Tailoring Electromechanical Properties of Natural Rubber Vitrimers by Cross-Linkers

被引:11
|
作者
Bui, Khoa [1 ,2 ]
Wemyss, Alan M. [1 ]
Zhang, Runan [3 ]
Nguyen, Giao T. M. [2 ]
Vancaeyzeele, Cedric [2 ]
Vidal, Frederic [2 ]
Plesse, Cedric [2 ]
Wan, Chaoying [1 ]
机构
[1] Univ Warwick, Int Inst Nanocomposites Mfg IINM, WMG, Coventry CV4 7AL, W Midlands, England
[2] CY Cergy Paris Univ, F-95000 Cergy, France
[3] Univ Bath, Dept Mech Engn, Bath BA2 7AY, Avon, England
关键词
NETWORKS; TRANSALKYLATION; TRANSESTERIFICATION; VULCANIZATE; PERFORMANCE; ROBUST;
D O I
10.1021/acs.iecr.2c01229
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The growing demand for smart polymeric transducers such as dielectric elastomer actuators and energy harvesters has urged the use of sustainable and recyclable elastomeric materials. Vitrimer chemistry has shed light on future reprocessable and recyclable thermosets and elastomers. In this work, epoxidized natural rubber (ENR) vitrimers were prepared using diacid or triacid cross-linkers and formed covalently cross-linking networks via thermally triggered reversible beta-hydroxy ester bonds. The cross-linked ENR elastomers exhibited Arrhenius-type viscoelastic behavior with a complete stress relaxation between 140 and 160 degrees C, that is, vitrimer characteristics, which were highly dependent on the cross-linking temperature. The mechanical and dielectric properties of the ENR vitrimers can be tuned by varying the molecular structure and concentration of the cross-linkers. Among the diacid and triacid cross-linkers, Pripol 1017 fatty polyacid (P1017) and 3,3'-dithiopropionic acid (DTPA) had similar effects on the cross-linking density and mechanical properties of the ENR vitrimers. The highest tensile strength of 8.70 +/- 1.9 or 15.6 +/- 2.6 MPa was obtained at 6 mol % of P1017 or DTPA, respectively. While for diamide-based diacid cross-linker (DME), 8 mol % was needed to reach the highest tensile strength of 13.1 +/- 2.7 MPa for the elastomer. The three ENR vitrimers showed increased relative permittivity epsilon' = 5 similar to 7 at 1 kHz while maintaining low dielectric losses compared to traditional dicumyl peroxide-cured ENR, with epsilon' = 3.57 at 1 kHz. With the optimized acidic cross-linker concentrations of P1017 at 6 mol 96, DTPA at 6 mol %, and DME at 8 mol 96, the ENR vitrimers exhibited improved actuation capabilities at lower electrical fields. Utilizing dynamic cross-linkers to tune the electromechanical properties of dielectric elastomers and the reversibly cross-linked polymer networks will open new opportunities for smart and sustainable dielectric elastomer devices.
引用
收藏
页码:8871 / 8880
页数:10
相关论文
共 50 条
  • [21] Nanospheres of doxorubicin as cross-linkers for a supramolecular hydrogelation
    Qiang Xue
    He Ren
    Chao Xu
    Gang Wang
    Chunhua Ren
    Jihui Hao
    Dan Ding
    Scientific Reports, 5
  • [22] Applications of α, ω-telechelic polydimethylsiloxane as cross-linkers for preparing high-temperature vulcanized silicone rubber
    Dong, Fuying
    Wang, Xianpeng
    Li, Shuaijie
    Hao, Jiawen
    Tang, Xinde
    Kuang, Rui
    Wang, Yanmin
    Feng, Shengyu
    POLYMERS FOR ADVANCED TECHNOLOGIES, 2019, 30 (04) : 932 - 940
  • [23] Investigation of polysiloxanes containing phenylethynyl groups as cross-linkers of heat-curable silicone rubber
    Xu, CH
    Feng, SY
    JOURNAL OF APPLIED POLYMER SCIENCE, 2000, 76 (10) : 1554 - 1557
  • [24] Effects of the cross-linkers on the buckling of microtubules in cells
    Li, Si
    Wang, Chengyuan
    Nithiarasu, Perumal
    JOURNAL OF BIOMECHANICS, 2018, 72 : 167 - 172
  • [25] CROSS-LINKERS TARGET ACIDIC AMINO ACIDS
    不详
    CHEMICAL & ENGINEERING NEWS, 2014, 92 (25) : 28 - 29
  • [26] Nanospheres of doxorubicin as cross-linkers for a supramolecular hydrogelation
    Xue, Qiang
    Ren, He
    Xu, Chao
    Wang, Gang
    Ren, Chunhua
    Hao, Jihui
    Ding, Dan
    SCIENTIFIC REPORTS, 2015, 5
  • [27] STUDIES ON CHROMATIN TOPOLOGY WITH PHOTOACTIVATABLE CROSS-LINKERS
    WYNS, L
    LASTERS, I
    WITTOUCK, E
    HAMERS, R
    ARCHIVES INTERNATIONALES DE PHYSIOLOGIE DE BIOCHIMIE ET DE BIOPHYSIQUE, 1977, 85 (01): : 211 - 212
  • [28] Thermal Conduction Across Graphene Cross-Linkers
    Liu, Xiangjun
    Zhang, Gang
    Zhang, Yong-Wei
    JOURNAL OF PHYSICAL CHEMISTRY C, 2014, 118 (23): : 12541 - 12547
  • [29] Dimethylacrylamide gels linked by dimethacrylate cross-linkers
    Tuncaboylu, Deniz Ceylan
    Yildirim, Tuana Seray
    POLYMER BULLETIN, 2019, 76 (10) : 5333 - 5344
  • [30] THE USE OF POLYGUANIDINES AS CROSS-LINKERS IN POWDER COATINGS
    COLLINS, MJ
    TAYLOR, JW
    BASSETT, DR
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1992, 204 : 178 - PMSE