Tensile and Fracture Properties of Cast and Forged Composite Synthesized by Addition of Al-Si Alloy to Magnesium

被引:7
|
作者
Swamy, H. M. Nanjunda [1 ]
Nath, S. K. [1 ]
Ray, S. [1 ]
机构
[1] Indian Inst Technol, Dept Met & Mat Engn, Roorkee 247667, Uttar Pradesh, India
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2009年 / 40A卷 / 13期
关键词
METAL-MATRIX COMPOSITE; MECHANICAL-BEHAVIOR; GRAIN-REFINEMENT; TOUGHNESS; PARAMETERS; ALUMINUM;
D O I
10.1007/s11661-009-0010-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Cast Mg-Al-Si composites synthesized by addition of Al-Si alloy containing 10, 15, and 20 wt pct of Si, in molten magnesium, to generate particles of Mg(2)Si by reaction between silicon and magnesium during stir casting has opened up the possibility to control the size of these particles. The microstructure of the cast composite consists of relatively dark polyhedral phase of Mg(2)Si and bright phase of beta-Al(12)Mg(17) along the boundary between dendrites of alpha-Mg solid solution. After hot forging at 350 degrees C, the microstructure has changed to relatively smaller sizes of beta-Al(12)Mg(17) and Mg(2)Si particles apart from larger grains surrounded by smaller grains due to dynamic recovery and recrystallization. Some of the Mg(2)Si particles crack during forging. In both the cast and forged composite, the Brinell hardness increases rapidly with increasing volume fraction of Mg(2)Si, but the hardness is higher in forged composites by about 100 BHN. Yield strength in cast composites improves over that of the cast alloy, but there is a marginal increase in yield strength with increasing Mg(2)Si content. In forged composites, there is significant improvement in yield strength with increasing Mg(2)Si particles and also over those observed in their cast counterpart. In cast composites, ultimate tensile strength (UTS) decreases with increasing Mg(2)Si content possibly due to increased casting defects such as porosity and segregation, which increases with increasing Mg(2)Si content and may counteract the strengthening effect of Mg(2)Si content. However, in forged composite, UTS increases with increasing Mg(2)Si content until 5.25 vol pct due to elimination of segregation and lowering of porosity, but at higher Mg(2)Si content of 7 vol pct, UTS decreases, possibly due to extensive cracking of Mg(2)Si Particles. On forging, the ductility decreases in forged alloy and composites possibly due to the remaining strain and the forged microstructure. The initiation fracture toughness, J(IC), decreases drastically in cast composites from that of Mg-9 wt pct. alloy designated as MA alloy due to the presence Mg(2)Si particles. Thereafter, JIC does not appear to be very sensitive to the increasing presence of Mg(2)Si particles. There is drastic reduction of JIC on forging of the alloy, which was attributed to the remaining strain and forged microstructure, and it is further lowered in the composites because of cracking of Mg(2)Si particles. The ratio of the tearing modulus to the elastic modulus in cast composites shows a lower ratio, which decreases with increasing Mg(2)Si content. The ratio decreases comparatively more on forging of cast MA alloy than those observed in forged composites.
引用
收藏
页码:3284 / 3293
页数:10
相关论文
共 50 条
  • [41] Improvement of Al-Si Hypoeutectic Cast Alloy Properties by Forging with Grain Refiner and Modifier
    Kumar, D. T. Arun
    Kumar, K. G. Basava
    Pattanaik, A.
    Mukherjee, M.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2020, 73 (12) : 3105 - 3112
  • [42] MECHANICAL PROPERTIES OF CAST HYPOEUTECTIC AL-SI ALLOY IN HEXACHLOROETHANE-COATED MOULD
    Shittu, M. D.
    Ibitoye, S. A.
    Olawale, J. O.
    JOURNAL OF ENGINEERING SCIENCE AND TECHNOLOGY, 2012, 7 (04): : 529 - 539
  • [43] Corrosion resistance and superhydrophobic properties of organic hybrid coating on cast Al-Si alloy
    Huang, Xuelin
    Yu, Liang
    Dong, Yinsheng
    PROGRESS IN ORGANIC COATINGS, 2020, 139
  • [44] Changes in microstructure and mechanical properties of cast Al-Si alloy due to hot rolling
    Toyama K.
    Matsuura K.
    Ohno M.
    Sato T.
    Nakayama M.
    Keikinzoku/Journal of Japan Institute of Light Metals, 2010, 60 (01): : 7 - 11
  • [45] Understanding the Effect of Be Addition on the Microstructure and Tensile Properties of Al–Si–Mg Cast Alloys
    E. A. Elsharkawi
    M. F. Ibrahim
    A. M. Samuel
    H. W. Doty
    F. H. Samuel
    International Journal of Metalcasting, 2022, 16 : 1777 - 1795
  • [46] Study on microstructure and mechanical properties of cast Al-Si alloy in lost form process
    Wu, Xian-Ming
    Wu, Wei-Gang
    Zhuzao/Foundry, 2007, 56 (04): : 369 - 371
  • [47] Improvement of mechanical properties of a cast Al-Si base alloy by friction stir processing
    Tsai, F. Y.
    Kao, P. W.
    MATERIALS LETTERS, 2012, 80 : 40 - 42
  • [48] Estimation of porosity and shrinkage in a cast eutectic Al-Si alloy
    Samavedam, S.
    Sakri, S. B.
    Rao, D. Hanumantha
    Sundarrajan, S.
    CANADIAN METALLURGICAL QUARTERLY, 2014, 53 (01) : 55 - 64
  • [49] REFINEMENT OF CAST STRUCTURES OF AL-SI ALLOY INGOTS BY RHEOCASTING
    ARAKANE, G
    TAKAMORI, S
    OHSAWA, Y
    SATO, A
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1995, 59 (05) : 559 - 563
  • [50] MICROSTRUCTURE AND WEAR OF CAST (AL-SI ALLOY) GRAPHITE COMPOSITES
    DAS, S
    PRASAD, SV
    RAMACHANDRAN, TR
    WEAR, 1989, 133 (01) : 173 - 187