Austenite stability in reversion-treated structures of a 301LN steel under tensile loading

被引:40
|
作者
Jarvenpaa, Antti [1 ]
Jaskari, Matias [1 ]
Man, Jiri [2 ]
Karjalainen, L. Pentti [3 ]
机构
[1] Univ Oulu, Kerttu Saalasti Inst, Pajatie 5, FI-85500 Nivala, Finland
[2] Inst Phys Mat ASCR, Zizkova 22, Brno 61662, Czech Republic
[3] Univ Oulu, Ctr Adv Steels Res, POB 4200, FI-90014 Oulu, Finland
关键词
Austenitic stainless steel; Austenite stability; Grain size; Reversion annealing; Strain-induced martensite; Tensile straining; DEFORMATION-INDUCED MARTENSITE; STACKING-FAULT ENERGY; GRAIN-SIZE; STAINLESS-STEEL; MECHANICAL-PROPERTIES; MICROSTRUCTURE EVOLUTION; INDUCED PLASTICITY; CYCLE FATIGUE; AISI; 304L; TRANSFORMATION;
D O I
10.1016/j.matchar.2017.01.040
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ultrafine-grained austenitic stainless steels can be produced by the martensitic reversion process, but the factors affecting the stability of refined austenite in subsequent deformation are still unclear. To clarify this, fully and partially austenitic reversed structures with the average grain size between 24 and 0.6 pm were created in a 60% cold-rolled 301LN type (18Cr-7Ni-0.16N) austenitic stainless steel by varying the annealing conditions. The amount of strain-induced alpha'-martensite (SIM) during tensile loading was determined by magnetic measurements and the microstructure evolution and texture examined by electron backscatter diffraction and X-ray diffraction methods. The extensive experimental data evidenced firmly that in completely austenitic structures the austenite stability increases with decreasing grain size down to about 1 mu m, obtained at 900 degrees C, but the stability decreases drastically in the ultrafine-grained and partially reversed structures, with the average grain size of 0.6-0.7 gm obtained at 800-700 degrees C. However, these structures are nonuniform also containing larger micron-size grains transformed from slightly deformed SIM. The low stability of austenite is not a result from the ultrafine grain size, neither due to retained phases nor texture, but the main reason is concluded to be the precipitation of CrN during the reversion at low temperatures of 800-700 degrees C. Due to this precipitation, micron-size grains in the ultrafine and partially reversed structures show most unstable behavior under tensile deformation. (C) 2017 Elsevier Inc. All rights reserved.
引用
收藏
页码:12 / 26
页数:15
相关论文
共 14 条
  • [11] The mechanical stability of retained austenite in low-alloyed TRIP steel under shear loading
    Blonde, R.
    Jimenez-Melero, E.
    Zhao, L.
    Schell, N.
    Brueck, E.
    van der Zwaag, S.
    van Dijk, N. H.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 594 : 125 - 134
  • [12] Mechanical stability of individual austenite grains in TRIP steel studied by synchrotron X-ray diffraction during tensile loading
    Blonde, R.
    Jimenez-Melero, E.
    Zhao, L.
    Wright, J. P.
    Bruck, E.
    van der Zwaag, S.
    van Dijk, N. H.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 618 : 280 - 287
  • [13] Strain sensing behavior of textile structures made of stainless steel continuous filament yarns under uni-axial tensile loading
    Yang, Bin
    Tao, XiaoMing
    Cai, Jiayang
    Yu, TongXi
    [J]. INTERNATIONAL CONFERENCE ON SMART MATERIALS AND NANOTECHNOLOGY IN ENGINEERING, PTS 1-3, 2007, 6423
  • [14] Repair of steel structures by bonded carbon fibre reinforced polymer patching: experimental and numerical study of carbon fibre reinforced polymer-steel double-lap joints under tensile loading
    Lam, Angus C. C.
    Cheng, J. J. Roger
    Yam, Michael C. H.
    Kennedy, Gaylene D.
    [J]. CANADIAN JOURNAL OF CIVIL ENGINEERING, 2007, 34 (12) : 1542 - 1553