共 50 条
- [1] Creep crack growth in nearly fully-lamellar gamma TiAl alloys CREEP AND FRACTURE OF ENGINEERING MATERIALS AND STRUCTURES, 2000, 171-1 : 147 - 152
- [2] Crack growth in a nearly fully-lamellar gamma TiAl alloy at 650°C and 800°C under sustained load GAMMA TITANIUM ALUMINIDES 1999, 1999, : 509 - 516
- [3] Crack growth in a nearly fully-lamellar gamma TiAl alloy at 650 °C and 800 °C under constant load conditions METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2002, 33 (09): : 2847 - 2857
- [4] Crack growth in a nearly fully-lamellar gamma TiAl alloy at 650 °C and 800 °C under constant load conditions Metallurgical and Materials Transactions A, 2002, 33 : 2847 - 2857
- [6] Microstructure and creep strength of fully-lamellar TiAl alloys containing beta-phase MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 329 : 802 - 809
- [8] Ultrafine fully-lamellar structures in two-phase gamma-TiAl alloys HIGH-TEMPERATURE ORDERED INTERMETALLIC ALLOYS VII, 1997, 460 : 219 - 223
- [9] The evolution of deformation substructure in a creep deformed fully-lamellar TiAl alloy MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 240 : 438 - 444
- [10] The role of interfacial substructure in the creep deformation of a fully-lamellar TiAl alloy STRUCTURAL INTERMETALLICS 1997, 1996, : 129 - 136