Effect of non-stoichiometry on hydrogen storage properties of La(Ni3.8Al1.0Mn0.2)x alloys

被引:22
|
作者
Li, S. L. [1 ,2 ]
Wang, P. [3 ]
Chen, W. [1 ,2 ]
Luo, G. [1 ,2 ]
Chen, D. M. [1 ]
Yang, K. [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China
[2] Chinese Acad Sci, Grad Sch, Beijing 100049, Peoples R China
[3] 404 Ltd Co, China Natl Nucl Corp, Lanzhou 732850, Peoples R China
基金
中国国家自然科学基金;
关键词
Metal hydride; Hydrogen absorbing materials; Gas-solid reactions; Thermodynamic properties; ELECTROCHEMICAL CYCLING STABILITY; HYDRIDE-FORMING COMPOUNDS; THERMODYNAMIC PARAMETERS; LANI5-BASED ALLOYS; CRYSTAL-STRUCTURE; RARE-EARTH; NI; SUBSTITUTION; SYSTEM; CO;
D O I
10.1016/j.ijhydene.2010.01.102
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The La(Ni3.8Al1.0Mn0.2)(x) (x= 0.94, 0.96, 0.98, 1.0) hydrogen storage alloys have been investigated to examine the effect of non-stoichiometry on the crystal structure, activation performance, hydrogen absorption/desorption properties and cycle life. It was found that for the stoichiometric compound, only single phase with CaCu5 type structure exists. However, for B-poor compounds of AB(5) alloys, there is a principal CaCu5 type phase with a small amount of second phase and the amount of second phase increased with decreasing x when x >= 0.96 and reached a maximum when x = 0.96. The activation becomes harder with decreasing x until x = 0.96 and easier when x decreased to 0.94. The plateau pressure increased and the hydrogen uptake capacity decreased with decreasing x when x >= 0.96, and then decreased and increased, respectively, when x further decreased to 0.94. Both the change in the lattice strain which could be estimated by FWHM (full width at half maximum) and the degree of slope factor S-f in the alloys show the same trend with the change of x, exhibiting a maximum at x = 0.96. The Delta H decreased with decreasing x when x >= 0.96 and then increased when x = 0.94 and it was found that the larger the cell volume, the larger the absolute value of the enthalpy. The pulverization resistance of the alloys was greatly improved by the non-stoichiometric. The kinetics of the alloys was very fast and almost not influenced by the change of non-stoichiometric x. After 300 absorption/desorption cycles, the hydrogen uptake capacity of the stoichiometric and non-stoichiometric alloys almost kept the same, but the particle size decreased greatly. (C) 2010 Professor T. Nejat Veziroglu. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:3537 / 3545
页数:9
相关论文
共 50 条
  • [41] Structure and electrochemical properties of La1−xMgxNi2.8Co0.4Mn0.1Al0.2 (x = 0.25, 0.30, 0.33) hydrogen storage alloys
    Si Li
    Huai-Ying Zhou
    Zhong-Min Wang
    Jian-Qiu Deng
    Qing-Rong Yao
    Rare Metals, 2020, 39 : 1464 - 1468
  • [42] Effects of Magnesium Content on Structure and Electrochemical Properties of La-Mg-Pr-Al-Mn-Co-Ni Hydrogen Storage Alloys
    Zarpelon, L. M. C.
    Banczek, E. P.
    Martinez, L. G.
    Lima, N. B.
    Costa, I.
    Faria, R. N.
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2018, 2018
  • [43] Effect of Al and W substitution for Ni on the microstructure and electrochemical properties of La1.3CaMg0.7Ni9-x (Al0.5W0.5)x hydrogen storage alloys
    Zhang, Peng
    Liu, Yongning
    Zhu, Jiewu
    Wei, Xuedong
    Yu, Guang
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2007, 32 (13) : 2488 - 2493
  • [44] Phase structure and electrochemical properties of the AB3.8-type La-Mg-Ni system hydrogen storage alloys
    Fan, Jingbo
    Deng, Anqiang
    Xia, Guangjun
    Qian, Kenong
    Luo, Yongchun
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2010, 39 (12): : 2142 - 2146
  • [45] Phase structures and hydrogen storage capabilities of the alloys (Ml)x (Ni3.8Co0.75Mn0.4Ti0.05)
    Ren, Ke
    Lei, Yongquan
    Chen, Lixin
    Zhang, Qingan
    Wang, Qidong
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2000, 29 (04): : 235 - 238
  • [46] Study on hydrogen storage properties of La0.6Nd0.4Ni4.8Mn0.2M0.1 (M=Cu,Zr) alloys
    Li Shenlan
    Cheng Honghui
    Deng Xiaoxia
    Lue Manqi
    Chen Demin
    Yang Ke
    RARE METAL MATERIALS AND ENGINEERING, 2008, 37 (04) : 599 - 603
  • [47] Phase Structure and Electrochemical Properties of the AB3.8-Type La-Mg-Ni System Hydrogen Storage Alloys
    Fan Jingbo
    Deng Anqiang
    Xia Guangjun
    Qian Kenong
    Luo Yongchun
    RARE METAL MATERIALS AND ENGINEERING, 2010, 39 (12) : 2142 - 2146
  • [48] Phase structures and hydrogen storage capabilities of the alloys (Ml)x (Ni3.8Co0.75Mn0.4Ti0.05)
    Ren, K
    Lei, YQ
    Chen, LX
    Zhang, QG
    Wang, QD
    RARE METAL MATERIALS AND ENGINEERING, 2000, 29 (04) : 235 - 238
  • [49] Structure and electrochemical properties of (La1-xDyx)0.8Mg0.2Ni3.4Al0.1 (x=0.0-0.20) hydrogen storage alloys
    Wang, Beiping
    Chen, Yuanzhen
    Liu, Yongning
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2012, 37 (11) : 9082 - 9087
  • [50] Effect of TiMn1.5 alloying on the structure, hydrogen storage properties and electrochemical properties of LaNi3.8Co1.1Mn0.1 hydrogen storage alloys
    Peng Lv
    Zhong-min Wang
    Nian-lei Shi
    Huai-ying Zhou
    Jian-qiu Deng
    Qing-rong Yao
    Huai-gang Zhang
    Russian Journal of Electrochemistry, 2014, 50 : 953 - 958