Comparison of slip system activation in Ti-6Al-2Sn-4Zr-2Mo and Ti-6Al-2Sn-4Zr-6Mo under tensile, fatigue and dwell-fatigue loadings

被引:41
|
作者
Hemery, S. [1 ]
Villechaise, P. [1 ]
机构
[1] Univ Poitiers, CNRS, ENSMA, UPR CNRS 3346,Phys & Mech Mat Dept,Inst Pprime, Teleport 2,1 Ave Clement Ader,BP 40109, F-86961 Futuroscope, France
关键词
Titanium alloys; EBSD; Crystal plasticity; Fatigue; STRAIN-RATE SENSITIVITY; ALPHA-TITANIUM; DEFORMATION-BEHAVIOR; AL ALLOY; MICROSTRUCTURE; TI-6AL-4V; CREEP; PHASE;
D O I
10.1016/j.msea.2017.05.021
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The deformation systems operating in Ti-6Al-2Sn-4Zr-2Mo and Ti-6Al-2Sn-4Zr-6Mo at the onset of plastic slip were characterized by means of monotonic in-situ tensile tests performed in a scanning electron microscope. A slip traces analysis was carried out using the local crystalline orientation characterized by the electron backscattered diffraction technique. The activation of the involved deformation processes were then characterized step by step and the critical resolved shear stress was estimated. Interrupted fatigue and dwell fatigue tests were conducted on both alloys as well to study the possible specificities associated to the operating slip system distribution under cyclic loadings. The main challenge of this work is thus to detect any significant difference in deformation behavior between both alloys that could explain, even partly, the difference they exhibit in dwell fatigue regime. A potential relationship between the operating slip systems and dwell-fatigue life debit is finally discussed.
引用
收藏
页码:177 / 183
页数:7
相关论文
共 50 条
  • [11] HYDROGEN EMBRITTLEMENT OF TI-6AL-2SN-4ZR-6MO ALLOY
    NIINOMI, M
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (05): : S738 - S738
  • [12] DEHYDRIDING OF TI-6AL-2SN-4ZR-6MO HYDRIDE POWDER
    BIRLA, NC
    DEPIERRE, V
    POWDER METALLURGY, 1975, 18 (35) : 15 - 31
  • [13] Microstructural effects on fatigue and dwell-fatigue crack growth in α/β Ti-6Al-2Sn-4Zr-2Mo-0.1 Si
    Shen, W
    Soboyejo, ABO
    Syejo, WO
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (01): : 163 - 187
  • [14] Fatigue and dwell-fatigue crack growth in Ti-6Al-2Sn-4Zr-2Mo-0.1Si with elongated α/β microstructure
    Shen, W
    Soboyejo, ABO
    Soboyejo, WO
    FATIGUE - DAVID L. DAVIDSON SYMPOSIUM, 2002, : 227 - 245
  • [15] Microstructural effects on fatigue and dwell-fatigue crack growth in α/β Ti-6Al-2Sn-4Zr-2Mo-0.1Si
    W. Shen
    W. O. Soboyejo
    A. B. O. Soboyejo
    Metallurgical and Materials Transactions A, 2004, 35 : 163 - 187
  • [16] OXIDATION AND EMBRITTLEMENT OF TI-6AL-2SN-4ZR-2MO ALLOY
    SHENOY, RN
    UNNAM, J
    CLARK, RK
    OXIDATION OF METALS, 1986, 26 (1-2): : 105 - 124
  • [17] INFLUENCE OF MICROSTRUCTURE ON FATIGUE CRACK GROWTH-RATES IN TI-6AL-2SN-4ZR-6MO
    BIDWELL, LR
    CHAKRABARTI, AK
    JOM-JOURNAL OF METALS, 1975, 27 (12): : A58 - A58
  • [18] MICROSTRUCTURES AND PROPERTIES OF TI-6AL-2SN-4ZR-6MO POWDER FORGINGS
    WEISS, I
    FROES, FH
    EYLON, D
    CHEN, CC
    JOURNAL OF METALS, 1983, 35 (12): : 21 - 21
  • [19] EFFECT OF COATINGS ON OXIDATION OF TI-6AL-2SN-4ZR-2MO FOIL
    CLARK, RK
    UNNAM, J
    WIDEMANN, KE
    OXIDATION OF METALS, 1987, 28 (5-6): : 391 - 405
  • [20] The effect of Ni on the creep deformation of Ti-6Al-2Sn-4Zr-2Mo
    Hayes, RW
    Viswanathan, B
    Mills, MJ
    CREEP DEFORMATION: FUNDAMENTALS AND APPLICATIONS, 2002, : 105 - 115