Physical and electrical characterization of WN Schottky contacts on 4H-SiC

被引:6
|
作者
Noblanc, O
Arnodo, C
Cassette, S
Brylinski, C
Kakanakova-Georgieva, A
Marinova, T
Kassamakova, L
Kakanakov, R
Pecz, B
Sulyok, A
Radnoczi, G
机构
[1] Thomson CSF, LCR, F-91404 Orsay, France
[2] Bulgarian Acad Sci, IGIC, BG-1113 Sofia, Bulgaria
[3] Inst Appl Phys, BG-4000 Plovdiv, Bulgaria
[4] Hungarian Acad Sci, RITP, H-1325 Budapest, Hungary
关键词
WN; Schottky rectifier; TEM; XPS;
D O I
10.4028/www.scientific.net/MSF.264-268.817
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
WN has been deposited by reactive sputtering on 4H-SiC to make Schottky rectifiers. The physical properties of the interface have I,een studied by XPS and TEM for as-deposited, 800 and 1200 degrees C annealed samples. The two former. samples reveal steep interface with a metallic layer made of W and W2N phases. No dissociation of the SiC is evidenced in these conditions. In the later one, tungsten silicide and tungsten carbide are evidenced. The rectifying properties are studied by I(V) measurements. Barrier height of 0.94 eV is measured for annealed samples up to 950 degrees C and thermal stability is observed up to 350 degrees C.
引用
收藏
页码:817 / 820
页数:4
相关论文
共 50 条
  • [1] Physical and electrical characterization of WN Schottky contacts on 4H-SiC
    Noblanc, O.
    Arnodo, C.
    Cassette, S.
    Brylinski, C.
    Kakanakova-Georgieva, A.
    Marinova, Ts.
    Kassamakova, L.
    Kakanakov, R.
    Pecz, B.
    Sulyok, A.
    Radnoczi, G.
    Materials Science Forum, 1998, 264-268 (pt 2): : 817 - 820
  • [2] Electrical characterization of inhomogeneous Ti/4H-SiC Schottky contacts
    Defives, D
    Noblanc, O
    Dua, C
    Brylinski, C
    Barthula, M
    Meyer, F
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 1999, 61-2 : 395 - 401
  • [3] Electrical characterization of 4H-SiC Schottky diodes with a RuO2 and a RuWOx Schottky contacts
    Buc, Dalibor
    Stuchlikova, Lubica
    Harmatha, Ladislav
    Hotovy, Ivan
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2008, 19 (8-9) : 783 - 787
  • [4] Electrical and ultraviolet characterization of 4H-SiC Schottky photodiodes
    Lioliou, G.
    Mazzillo, M. C.
    Sciuto, A.
    Barnett, A. M.
    OPTICS EXPRESS, 2015, 23 (17): : 21657 - 21670
  • [5] Electrical behaviour and microstructural analysis of metal Schottky contacts on 4H-SiC
    Defives, D
    Durand, O
    Wyczisk, F
    Noblanc, O
    Brylinski, C
    Meyer, F
    MICROELECTRONIC ENGINEERING, 2001, 55 (1-4) : 369 - 374
  • [6] Electrical characteristics of Schottky contacts on Ge-doped 4H-SiC
    Vivona, M.
    Alassaad, K.
    Souliere, V.
    Giannazzo, F.
    Roccaforte, F.
    Ferro, G.
    SILICON CARBIDE AND RELATED MATERIALS 2013, PTS 1 AND 2, 2014, 778-780 : 706 - +
  • [7] Electrical characterization of 4H-SiC Schottky diodes with RuWOx Schottky contacts before and after irradiation by fast electrons
    Benkovska, Jana
    Stuchlikova, Lubica
    Buc, Dalibor
    Caplovic, Lubomir
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2012, 209 (07): : 1384 - 1389
  • [8] Cr/4H-SiC Schottky contacts investigated by electrical and photoelectron spectroscopy techniques
    Koliakoudakis, C.
    Dontas, J.
    Karakalos, S.
    Kayambaki, M.
    Ladas, S.
    Konstantinidis, G.
    Zekentes, K.
    Kennou, S.
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2008, 205 (11): : 2536 - 2540
  • [9] Tungsten and tungsten nitride Schottky contacts to 4H-SiC
    Pecz, B
    Sulyok, A
    Radnoczi, G
    Noblanc, O
    Arnodo, C
    Cassette, S
    Brylinski, C
    MICROSCOPY OF SEMICONDUCTING MATERIALS 1997, 1997, (157): : 519 - 522
  • [10] Thermal stability of Pt Schottky contacts to 4H-SiC
    Shalish, I
    de Oliveira, CEM
    Shapira, Y
    Burstein, L
    Eizenberg, M
    JOURNAL OF APPLIED PHYSICS, 2000, 88 (10) : 5724 - 5728