Effects of Microstructure and Loading on Fracture of Sn-3.8Ag-0.7Cu Joints on Cu Substrates with ENIG Surface Finish

被引:8
|
作者
Huang, Z. [1 ]
Kumar, P. [2 ]
Dutta, I. [1 ]
Sidhu, R. [3 ]
Renavikar, M. [3 ]
Mahajan, R. [3 ]
机构
[1] Washington State Univ, Sch Mech & Mat Engn, Pullman, WA 99164 USA
[2] Indian Inst Sci, Dept Mat Engn, Bangalore 560012, Karnataka, India
[3] Intel Corp, Assembly Technol Dev, Chandler, AZ 85226 USA
基金
美国国家科学基金会;
关键词
Solder joint fracture; Sn-Ag solders; ENIG surface finish; fracture mechanism map; interfacial fracture; INTERFACIAL REACTIONS; INTERMETALLIC COMPOUNDS; SOLDER JOINTS; SN; NI; TEMPERATURE; RELIABILITY; MORPHOLOGY; GROWTH; BEHAVIOR;
D O I
10.1007/s11664-014-3441-6
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
When dropped, electronic packages often undergo failure by propagation of an interfacial crack in solder joints under a combination of tensile and shear loading. Hence, it is crucial to understand and predict the fracture behavior of solder joints under mixed-mode high-rate loading conditions. In this work, the effects of the loading conditions (strain rate and loading angle) and microstructure [interfacial intermetallic compound (IMC) morphology and solder yield strength] on the mixed-mode fracture toughness of Sn-3.8 wt.%Ag-0.7 wt.%Cu solder joints sandwiched between two Cu substrates with electroless nickel immersion gold (ENIG) metallization have been studied, and compared with the fracture behavior of joints attached to bare Cu. Irrespective of the surface finish, the fracture toughness of the solder joints decreased monotonically with strain rate and mode-mixity, both resulting in increased fracture proportion through the interfacial IMC layer. Furthermore, the proportion of crack propagation through the interfacial IMC layer increased with increase in the thickness and the roughness of the interfacial IMC layer and the yield strength of the solder, resulting in a decrease in the fracture toughness of the joint. However, under most conditions, solder joints with ENIG finish showed higher resistance to fracture than joints attached directly to Cu substrates without ENIG metallization. Based on the experimental observations, a fracture mechanism map is constructed correlating the yield strength of the solder, the morphology and thickness of the interfacial IMC, and the fracture mechanisms as well as the fracture toughness values for different solder joints under mode I loading.
引用
收藏
页码:4485 / 4496
页数:12
相关论文
共 50 条
  • [31] Reliability of fine pitch Sn-3.8Ag-0.7Cu flip chip solder joints with different connection pads on PCB
    Li, Dezhi
    Liu, Changqing
    Conway, Paul P.
    JOURNAL OF ELECTRONIC PACKAGING, 2008, 130 (01) : 0110051 - 0110057
  • [32] Effect of Gold Addition on the Microstructure and Mechanical Properties of Sn-3.8Ag-0.7Cu Lead-Free Solder Alloy
    Niranjani, V. L.
    Venkateswarlu, Pamidi
    Singh, Vajinder
    Chandra Rao, B. S. S.
    Kamat, S. V.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (06) : 1497 - 1505
  • [33] Interfacial reaction and dissolution behavior of Cu substrate in molten Sn-3.8Ag-0.7Cu in the presence of Mo nanoparticles
    Arafat, M. M.
    Haseeb, A. S. M. A.
    Johan, Mohd Rafie
    SOLDERING & SURFACE MOUNT TECHNOLOGY, 2011, 23 (03) : 140 - 149
  • [34] Aging induced structural and electrochemical corrosion behaviour of Sn-1.0Ag-0.5Cu and Sn-3.8Ag-0.7Cu solder alloys
    Kaushik, Raj K.
    Batra, Uma
    Sharma, J. D.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 745 : 446 - 454
  • [35] Effects of Co nanoparticle addition to Sn-3.8Ag-0.7Cu solder on interfacial structure after reflow and ageing
    Haseeb, A. S. M. A.
    Leng, Tay See
    INTERMETALLICS, 2011, 19 (05) : 707 - 712
  • [37] Brittle Fracture Behavior and Interfacial Reaction of Sn-Ag-Cu solders on ENIG and ENEPIG Surface Finish
    Kwon, Sang-Hyun
    Kim, Kang-Dong
    Lee, Tae-Ho
    Han, Deok-Gon
    Sung, Tae-Hyun
    Lee, Chang-Woo
    Yoo, Sehoon
    PROCEEDINGS OF THE 2012 IEEE 14TH ELECTRONICS PACKAGING TECHNOLOGY CONFERENCE, 2012, : 206 - 210
  • [38] Solidification Condition Effects on Microstructures and Creep Resistance of Sn-3.8Ag-0.7Cu Lead-Free Solder
    J. Liang
    N. Dariavach
    D. Shangguan
    Metallurgical and Materials Transactions A, 2007, 38 : 1530 - 1538
  • [39] Viscosity and Electrical Conductivity of the Liquid Sn-3.8Ag-0.7Cu Alloy with Minor Co Admixtures
    A. Yakymovych
    V. Sklyarchuk
    Yu. Plevachuk
    B. Sokoliuk
    Journal of Materials Engineering and Performance, 2016, 25 : 4437 - 4443
  • [40] Viscosity and Electrical Conductivity of the Liquid Sn-3.8Ag-0.7Cu Alloy with Minor Co Admixtures
    Yakymovych, A.
    Sklyarchuk, V.
    Plevachuk, Yu.
    Sokoliuk, B.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (10) : 4437 - 4443