Correlation Between Isothermal Expansion and Functional Properties Change of the Fe81B13Si4C2 Amorphous Alloy

被引:7
|
作者
Kalezic-Glisovic, A. [1 ]
Maricic, V. A. [1 ]
Kosanovic, D. A. [2 ]
Dukic, S. [1 ]
Simeunovic, R. [1 ]
机构
[1] Tech Fac Cacak, Cacak 32000, Serbia
[2] Serbian Acad Arts & Sci, Inst Tech Sci, Belgrade 11000, Serbia
关键词
Amorphous materials; Structural relaxation; Thermal expansion; Magnetic susceptibility; CRYSTALLIZATION;
D O I
10.2298/SOS0903283K
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The structural changes effect on functional properties of ribbon shaped samples of the Fe81B13Si4C2 amorphous alloy during annealing process was investigated ill this paper. Differential scanning calorimetry method has shown that this alloy crystallizes ill one stage, in temperature range from room temperature up to 700 degrees C. Structural relaxation process was investigated by sensitive dilatation method in nonisothermal and isothermal conditions. It has been shown that structural relaxation process occurs in two stages by measuring thermal expansion at constant temperatures of t(1) = 420 degrees C, t(2) = 440 degrees C and t(3) = 460 degrees C. The first stage is characterized by linear logarithmic dependence of thermal expansion upon time at constant temperature. The second stage of structural relaxation process is characterized by linear dependence of isothermal expansion upon the square root of process time These results imply that the first stage of structural relaxation process is a rapid kinetic process, while the second stage of structural relaxation process is a slow diffusion process. The rate constants k(11) = 2,27.10(-3)s(-1), k(12) = 2,79.10(-3) s(-1)', k(13) = 3,6.10(-3) s(-1), k(21) = 0.67.10(-4) s(-1), k(22) = 3, 72.10(-4) s(-1), k(23) = 21,53.10(-4) s(-1) and activation energies E-1 = 48,64 kJ/mol and E-2 = 366, 23 kJ/mol were determined for both stages of structural relaxation process. The distinct correlation between structural relaxation process and magnetic susceptibility relative change was determined by thermomagnetic measurements. It has been shown that magnetic susceptibility call be increased by up to 80%, by convenient annealings after structural relaxation process, at magnetic field intensity of 8 kA/m.