Oxidation Kinetics of Nd-Fe-B Permanent Magnets Prepared by Spark Plasma Sintering

被引:11
|
作者
Liu, W. Q. [1 ]
Yue, M. [1 ]
Wang, G. P. [2 ]
Zhang, D. T. [1 ]
Zhang, J. X. [1 ]
机构
[1] Beijing Univ Technol, Coll Mat Sci & Engn, Beijing 100124, Peoples R China
[2] Jiangxi Normal Univ, Coll Phys & Commun Elect, Nanchang 330022, Peoples R China
基金
高等学校博士学科点专项科研基金;
关键词
microstructure; Nd-Fe-B magnet; oxidation resistance; spark plasma sintering; CORROSION; BEHAVIOR;
D O I
10.5006/1.3430464
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An an isotropic Nd-Fe-B magnet was prepared by the spark plasma sintering (SPS) technique. A magnet with the same composition was produced using the conventional sintering method for comparison. The oxidation behavior in oxidizing environments for both magnets was studied. The microstructure and composition of the magnets were investigated using scanning electron microscopy with an energy-dispersive x-ray detector. Compared with the conventional sintered Nd-Fe-B magnet, the SPS magnet possesses a lower oxygen diffusion coefficient, which leads to a lower oxidation rate, a thinner oxidation layer, and lower oxygen Content. Microstructure observation shows that the SPS magnet possesses a unique microstructure due to the special sintering mechanism. In detail, the grain size of the Nd2Fe14B main phase is fine and uniform. Only a little of the Nd-rich phase forms along the grain boundaries of the Nd2Fe14B phase, while most of it agglomerates into triple junctions as small particles. Therefore, the pathways for oxidation propagation are restricted and the intergranular oxidation process through the Nd-rich phase in the magnet is suppressed effectively. As a result, the SPS Nd-Fe-B magnet: possesses better oxidation resistance than that of the conventional magnet.
引用
收藏
页数:5
相关论文
共 50 条
  • [41] OXIDATION AND OXIDATION PROTECTION OF ND-FE-B MAGNETS
    KIM, AS
    JACOBSON, JM
    IEEE TRANSACTIONS ON MAGNETICS, 1987, 23 (05) : 2509 - 2511
  • [42] OXIDATION BEHAVIOR OF ND-FE-B MAGNETS
    JACOBSON, J
    KIM, A
    JOURNAL OF APPLIED PHYSICS, 1987, 61 (08) : 3763 - 3765
  • [43] Corrosion behaviour of Nd-Fe-B permanent magnets
    Mummert, K
    El-Aziz, AM
    Barkleit, G
    Rodewald, W
    Schultz, L
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2000, 51 (01): : 13 - 19
  • [44] ON THE TEXTURE OF ND-FE-B PERMANENT-MAGNETS
    ZHENG, CH
    FU, T
    ZENG, XY
    JOURNAL OF THE LESS-COMMON METALS, 1990, 159 (1-2): : 69 - 74
  • [45] Degradation processes in Nd-Fe-B permanent magnets
    Hrivnáková, D
    Hrnciar, V
    Caplovic, L
    KOVOVE MATERIALY-METALLIC MATERIALS, 2000, 38 (03): : 188 - 197
  • [46] THE ND-FE-B MATERIALS FOR PERMANENT-MAGNETS
    HIROSAWA, S
    TSUBOKAWA, Y
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1990, 84 (03) : 309 - 316
  • [47] Temperature characteristics of Nd-Fe-B permanent magnets
    Nagata, H.
    Makita, K.
    Hirosawa, S.
    Sagawa, M.
    IEEE translation journal on magnetics in Japan, 1988, 3 (06): : 430 - 431
  • [48] The development of Nd-Fe-B permanent magnets for automobile
    Tomizawa, Hiroyuki
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2005, 52 (03): : 158 - 163
  • [49] Anisotropic exchange in Nd-Fe-B permanent magnets
    Gong, Qihua
    Yi, Min
    Evans, Richard F. L.
    Gutfleisch, Oliver
    Xu, Bai-Xiang
    MATERIALS RESEARCH LETTERS, 2020, 8 (03): : 89 - 96
  • [50] SINTERED ND-FE-B PERMANENT-MAGNETS
    HIGUCHI, A
    HIROSAWA, S
    IEEE TRANSACTIONS ON MAGNETICS, 1989, 25 (05) : 3555 - 3560