Characterisation of a new plasma-enhanced film to improve shear bond strength between zirconia and veneering ceramic

被引:23
|
作者
Bitencourt, Sandro B. [1 ]
dos Santos, Daniela M. [1 ]
da Silva, Emily V. F. [1 ]
Barao, Valentim A. R. [2 ]
Rangel, Elidiane C. [3 ]
da Cruz, Nilson C. [3 ]
de Souza, Grace M. [4 ]
Goiato, Marcelo C. [1 ]
Pesqueira, Aldieris A. [1 ]
机构
[1] Univ Estadual Paulista UNESP, Aracatuba Dent Sch, Dept Dent Mat & Prosthodont, R Jose Bonifacio 1193, BR-16015050 Aracatuba, SP, Brazil
[2] Univ Campinas UNICAMP, Piracicaba Dent Sch, Dept Prosthodont & Periodontol, Ave Limeira 901, BR-13414903 Piracicaba, SP, Brazil
[3] Univ Estadual Paulista UNESP, ICTS, Lab Technol Plasmas, Ave Tres de Marco 511, BR-18087180 Sorocaba, SP, Brazil
[4] Univ Toronto, Fac Dent, Dept Clin Sci, 124 Edward St, Toronto, ON M5G 1G6, Canada
基金
巴西圣保罗研究基金会;
关键词
Ceramics; Y-TZP ceramic; Shear bond strength; Aluminum oxide; Zirconium oxide; Fracture strength; Y-TZP; SURFACE CHARACTERIZATION; DENTAL CERAMICS; PORCELAIN; ADHESION; RESTORATIONS; INTERFACE; CORES; RESIN; METAL;
D O I
10.1016/j.msec.2018.06.052
中图分类号
TB3 [工程材料学]; R318.08 [生物材料学];
学科分类号
0805 ; 080501 ; 080502 ;
摘要
The aim of this study was to develop and characterise a new plasma-enhanced chemical vapor deposition (PECVD) film for improving shear bond strength (SBS) between yttria-stabilised tetragonal zirconia (Y-TZP) and veneering ceramic. In total, 192 Y-TZP samples (13 x 5.4 x 5 mm) were divided into 6 groups: control - no treatment (C), airborne-particle abrasion with 27 mu m aluminum oxide particles (Al-27), 110 mu m aluminum oxide particles (Al-110), and 250 mu m aluminum oxide particles (Al-250, application of liner for zirconia (L) and the PECVD film application (P). The Y-TZP surface was characterised by means of Scanning Electronic Microscopy (SEM), Energy-dispersive Spectroscopy (EDS), atomic force microscopy (AFM), surface profilometry and surface free energy (SFE). SBS between Y-TZP and veneering ceramic was tested before and after thermocycling (20,000 cycles of 5 and 55 degrees C), and failure mode was also evaluated. Data were analysed by ANOVA and Tukey's HSD test (alpha = 0.05). Data analysis showed that PECVD film had no effect on surface roughness of Y-TZP (p > 0.05 vs control), whilst the other groups presented higher roughness values (p < 0.05). All treatments increased SFE, except the Al-27 group. The highest SBS was presented by the P group (p < 0.05), and values were similar to those of the Al-27 group (p = 0.107). Mixed failures were prevalent in all groups, and premature failures were found only in Al groups after thermocycling. Whilst PECVD treatment did not affect Y-TZP surface roughness, high SBS between Y-TZP and the veneering layer was observed. Therefore, PECVD treatment is a promising alternative to improve the performance of bi-layer zirconia-based restorations.
引用
下载
收藏
页码:196 / 205
页数:10
相关论文
共 50 条
  • [21] Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites
    Fischer, Jens
    Stawarzcyk, Bogna
    Trottmann, Albert
    Haemmerle, Christoph H. F.
    DENTAL MATERIALS, 2009, 25 (04) : 419 - 423
  • [22] Effect of coloring liquids on color of zirconia frameworks bond strength of zirconia/veneering ceramic
    Celik, Selin
    Ucar, Yurdanur
    Ekren, Orhun
    JOURNAL OF PROSTHETIC DENTISTRY, 2020, 124 (01): : 110 - 115
  • [23] The effect of repair protocols on shear bond strength to zirconia and veneering porcelain
    Uzun, Ismail Hakki
    Malkoc, Meral Arslan
    Polat, Nilufer Tulin
    Ogreten, Ayse Tuba
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2016, 30 (16) : 1741 - 1753
  • [24] Effect of Various Surface Treatments on the Bond Strength Between Composite Resin and Zirconia Veneering Ceramic
    Joen, Jin Yong
    Choe, Han Cheol
    Chung, Chae Heon
    Kang, Dong Wan
    Son, Mee Kyoung
    SCIENCE OF ADVANCED MATERIALS, 2015, 7 (01) : 57 - 62
  • [25] Correlation between Surface Roughness and Shear Bond Strength in Zirconia Veneering Ceramics: a Preliminary Report
    Gasparic, Lana Bergman
    ACTA STOMATOLOGICA CROATICA, 2013, 47 (01) : 45 - 50
  • [26] The Effect of Selective Infiltration Etching (SIE) Associated with Zirconia Nanoparticles on the Shear Bond Strength of Zirconia Core/Veneering Ceramic in Dentistry
    Park, Da-Ryeong
    Uhm, Soo-Hyuk
    Kim, Kyung-Nam
    Bae, Ji-Myung
    Kim, Jeong-Mi
    Jung, Soo-Ha
    Kim, Jae-Hong
    Oh, Seunghan
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2016, 16 (11) : 11957 - 11963
  • [27] Effect of Nonthermal Plasma on Shear Bond Strength of Translucent Zirconia in Layering Ceramic
    Seyedi, Dorsa
    Valizadeh, Sara
    Ghodsi, Safoura
    Salimi, Kimia
    Atri, Faezeh
    INTERNATIONAL JOURNAL OF DENTISTRY, 2023, 2023
  • [28] Effect of alternative sonochemical treatment on zirconia surface and bond strength with veneering ceramic
    Bastos, Natalia Almeida
    Lisboa-Filho, Paulo Noronha
    Tabata, Americo
    Silveira Francisconi, Paulo Afonso
    Furuse, Adilson Yoshio
    Honorio, Heitor Marques
    Sanches Borges, Ana Flavia
    MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2020, 252 (252):
  • [29] The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic
    Chaiyabutr, Yada
    McGowan, Steve
    Phillips, Keith M.
    Kois, John C.
    Giordano, Russell A.
    JOURNAL OF PROSTHETIC DENTISTRY, 2008, 100 (03): : 194 - 202
  • [30] Zirconia Primers Improve the Shear Bond Strength of Dental Zirconia
    Steiner, Rene
    Heiss-Kisielewsky, Irene
    Schwarz, Vincent
    Schnabl, Dagmar
    Dumfahrt, Herbert
    Laimer, Johannes
    Steinmassl, Otto
    Steinmassl, Patricia-Anca
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2020, 29 (01): : 62 - 68