Developments of high strength Bi-containing Sn0.7Cu lead-free solder alloys prepared by directional solidification

被引:69
|
作者
Hu, Xiaowu [1 ]
Li, Yulong [1 ]
Liu, Yi [2 ]
Min, Zhixian [3 ]
机构
[1] Nanchang Univ, Sch Mech Elect Engn, Nanchang 330031, Peoples R China
[2] Nanchang Univ, Sch Mat Sci & Engn, Nanchang 330031, Peoples R China
[3] China Elect Technology Grp Corp, Res Inst 38, Hefei 230088, Peoples R China
关键词
Lead-free solder; Cu6Sn5; fiber; Microstructure; Directional solidification; Tensile properties; MECHANICAL-PROPERTIES; CU SUBSTRATE; SN-AG; MICROSTRUCTURE; BEHAVIOR; GROWTH; JOINT; NI;
D O I
10.1016/j.jallcom.2014.10.205
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Bi-containing Sn0.7Cu (SC) eutectic solder alloys were prepared and subjected to directional solidification, through which new types of fiber reinforced eutectic composites were generated. The influences of Bi addition on the microstructures and tensile properties of directionally solidified (DS) Bi-containing eutectic SC lead-free solder alloys have been investigated by using differential scanning calorimetry (DSC), scanning electron microscopy (SEM), energy dispersive spectrometry (EDS) and a tensile testing machine. The experimental results showed that addition of Bi could effectively reduce both the melting temperature and undercooling of SC solder alloy. The microstructures of DS SC-xBi solder alloys were composed of Sn-rich phase (beta) and Cu6Sn5 fiber. No other intermetallic compounds (IMCs) with Bi content were observed in the solder matrix for SC solder alloys with various Bi contents. Both fiber spacing and diameter all decreased gradually with increasing growth rate and/or Bi content. Besides, the regularity of Cu6Sn5 fibers alignment also decreased with increasing growth rate, too. The tensile strengths of the SC-xBi eutectic solder alloys varied parabolically with growth rate (R). When R was 60 mu m/s, maximum tensile strengths of 43.8, 55.2 and 56.37 MPa were reached for SC, SC0.7Bi and SC1.3Bi solder alloys. A comparison of tensile strength of SC, SC0.7Bi and SC1.3Bi with the same R indicated that the tensile strength increased with increasing Bi content, which was attributed to the presence of Bi and its role in refining microstructure and solid solution strengthening. (C) 2014 Elsevier B. V. All rights reserved.
引用
收藏
页码:241 / 250
页数:10
相关论文
共 50 条
  • [21] Electroplating of lead-free solder alloys composed of Sn-Bi, Sn-Ag, and Sn-Cu
    Yanada, Isamu
    Gudeczauskas, Donald
    Proceedings of the AESF Annual Technical Conference, 1999, : 457 - 468
  • [22] Microstructure and tensile properties of Sn-1Cu lead-free solder alloy produced by directional solidification
    Hu, Xiaowu
    Chen, Wenjing
    Wu, Bin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 556 : 816 - 823
  • [23] Microstructures and properties of Sn-Ag-Cu lead-free solder alloys containing La
    Zhou Ying-chun
    Pan Qing-lin
    He Yun-bin
    Liang Wen-jien
    Li Wen-bin
    Li Yun-chun
    Lu Cong-ge
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2007, 17 : S1043 - S1048
  • [24] Interfacial reaction and IMC growth between Bi-containing Sn0.7Cu solders and Cu substrate during soldering and aging
    Hu, Xiaowu
    Li, Yulong
    Min, Zhixian
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 582 : 341 - 347
  • [25] Microstructures and properties of Sn-Ag-Cu lead-free solder alloys containing La
    周迎春
    潘清林
    何运斌
    梁文杰
    李文斌
    李运春
    路聪阁
    Transactions of Nonferrous Metals Society of China, 2007, (S1) : 1043 - 1048
  • [26] Solidification Mechanisms in the Sn-Cu-Ni Lead-Free Solder System
    Ventura, Tina
    Cho, Younghee
    Dahle, Arne K.
    PRICM 7, PTS 1-3, 2010, 654-656 : 1381 - 1384
  • [27] Stabilisation of Cu6Sn5 by Ni in Sn-0.7Cu-0.05Ni lead-free solder alloys
    Nogita, Kazuhiro
    INTERMETALLICS, 2010, 18 (01) : 145 - 149
  • [28] Thermodynamic analysis and characterization of Bi–Cu–Sn alloys as advanced lead-free solder materials for high temperature application
    Dragana Živković
    Duško Minić
    Dragan Manasijević
    Nadežda Talijan
    Iwao Katayama
    Ana Kostov
    Journal of Materials Science: Materials in Electronics, 2011, 22 : 1130 - 1135
  • [29] Solidification Condition Effects on Microstructures and Creep Resistance of Sn-3.8Ag-0.7Cu Lead-Free Solder
    J. Liang
    N. Dariavach
    D. Shangguan
    Metallurgical and Materials Transactions A, 2007, 38 : 1530 - 1538
  • [30] A high-performance lead-free solder - the effects of In on 99.3Sn/0.7Cu
    Hwang, JS
    Guo, ZF
    Koenigsmann, H
    SOLDERING & SURFACE MOUNT TECHNOLOGY, 2001, 13 (02) : 7 - 13