摘要
Aluminium metal matrix composites (AMCs) have become quite popular for light weight, low cost, and good workability. The present work reports the impact of silicon carbide (SiC) reinforcement on the physical, microstructural, and mechanical characteristics of Al-4032/SiC composites with 4, 6, 8% of SiC (particle size 54 mu m) fabricated through bottom pouring stir casting set-up. Density and porosity measurements of the AMC samples have been performed using the rule of mixture. The microstructure of the AMC samples has been analyzed using optical microscope (OM), x-ray diffraction analysis (XRD), and scanning electron microscopy (SEM) equipped with energy dispersive spectroscopy (EDS). The mechanical properties, in terms of the ultimate tensile strength (UTS), elongation, micro-hardness, and impact toughness of the AMCs have also been measured according to American society for testing and materials (ASTM) standards. A maximum 1.52% increase in theoretical density, while a maximum 2.92% decrease in experimental density has been recorded for 8% reinforcement. The UTS, microhardness, and impact toughness of the AMC samples have been found to improve significantly owing to the addition of ceramic particles. The uniform distribution of SiC particles all over base Al-4032 matrix material has been noticed by SEM and OM for AMCs up to 6% reinforcement. The reinforcement particles tend to agglomerate beyond this composition.
引用
收藏
页数:13
相关论文
共 50 条
  • [21] Sliding Wear of the Ti-Reinforced Al Matrix Bi-metal Composite: A Potential Replacement to Conventional SiC-Reinforced Composites for Automotive Application
    Ridvan Gecu
    Ahmet Karaaslan
    International Journal of Metalcasting, 2019, 13 : 641 - 652
  • [22] CHARACTERIZATION AND PERFORMANCE IMPROVEMENT OF SiC-REINFORCED Cu-MATRIX-BASED COMPOSITES AS ELECTRODE FOR EDM MACHINING
    Somani, Nalin
    Tyagi, Y. K.
    Gupta, Nitin Kumar
    Das, Anshuman
    SURFACE REVIEW AND LETTERS, 2023, 30 (05)
  • [23] Optimization of process parameters inend milling of Al-4032 based metal matrix composite using TGRA
    Saini, Pardeep
    Singh, Pradeep K.
    Kumar, Deepak
    Maurya, Anuj
    ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, 2022, 8 : 1346 - 1358
  • [24] Fabrication of SiC reinforced aluminium metal matrix composites through microwave sintering
    Liu, Jianhua
    Zhou, Bo
    Xu, Lei
    Han, Zhaohui
    Zhou, Junwen
    MATERIALS RESEARCH EXPRESS, 2020, 7 (12)
  • [25] INTERFACE, MATRIX AND FIBER MICROSTRUCTURE IN SIC-REINFORCED GLASS-CERAMIC COMPOSITES
    MURTHY, VSR
    PHARAOH, MW
    LEWIS, MH
    INSTITUTE OF PHYSICS CONFERENCE SERIES, 1990, (111): : 185 - 196
  • [26] Sliding wear characteristics of Al-4032/SiC/GMP hybrid composites using L-16 orthogonal array
    Kumar, Deepak
    Singh, Pradeep K.
    ENGINEERING RESEARCH EXPRESS, 2022, 4 (02):
  • [27] EROSION OF SIC-REINFORCED ALUMINA CERAMIC COMPOSITES
    SYKES, MT
    SCATTERGOOD, RO
    ROUTBORT, JL
    COMPOSITES, 1987, 18 (02): : 153 - 163
  • [29] Wear of SiC-reinforced Al-matrix composites in the temperature range 20-200 degrees C
    Martin, A
    Martinez, MA
    LLorca, J
    WEAR, 1996, 193 (02) : 169 - 179
  • [30] Micromechanical stresses in SiC-reinforced Al2O3 composites
    Li, Z., 1600, Pharmacotherapy Publications Inc. (72):