Tailoring Electromechanical Properties of Natural Rubber Vitrimers by Cross-Linkers

被引:8
|
作者
Bui, Khoa [1 ,2 ]
Wemyss, Alan M. [1 ]
Zhang, Runan [3 ]
Nguyen, Giao T. M. [2 ]
Vancaeyzeele, Cedric [2 ]
Vidal, Frederic [2 ]
Plesse, Cedric [2 ]
Wan, Chaoying [1 ]
机构
[1] Univ Warwick, Int Inst Nanocomposites Mfg IINM, WMG, Coventry CV4 7AL, W Midlands, England
[2] CY Cergy Paris Univ, F-95000 Cergy, France
[3] Univ Bath, Dept Mech Engn, Bath BA2 7AY, Avon, England
关键词
NETWORKS; TRANSALKYLATION; TRANSESTERIFICATION; VULCANIZATE; PERFORMANCE; ROBUST;
D O I
10.1021/acs.iecr.2c01229
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The growing demand for smart polymeric transducers such as dielectric elastomer actuators and energy harvesters has urged the use of sustainable and recyclable elastomeric materials. Vitrimer chemistry has shed light on future reprocessable and recyclable thermosets and elastomers. In this work, epoxidized natural rubber (ENR) vitrimers were prepared using diacid or triacid cross-linkers and formed covalently cross-linking networks via thermally triggered reversible beta-hydroxy ester bonds. The cross-linked ENR elastomers exhibited Arrhenius-type viscoelastic behavior with a complete stress relaxation between 140 and 160 degrees C, that is, vitrimer characteristics, which were highly dependent on the cross-linking temperature. The mechanical and dielectric properties of the ENR vitrimers can be tuned by varying the molecular structure and concentration of the cross-linkers. Among the diacid and triacid cross-linkers, Pripol 1017 fatty polyacid (P1017) and 3,3'-dithiopropionic acid (DTPA) had similar effects on the cross-linking density and mechanical properties of the ENR vitrimers. The highest tensile strength of 8.70 +/- 1.9 or 15.6 +/- 2.6 MPa was obtained at 6 mol % of P1017 or DTPA, respectively. While for diamide-based diacid cross-linker (DME), 8 mol % was needed to reach the highest tensile strength of 13.1 +/- 2.7 MPa for the elastomer. The three ENR vitrimers showed increased relative permittivity epsilon' = 5 similar to 7 at 1 kHz while maintaining low dielectric losses compared to traditional dicumyl peroxide-cured ENR, with epsilon' = 3.57 at 1 kHz. With the optimized acidic cross-linker concentrations of P1017 at 6 mol 96, DTPA at 6 mol %, and DME at 8 mol 96, the ENR vitrimers exhibited improved actuation capabilities at lower electrical fields. Utilizing dynamic cross-linkers to tune the electromechanical properties of dielectric elastomers and the reversibly cross-linked polymer networks will open new opportunities for smart and sustainable dielectric elastomer devices.
引用
收藏
页码:8871 / 8880
页数:10
相关论文
共 50 条
  • [1] Cross-Linking Vitrimers after Melt Processing Using Supramolecularly Masked Dynamic Cross-Linkers
    Formon, Georges J. M.
    Jayaratnam, Jonathan
    Guibert, Clement
    Van Zee, Nathan J.
    Nicolay, Renaud
    [J]. MACROMOLECULES, 2024, 57 (17) : 8277 - 8286
  • [2] Controlled Release of Metal Ion Cross-Linkers and Development of Self-Healable Epoxidized Natural Rubber
    Mandal, Subhradeep
    Simon, Frank
    Banerjee, Shib Shankar
    Tunnicliffe, Lewis B.
    Nakason, Charoen
    Das, Chayan
    Das, Mithun
    Naskar, Kinsuk
    Wiessner, Sven
    Heinrich, Gert
    Das, Amit
    [J]. ACS APPLIED POLYMER MATERIALS, 2021, 3 (02) : 1190 - 1202
  • [3] Thiomers: Impact of in situ cross-linkers on mucoadhesive properties
    Hung Thanh Lam
    Leonaviciute, Gintare
    Zupancic, Ozbej
    Bernkop-Schnurch, Andreas
    [J]. EUROPEAN JOURNAL OF PHARMACEUTICAL SCIENCES, 2017, 106 : 41 - 48
  • [4] Temperature dependent dynamic mechanical properties of hydrogenated nitrile butadiene rubber and the effect of peroxide cross-linkers
    Likozar, Blaz
    Krajnc, Matjaz
    [J]. E-Polymers, 2007,
  • [5] Temperature dependent dynamic mechanical properties of hydrogenated nitrile butadiene rubber and the effect of peroxide cross-linkers
    Likozar, Blaz
    Krajnc, Matjaz
    [J]. E-POLYMERS, 2007,
  • [6] Tailoring polystyrene solid-phase synthesis resins: Incorporation of flexible cross-linkers
    Toy, PH
    Reger, TS
    Janda, KD
    [J]. ALDRICHIMICA ACTA, 2000, 33 (03) : 87 - 93
  • [7] The Electromechanical Properties of Crosslinked Natural Rubber
    Niamlang, Sumonman
    Thongchai, Santi
    Pawananant, Nipaporn
    Sirivat, Anuvat
    [J]. 10TH ECO-ENERGY AND MATERIALS SCIENCE AND ENGINEERING SYMPOSIUM, 2013, 34 : 697 - 704
  • [8] Nucleoside-Based Cross-Linkers for Hydrogels with Tunable Properties
    Itzhakov, Rafael
    Tworowski, Dmitry
    Sadot, Noy
    Sayas, Tali
    Fallik, Elazar
    Kleiman, Maya
    Poverenov, Elena
    [J]. ACS APPLIED MATERIALS & INTERFACES, 2023, 15 (05) : 7359 - 7370
  • [9] SYNTHESIS AND PROPERTIES OF PHENOL BLOCKED TOLUENE DIISOCYANATE CROSS-LINKERS
    KOTHANDARAMAN, H
    NASAR, AS
    [J]. JOURNAL OF MACROMOLECULAR SCIENCE-PURE AND APPLIED CHEMISTRY, 1995, A32 (05): : 1017 - 1024
  • [10] Effect of natural cross-linkers and drying methods on physicochemical and thermal properties of dried porcine plasma protein
    Samsalee, Namfon
    Sothornvit, Rungsinee
    [J]. FOOD BIOSCIENCE, 2017, 19 : 26 - 33