The evolution of deformation substructure in a creep deformed fully-lamellar TiAl alloy

被引:23
|
作者
Hsiung, LM [1 ]
Nieh, TG [1 ]
机构
[1] Univ Calif Lawrence Livermore Natl Lab, Livermore, CA 94551 USA
关键词
creep deformation; deformation substructure; primary creep stage; interfacial dislocation; interface sliding; secondary creep stage; deformation twinning;
D O I
10.1016/S0921-5093(97)00614-X
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The evolution of deformation substructure in a powder metallurgy (P/M) TIAl alloy creep deformed at 760 degrees C has been examined using transmission electron microscopy. Since the multiplication of lattice dislocations within gamma lamellae becomes limited as a result of a refined fully-lamellar (FL) microstructure (i.e. refined lamellar spacing) within the PIM TiAl alloy, the deformation of the alloy at the primary creep stage is mainly accommodated by soft lamellar grains through the movement of interfacial dislocations in the gamma-alpha(2) and gamma-gamma interfaces. The mobility of interfacial dislocations is primarily impeded by grain boundaries, interface ledges and dislocation barriers formed by the impingement of lattice dislocations to the lamellar interfaces. When the alloy is deformed into the secondary creep stage, the density of interfacial dislocations increases and deformation twins nucleate and grow from the lamellar interfaces. It is suggested that deformation twinning in FL-TiAl results from a stress-relief process due to the pile-up of interfacial dislocations during deformation. The alloy becomes more resistant to creep deformation as a result of the deformation twinning because the deformation twins further restrict the dislocation motion within the gamma lamellae, and the formation of sessile dislocations at the intersections between the deformation twins and the gamma or alpha(2) lamellae provides effective barriers for the movement of interfacial dislocations. (C) 1997 Elsevier Science S.A.
引用
收藏
页码:438 / 444
页数:7
相关论文
共 50 条
  • [1] The role of interfacial substructure in the creep deformation of a fully-lamellar TiAl alloy
    Hsiung, LM
    Nieh, TG
    STRUCTURAL INTERMETALLICS 1997, 1996, : 129 - 136
  • [2] Substructure in a creep deformed lamellar Tial alloy
    Hsiung, LM
    Nieh, TG
    SCRIPTA MATERIALIA, 1997, 36 (03) : 323 - 330
  • [3] Microstructural characterization of creep cavitation in a fully-lamellar TiAl alloy
    Du, XW
    Zhu, J
    Kim, YW
    INTERMETALLICS, 2001, 9 (02) : 137 - 146
  • [4] Formation of the creep-induced β2 phase and its influence on deformation in a fully-lamellar TiAl alloy
    Du, XW
    Zhu, J
    Zhang, X
    Cheng, ZY
    Kim, YW
    INTERMETALLICS, 2001, 9 (03) : 181 - 187
  • [5] Creep induced α2→β2 phase transformation in a fully-lamellar TiAl alloy
    Du, XW
    Zhu, J
    Zhang, X
    Cheng, ZY
    Kim, YW
    SCRIPTA MATERIALIA, 2000, 43 (07) : 597 - 602
  • [6] In situ observation of deformation-induced interface migration in a fully-lamellar TiAl alloy
    Hsiung, LM
    Schwartz, AJ
    Nieh, TG
    SCRIPTA MATERIALIA, 1997, 36 (09) : 1017 - 1022
  • [7] Creep crack growth in nearly fully-lamellar gamma TiAl alloys
    Jata, K.V.
    Kim, Y.-W.
    Key Engineering Materials, 2000, 171-174 : 147 - 152
  • [8] Creep crack growth in nearly fully-lamellar gamma TiAl alloys
    Jata, KV
    Kim, YW
    CREEP AND FRACTURE OF ENGINEERING MATERIALS AND STRUCTURES, 2000, 171-1 : 147 - 152
  • [9] A model of creep based on interacting elements and its application to the primary creep of fully-lamellar γ-TiAl
    Daehn, GS
    Viswanathan, GB
    Mills, MJ
    Vasudevan, VK
    CREEP BEHAVIOR OF ADVANCED MATERIALS FOR THE 21ST CENTURY, 1999, : 31 - 40
  • [10] Observations on the creep behavior of fully-lamellar polycrystalline TiAl: Identification of critical effects
    Parthasarathy, TA
    Mendiratta, MG
    Dimiduk, DM
    SCRIPTA MATERIALIA, 1997, 37 (03) : 315 - 321