摘要
When some of the iron in the B2 iron aluminide Fe-45 at.% Al is replaced by nickel, several important changes occur. Nickel dramatically slows down the removal of quenched-in thermal vacancies during annealing. Also, nickel additions render the hardening due to thermal vacancies less effective than that in binary iron aluminides. Both of these effects may be linked to the formation of nickel-vacancy complexes. Nickel additions also cause substantial solid solution strengthening, and possible reasons for this result are discussed. Our findings are supported by vacancy concentration determinations, by yield strength measurements, and by transmission electron microscope observations. (C) 1997 Elsevier Science S.A.
引用
收藏
页码:245 / 250
页数:6
相关论文
共 50 条
  • [21] THE CHEMISTRY OF NICKEL-CONTAINING ENZYMES
    KOLODZIEJ, AF
    PROGRESS IN INORGANIC CHEMISTRY, VOL 41, 1994, 41 : 493 - 597
  • [22] A combined electrochemical and xps study on the passivity of B2 iron aluminides in sulphuric acid solution
    Frangini, S
    DeCristofaro, NB
    Mignone, A
    Lascovich, J
    Giorgi, R
    CORROSION SCIENCE, 1997, 39 (08) : 1431 - 1442
  • [23] The strength properties of iron aluminides
    Yoshimi, K
    Hanada, S
    JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1997, 49 (08): : 46 - 49
  • [24] The strength properties of iron aluminides
    Kyosuke Yoshimi
    Shuji Hanada
    JOM, 1997, 49 : 46 - 49
  • [25] NICKEL ALLERGY AND NICKEL-CONTAINING DENTAL ALLOYS
    MAGNUSSON, B
    BERGMAN, M
    BERGMAN, B
    SOREMARK, R
    SCANDINAVIAN JOURNAL OF DENTAL RESEARCH, 1982, 90 (02): : 163 - 167
  • [26] Ideal tensile strength of B2 transition-metal aluminides -: art. no. 054107
    Li, TS
    Morris, JW
    Chrzan, DC
    PHYSICAL REVIEW B, 2004, 70 (05) : 054107 - 1
  • [27] Reducing Roasting of Hematite Laterite Nickel Ores with the Formation of Granulated Nickel-Containing Cast Iron
    G. B. Sadykhov
    K. G. Anisonyan
    K. V. Goncharov
    D. Yu. Kop’ev
    T. V. Olyunina
    A. B. Mikhailova
    Russian Metallurgy (Metally), 2019, 2019 : 659 - 664
  • [28] Theoretical calculation of elastic properties and electronic structure of B2 iron aluminides and ternary iron-aluminum alloys
    Chen Yu
    Yao Zheng-Jun
    Zhang Ping-Ze
    Luo Xi-Xi
    MATERIALS RESEARCH EXPRESS, 2019, 6 (12)
  • [29] Study of Factors Affecting the Strength of Briquettes Made of Aluminum and Nickel-Containing Slags
    Al-Saraireh, Falah Mustafa
    METALLURGICAL & MATERIALS ENGINEERING, 2024, 30 (03) : 94 - 102
  • [30] Reducing Roasting of Hematite Laterite Nickel Ores with the Formation of Granulated Nickel-Containing Cast Iron
    Sadykhov, G. B.
    Anisonyan, K. G.
    Goncharov, K. V.
    Kop'ev, D. Yu.
    Olyunina, T. V.
    Mikhailova, A. B.
    RUSSIAN METALLURGY, 2019, 2019 (07): : 659 - 664