The wear and corrosion properties of stainless steel nitrided by low-pressure plasma-arc source ion nitriding at low temperatures

被引:85
|
作者
Wang, L [1 ]
Xu, B [1 ]
Yu, ZW [1 ]
Shi, YQ [1 ]
机构
[1] Dalian Maritime Univ, Inst Met & Technol, Dalian 116024, Peoples R China
来源
SURFACE & COATINGS TECHNOLOGY | 2000年 / 130卷 / 2-3期
关键词
low pressure plasma arc source; nitriding; stainless steel; wear and pitting corrosion;
D O I
10.1016/S0257-8972(00)00713-1
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Low pressure plasma are discharge-assisted nitriding of AISI 304 austenitic stainless steel is a process that produces surface layers with useful properties such as a high surface hardness of approximately 1500 Hv(0.1) and a high resistance to frictional wear and corrosion. The phase composition, the thickness, the microstructure and the surface topography of the nitrided layer, as well as its properties, depend essentially on the process parameters. Among them, the processing temperature is the most important factor for forming 21 hard layer with good wear and corrosion resistance. Nitriding austenitic stainless steel at approximately 420 degrees C for 70 min can produce a thin layer of 7-8 mu m with very high hardness and good corrosion resistance on the surface. The microstructure was studied by optical microscopy and both glancing angle and conventional Bragg-Brentano (theta-2 theta) symmetric geometry X-ray diffraction (XRD). The formation of expanded austenite was observed. Measurements of the wear depths indicated that the wear resistance of austenitic stainless steel can be improved greatly by nitriding at approximately 420 degrees C using low-pressure plasma-are source ion nitriding. (C) 2000 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:304 / 308
页数:5
相关论文
共 50 条
  • [41] Development of an Extended Arc Plasma Source for Low-Pressure Surface Treatment
    Plaksin, Vadim Yu.
    Lee, Heon Ju
    Yim, Chan Joo
    Ko, Min Kock
    JOURNAL OF THE KOREAN PHYSICAL SOCIETY, 2008, 53 (05) : 3077 - 3082
  • [42] Tribological studies of plasma source ion nitrided low alloy tool steel
    Lei, MK
    Wang, P
    Huang, Y
    Yu, ZW
    Yuan, LJ
    Zhang, ZL
    WEAR, 1997, 209 (1-2) : 301 - 307
  • [43] IMPROVEMENT OF MECHANICAL PROPERTIES OF MARTENSITIC STAINLESS STEEL BY PLASMA NITRIDING AT LOW TEMPERATURE
    Y.T.Xi~* D.X.Liu D.Han Corrosion and Protection Research Lab
    ActaMetallurgicaSinica(EnglishLetters), 2008, (01) : 21 - 29
  • [44] Improvement of mechanical properties of martensitic stainless steel by plasma nitriding at low temperature
    Corrosion and Protection Research Lab, Northwestern Polytechnical University, Xi'an, 710072, China
    不详
    Acta Metal Sin, 2008, 1 (21-29):
  • [45] Influence of Nitrogen in Plasma-Arc Remelting on the Structure and Properties of Stainless Steel
    Baeva L.A.
    Il’ichev M.V.
    Tyuftyaev A.S.
    Filippov G.A.
    Shchukina L.E.
    Steel in Translation, 2017, 47 (12) : 827 - 829
  • [46] LOW-PRESSURE ION-SOURCE
    FITCH, RK
    RUSHTON, GJ
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1972, 9 (01): : 379 - &
  • [47] MICROSTRUCTURE OF NITRIDED LAYERS IN AISI 316L STAINLESS STEEL AFTER LOW TEMPERATURE ION NITRIDING
    Dalibon, E. L.
    Bozzano, P. B.
    Bruehl, S. P.
    ACTA MICROSCOPICA, 2013, 22 (01): : 4 - 11
  • [48] Wear and corrosion properties of AISI 420 martensitic stainless steel treated by active screen plasma nitriding
    Li, Yang
    He, Yongyong
    Xiu, JunJie
    Wang, Wei
    Zhu, YiJie
    Hu, Baoguo
    SURFACE & COATINGS TECHNOLOGY, 2017, 329 : 184 - 192
  • [49] Effect of Screen Open Hole on Nitriding Behavior, Corrosion Resistance and Wear Resistance of Plasma Nitrided Low Carbon Steel Using Ti Screen
    Imamura, Kodai
    Nishimoto, Akio
    JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2021, 85 (03) : 95 - 102
  • [50] Effect of screen open hole on nitriding behavior, corrosion resistance and wear resistance of plasma nitrided low carbon steel using ti screen
    Imamura, Kodai
    Nishimoto, Akio
    Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals, 2021, 85 (03): : 95 - 102