Precipitation formation on Σ5 and Σ7 grain boundaries in 316L stainless steel and their roles on intergranular corrosion

被引:40
|
作者
Tsai, Shao-Pu [1 ]
Makineni, Surendra Kumar [1 ,4 ]
Gault, Baptiste [1 ,2 ]
Kawano-Miyata, Kaori [3 ]
Taniyama, Akira [3 ]
Zaefferer, Stefan [1 ]
机构
[1] Max Planck Inst Eisenforsch GmbH, Max Planck Str 1, D-40237 Dusseldorf, Germany
[2] Imperial Coll London, Royal Sch Mines, Dept Mat, London SW7 2AZ, England
[3] Nippon Steel Corp Ltd, Res & Dev, 1-8 Fuso Cho, Amagasaki, Hyogo 6600891, Japan
[4] Indian Inst Sci, Dept Mat Engn, Bangalore 560012, Karnataka, India
关键词
Stainless steel; Coincidence site lattice (CSL); Faceting; GB energy anisotropy; CARBIDE PRECIPITATION; CHARACTER-DISTRIBUTION; CHROMIUM DEPLETION; M23C6; CARBIDE; LAVES PHASE; BEHAVIOR; SEGREGATION; SERRATION; ENERGIES; SENSITIZATION;
D O I
10.1016/j.actamat.2021.116822
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In sensitized (700 degrees C for 10 h) AISI 316L stainless steel samples attacked by an HF solution, coincidence site lattice (CSL) Sigma 7 grain boundaries (GBs) always show corrosion while Sigma 5 GBs never do. This distinct corrosion behaviour can be related to the distinct precipitation behaviour of the different GBs, which itself depends on the GB characters. It is found that Sigma 5 GBs, although being curved both macro- and microscopically, neither show facets nor precipitates. The amount of segregation is enhanced in sensitized Sigma 5 GBs compared to solution-annealed ones. In contrast, Sigma 7 GBs show clear faceting in both the solution-annealed and sensitized state, with one facet orientation showing strong segregation while the other not. GB energy anisotropy is applied to explain the faceting phenomenon. The formation of two kinds of precipitates, i.e., C14 Laves phase and M23C6 carbide, holding responsible for two distinct morphologies of corrosion, are believed to be both linked to intensive faceting and the anisotropic segregation of Sigma 7 GBs. For the carbide, a preferred {111} orientation out of all Sigma 7 facets measured by trace analyses is presumed to facilitate its nucleation. (C) 2021 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页数:15
相关论文
共 50 条
  • [21] Determination of susceptibility to intergranular corrosion and electrochemical reactivation behaviour of AISI 316L type stainless steel
    Aydogdu, G. H.
    Aydinol, M. K.
    CORROSION SCIENCE, 2006, 48 (11) : 3565 - 3583
  • [22] Investigation of intergranular corrosion of 316L stainless steel diffusion bonded joint by electrochemical potentiokinetic reactivation
    Li, Shu-Xin
    Li, Lei
    Yu, Shu-Rong
    Akid, R.
    Xia, Hong-Bo
    CORROSION SCIENCE, 2011, 53 (01) : 99 - 104
  • [23] On the unusual intergranular corrosion resistance of 316L stainless steel additively manufactured by selective laser melting
    Laleh, Majid
    Hughes, Anthony E.
    Xu, Wei
    Haghdadi, Nima
    Wang, Ke
    Cizek, Pavel
    Gibson, Ian
    Tan, Mike Yongjun
    CORROSION SCIENCE, 2019, 161
  • [24] Structural analysis and intergranular corrosion tests of AISI 316L steel
    Stonawska, Z.
    Svoboda, M.
    Sozanska, M.
    Kristkova, M.
    Sojka, J.
    Dagbert, C.
    Hyspecka, L.
    JOURNAL OF MICROSCOPY-OXFORD, 2006, 224 (01): : 62 - 64
  • [26] On Grain Boundary Engineering for a 316L Austenitic Stainless Steel
    Dolzhenko, Pavel
    Tikhonova, Marina
    Odnobokova, Marina
    Kaibyshev, Rustam
    Belyakov, Andrey
    METALS, 2022, 12 (12)
  • [27] Recrystallization and Grain Growth of 316L Stainless Steel Wires
    Xiuyun Zhao
    Yong Liu
    Yan Wang
    Ping Feng
    Huiping Tang
    Metallurgical and Materials Transactions A, 2014, 45 : 3446 - 3453
  • [28] Recrystallization and Grain Growth of 316L Stainless Steel Wires
    Zhao, Xiuyun
    Liu, Yong
    Wang, Yan
    Feng, Ping
    Tang, Huiping
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (08): : 3446 - 3453
  • [29] Grain boundary networks in AISI 316L stainless steel
    Gertsman, VY
    Janecek, M
    Tangri, K
    PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1996, 157 (02): : 241 - 247
  • [30] Grain growth behaviour of type 316L stainless steel
    Kashyap, B.P.
    Tangri, K.
    Materials Science and Engineering A, 1992, A149 (02)