reaction activity and the surface properties of the catalysts were examined. The reaction activity at 873 K of the catalysts containing the rear earth element of higher atomic number than Eu was remarkably higher than that of the catalysts having lower atomic number than Eu. The surface properties of the Co/La2O3, Co/Sm2O3 and Co/Eu2O3 catalysts decomposed from LaCoO3, SmCoO3 and EuCoO3 were particularly examined. EuCoO3 was reduced much easier to metallic cobalt and europium oxide than LaCoO3 and SmCoO3. The decomposed products by reduction were led to the catalyst with high activity. On the other hand, LaCoO3 and SmCoO3 were not fully and easily reduced and very small amount of cobalt oxides remained on the surface. The difficulty of reducibility of LaCoO3 and SmCoO3 caused the lost or low activity. The decomposed Co/Eu2O3 catalyst had two kinds of active sites which operated at relatively low (873 K) and high temperature (1073 K) regions. The other two kinds of catalysts had only one active site which operated at high temperature. This caused the lost or low activity at low temerature such as 873 K in the case of the latter. Especially the decomposed Co/La2O3 catalyst had a strong affinity to CO2 and easily produced a lanthanum carbonate which was decomposed at high temperature (> 973 K). The formation of the carbonate inhibited the reaction, probably by the oxidation of the metallic cobalt on the catalyst surface.
引用
收藏
页码:613 / 620
页数:8
相关论文
共 50 条
  • [21] Mechanical Activation of Perovskite-Type Oxides for Catalytic Combustion
    S. Soiron
    L. Aymard
    A. Rougier
    J.-M. Tarascon
    [J]. Topics in Catalysis, 2001, 16-17 : 391 - 395
  • [22] Effect of metal oxides on the reforming of methane with carbon dioxide
    Yaquan Wang
    Li Yang
    Tao Wang
    Zaiyi Zhang
    Gang Ruan
    Sen Han
    [J]. Reaction Kinetics and Catalysis Letters, 1999, 68 : 183 - 190
  • [23] Effect of metal oxides on the reforming of methane with carbon dioxide
    Wang, YQ
    Yang, L
    Wang, T
    Zhang, ZY
    Ruan, G
    Han, S
    [J]. REACTION KINETICS AND CATALYSIS LETTERS, 1999, 68 (02): : 183 - 190
  • [24] CO2 reforming of methane over supported LaNiO3 perovskite-type oxides
    Rabelo-Neto, R. C.
    Sales, H. B. E.
    Inocencio, C. V. M.
    Varga, E.
    Oszko, A.
    Erdohelyi, A.
    Noronha, F. B.
    Mattos, L. V.
    [J]. APPLIED CATALYSIS B-ENVIRONMENTAL, 2018, 221 : 349 - 361
  • [25] Mechanical activation of perovskite-type oxides for catalytic combustion
    Soiron, S
    Aymard, L
    Rougier, A
    Tarascon, JM
    [J]. TOPICS IN CATALYSIS, 2001, 16 (1-4) : 391 - 395
  • [26] Perovskite-type mixed oxides as catalytic material for NO removal
    Zhu, Junjiang
    Thomas, Arne
    [J]. APPLIED CATALYSIS B-ENVIRONMENTAL, 2009, 92 (3-4) : 225 - 233
  • [27] CATALYTIC OXIDATION OF METHANE AT LOW TEMPERATURE OVER Ni-CONTAINING PEROVSKITE-TYPE OXIDES
    Wu, Yuehui
    Luo, Laitao
    Yan, Liushui
    [J]. OXIDATION COMMUNICATIONS, 2012, 35 (01): : 51 - 57
  • [28] Catalytic evaluation of perovskite-type oxide LaNi1-xRuxO3 in methane dry reforming
    de Arauj, Genira Carneiro
    de Lima, Sania Maria
    Assaf, Jose Mansur
    Pena, Miguel Antonio
    Garcia Fierro, Jose Luis
    Rangel, Maria do Carmo
    [J]. CATALYSIS TODAY, 2008, 133 (129-135) : 129 - 135
  • [30] OXIDATIVE COUPLING OF METHANE OVER PEROVSKITE-TYPE OXIDES.
    France, J.E.
    Shamsi, A.
    Ahsan, M.Q.
    [J]. 1988, 2 (02): : 235 - 236