Investigation on Wear Behavior of Cryogenically Treated Ti-6Al-4V Titanium Alloy under Dry and Wet Conditions

被引:18
|
作者
Li, Yonggang [1 ,2 ]
Wang, Xingfu [1 ]
Yang, Shengqiang [1 ]
Hou, Lifeng [3 ]
Wei, Yinghui [3 ]
Zhang, Zhongjie [1 ]
Yang, Xiaoni [4 ]
机构
[1] Taiyuan Univ Technol, Coll Mech & Vehicle Engn, Taiyuan 030024, Shanxi, Peoples R China
[2] Taiyuan Heavy Machinery Grp Co Ltd, Taiyuan 030024, Shanxi, Peoples R China
[3] Taiyuan Univ Sci & Technol, Coll Mat Sci & Engn, Taiyuan 030024, Shanxi, Peoples R China
[4] Taiyuan Univ Technol, Coll Water Resources Sci & Engn, Taiyuan 030024, Shanxi, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
Ti-6Al-4V alloy; cryogenic treatment; wear behavior; MECHANICAL-PROPERTIES; SLIDING WEAR; FRETTING WEAR; MICROSTRUCTURAL VARIATION; LOW-TEMPERATURE; RESISTANCE; PERFORMANCE; FRICTION; COATINGS; EVOLUTION;
D O I
10.3390/ma12182850
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Titanium alloys are widely used in many fields because of their excellent comprehensive properties. However, its poor friction and wear properties limit its many potential applications. In general, the surface roughness of important parts manufactured by titanium alloy should meet certain requirements. As a low-cost and high-efficiency processing method, barrel finishing has been used for the surface finishing of titanium alloys. The main material removal mechanism of barrel finishing is micro-cutting/grinding, which is similar to the material wear mechanism under some conditions. In addition, titanium alloys are subjected to a low force in common surface finishing processes. Cryogenic treatment is a method that can improve the comprehensive properties of titanium alloys. Therefore, the friction and wear behavior of cryogenically treated Ti-6Al-4V titanium alloy (CT Ti alloy) and non-cryogenically treated Ti-6Al-4V titanium alloy (NT Ti alloy) at a low load and scratch speed was studied comparatively in this paper. The results show that the CT Ti alloy exhibits a lower friction coefficient and wear rate under both dry and wet wear conditions. Under wet conditions, the stabilized friction coefficient is lower than that under dry conditions. The stabilized friction coefficient of CT Ti alloy is 0.18 after reaching a stable wear stage under wet conditions. Under dry wear conditions, the NT Ti alloy mainly showed typical abrasive wear, heavy adhesion wear and oxidation wear characters. The wear mechanisms of CT Ti alloy are mainly abrasive wear, slight adhesion wear and oxidation wear. Under wet wear conditions, the wear mechanism of NT Ti alloy is abrasive wear and slight adhesion wear. After cryogenic treatment, the mechanism for CT Ti alloy is slight abrasive wear.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Fretting Wear Behavior of Cu–Al Coating on Ti-6Al-4V Substrate under Dry and Wet (Lubricated) Contact Condition
    Hyukjae Lee
    Shankar Mall
    Karl N. Murray
    Tribology Letters, 2007, 28 : 19 - 25
  • [22] Dry sliding wear of Ti-6Al-4V alloy in air and vacuum
    Liu, Y
    Yang, DZ
    He, SY
    Wu, WL
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2003, 13 (05) : 1137 - 1140
  • [23] Dry sliding wear of Ti-6Al-4V alloy in air and vacuum
    刘勇
    杨德庄
    何世禹
    武万良
    Transactions of Nonferrous Metals Society of China, 2003, (05) : 1137 - 1140
  • [24] Study of the Friction and Wear Behavior of Ti-6Al-4V Alloy Under Low TemperaturesStudy of the Friction and Wear Behavior of Ti-6Al-4V Alloy Under Low TemperaturesZhu, Song, Deng, Zhao, and He
    Yue Zhu
    Linlin Song
    Zehaochen Deng
    Lei Zhao
    Jianchao He
    JOM, 2025, 77 (3) : 1659 - 1670
  • [25] Tool wear and hole quality investigation in dry helical milling of Ti-6Al-4V alloy
    Hao Li
    Gaiyun He
    Xuda Qin
    Guofeng Wang
    Cui Lu
    Linjing Gui
    The International Journal of Advanced Manufacturing Technology, 2014, 71 : 1511 - 1523
  • [26] Tool wear and hole quality investigation in dry helical milling of Ti-6Al-4V alloy
    Li, Hao
    He, Gaiyun
    Qin, Xuda
    Wang, Guofeng
    Lu, Cui
    Gui, Linjing
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2014, 71 (5-8): : 1511 - 1523
  • [27] Tool wear and hole quality investigation in dry helical milling of Ti-6Al-4V alloy
    Qin, X. (qxd@tju.edu.cn), 1600, Springer London (71): : 5 - 8
  • [28] Comparative analysis of tool wear progression of dry and cryogenic turning of titanium alloy Ti-6Al-4V under low, moderate and high tool wear conditions
    Muhammad Ali Khan
    Syed Husain Imran Jaffery
    Aamer Ahmed Baqai
    Mushtaq Khan
    The International Journal of Advanced Manufacturing Technology, 2022, 121 : 1269 - 1287
  • [29] Comparative analysis of tool wear progression of dry and cryogenic turning of titanium alloy Ti-6Al-4V under low, moderate and high tool wear conditions
    Khan, Muhammad Ali
    Jaffery, Syed Husain Imran
    Baqai, Aamer Ahmed
    Khan, Mushtaq
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 121 (1-2): : 1269 - 1287
  • [30] Study of the Friction and Wear Behavior of Ti-6Al-4V Alloy Under Low Temperatures
    Zhu, Yue
    Song, Linlin
    Deng, Zehaochen
    Zhao, Lei
    He, Jianchao
    JOM, 2025, 77 (03) : 1659 - 1670