Thermal shock resistance and toughening mechanism of W/Ta and W/TiN/Ta laminated composites

被引:3
|
作者
Xu, Gaoyong [1 ]
Yan, Zizhi [1 ]
Lu, Hui [1 ]
Cai, Jili [1 ]
Wang, Ruoqi [1 ]
Feng, Fan [2 ]
Cai, Chao [1 ]
Suo, Jinping [1 ]
机构
[1] Huazhong Univ Sci & Technol, Sch Mat Sci & Engn, State Key Lab Mat Proc & Die & Mould Technol, Wuhan 430074, Peoples R China
[2] Southwestern Inst Phys, Chengdu 610225, Peoples R China
基金
中国国家自然科学基金;
关键词
W-based laminated composites; Diffusion; Thermal shock resistance; Toughening mechanism; Interfacial structure; TUNGSTEN; BEHAVIOR; BOUNDARIES; DIFFUSION; SYSTEM;
D O I
10.1016/j.ijrmhm.2022.105810
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The brittleness of tungsten (W) is a significant limitation on its widespread applications as a high-temperature structural material. Laminated composite technology proved to be an effective method to improve the toughness of W. In this work, W/Ta and W/TiN/Ta laminated composites were prepared by spark plasma sintering (SPS) to overcome the brittleness of W. The toughening properties of the W/Ta and W/TiN/Ta laminated composites were evaluated by electron beam thermal shock and laser thermal diffusivity testing. The toughening mechanism was clarified by scanning electron microscopy, electron probe micro-analysis, and transmission electron microscopy. After the three-point bending test, interfacial debonding was observed predominantly at the incoherent W-TiN rather than at the semi-coherent Ta-TiN interfaces. At 0.30 GW/m2 of electron beam thermal shock, the average width and depth of thermal shock cracks in the W/Ta laminated composite were - 9.4 mu m and - 30.0 mu m, respectively, which were much smaller than those in the W/W laminates and W/TiN/Ta laminated composite.
引用
收藏
页数:9
相关论文
共 50 条
  • [21] Comparison of hydrogen retention in W and W/Ta alloys
    Schmid, K.
    Rieger, V.
    Manhard, A.
    JOURNAL OF NUCLEAR MATERIALS, 2012, 426 (1-3) : 247 - 253
  • [22] Deformation twins in a shock-loaded Ta-2.5(w)/W-o precursor plate and a recovered, Ta-2.5(w)/W-o explosively formed penetrator
    Pappu, S
    Kennedy, C
    Murr, LE
    Meyers, MA
    SCRIPTA MATERIALIA, 1996, 35 (08) : 959 - 965
  • [23] Plastic Deformation Characteristic of Ta-W Alloy at Shock Loading
    Northwest Inst. Nonfer. Metal Res., Xi'an 710016, China
    Xiyou Jinshu Cailiao Yu Gongcheng, 2 (17):
  • [24] Plastic deformation characteristic of Ta-W alloy at shock loading
    Zhang, TJ
    Zhang, DY
    Ding, X
    RARE METAL MATERIALS AND ENGINEERING, 1997, 26 (02) : 12 - 17
  • [25] The ductile-brittle transition behaviors of W/Ta multilayer composites
    Chen, C.
    Chen, Y.
    Li, K. L.
    Yang, S. Y.
    Wang, J.
    Wang, S.
    Mao, Y. R.
    Luo, L. M.
    Wu, Y. C.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 946
  • [26] Study on W/(TiN)Ta composite and its application in shape charge liner
    Zizhi Yan
    Gaoyong Xu
    Jinping Suo
    SN Applied Sciences, 2020, 2
  • [27] Study on W/(TiN)Ta composite and its application in shape charge liner
    Yan, Zizhi
    Xu, Gaoyong
    Suo, Jinping
    SN APPLIED SCIENCES, 2020, 2 (10):
  • [28] ISOCHRONAL ANNEALING BEHAVIOR OF TA-8W-2HF AND TA-10W
    FLINN, JE
    JOURNAL OF METALS, 1965, 17 (09): : 1027 - &
  • [29] Compressive Property and Toughening Mechanism of Directionally Solidified Fe(Al, Ta)/Fe2Ta (Al) Eutectic Composites
    Liang, Zhanpeng
    Cui, Chunjuan
    Li, Wei
    Zhang, Kai
    Wang, Zhicong
    Wu, Tongchao
    Song, Yonghui
    Su, Haijun
    ADVANCED ENGINEERING MATERIALS, 2024, 26 (12)
  • [30] INTERDIFFUSION IN THE TA-W SYSTEM
    ROMIG, AD
    CIESLAK, MJ
    HILLS, CR
    JOURNAL OF METALS, 1984, 36 (12): : 79 - 79