Dissimilar aluminum alloys such as 2024-T3 and 7075-T6 plates 3 mm thickness were friction stir butt welded. The welding was carried out at a constant welding speed of 100 mm/min and rotation speeds of 400, 800, 1200 1600 and 2000 min(-1). Effects of rotation speeds and fixed location of two alloys on microstructures especially the homogeneity of elemental distribution in the stir zone (SZ), hardness distributions, and tensile properties of the joints were investigated. The homogeneity of constituents of the two alloys in the SZ was analyzed by a scanning electron microscope (SEM) equipped with an energy dispersive X-ray spectroscopy (EDS). At the lowest rotation speed of 400 min(-1) there was no mixing of two alloys in the SZ and a border between them was observed regardless of the fixed location. Increase of rotation speed more than 400 min(-1) brought about a mixed structure likewise onion ring with periodic change of equiaxed grain size and heterogeneous distribution of alloying elements in the SZ. At 2000 min(-1) of rotation speed the SZ mainly composed of the material fixed on the advancing side. The hardness increased in the zones occupied by 2024-T3 Al alloy and fluctuations took place in the SZ due to the onion ring at the higher rotation speeds till 1600 min(-1). At 2000 min(-1) of rotation speed the hardness of SZ mainly depend on the material fixed on the advancing side. Hardness minima was in the heat affected zone (HAZ) on the side of AA2024-T3 Al alloy and the values slightly increased as the rotation speed increased. In the case of transverse tensile test, defect-free joints were fractured at the HAZ on 2024-T3 side and a maximum tensile strength of the joints was achieved at 1200 mint of rotation speed when 2024-T3 Al alloy was located on the advancing side. On the other hand. the tensile properties of SZ in the longitudinal direction showed higher values when 7075 Al alloy was located on the advancing side.
引用
收藏
页码:1928 / 1937
页数:10
相关论文
共 50 条
  • [41] INFLUENCE OF FRICTION STIR WELDING PARAMETERS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF AA2024-T3 ALUMINUM ALLOY
    Khodir, Saad Ahmed
    Shibayanagi, Toshiya
    Naka, Masaaki
    [J]. CHARACTERIZATION AND CONTROL OF INTERFACES FOR HIGH QUALITY ADVANCED MATERIALS II, 2007, 198 : 91 - 96
  • [42] Investigation on microstructural evolution and local mechanical performance of friction stir lap welded AA6061-T6/AA7075-T6 joints
    Jha, Kishor Kumar
    Kesharwani, Rahul
    Imam, Murshid
    [J]. ENGINEERING FAILURE ANALYSIS, 2024, 160
  • [43] Effect of friction stir welding on dynamic properties of AA2024-T3 and AA7075-T7351
    Chao, YJ
    Wang, Y
    Miller, KW
    [J]. WELDING JOURNAL, 2001, 80 (08) : 196S - 200S
  • [44] Influence of rotation speed on mechanical properties and corrosion sensitivity of friction stir welded AA2024-T3 joints
    Li, Na
    Li, Wenya
    Xu, Yaxin
    Yang, Xiawei
    Alexopoulos, Nikolaos D.
    [J]. MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (08): : 1016 - 1024
  • [45] Microstructure and mechanical properties of dissimilar friction stir welded AA2024-7075 joints: Influence of joining material direction
    Zhang, Chenghang
    Huang, Guangjie
    Cao, Yu
    Zhu, Yulong
    Li, Wei
    Wang, Xiaodong
    Liu, Qing
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 766
  • [46] Effect of Welding Parameters on Tensile Strength of AA7075-T6 Friction Stir Welded Joints
    Chennaiah, Mallapuram Bala
    Kumar, Podaralla Nanda
    Rao, Karanam Prahlada
    [J]. ADVANCES IN ADDITIVE MANUFACTURING AND JOINING, AIMTDR 2018, 2020, : 641 - 649
  • [47] Impact of cold spraying on microstructure and mechanical properties of optimized friction stir welded AA2024-T3 joint
    Li, W. Y.
    Li, N.
    Yang, X. W.
    Feng, Y.
    Vairis, A.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 702 : 73 - 80
  • [48] Correlation of microstructure, texture, and mechanical properties of friction stir welded Joints of AA7075-T6 plates using a flat tool pin profile
    Kesharwani, Rahul
    Jha, Kishor Kumar
    Imam, Murshid
    Sarkar, Chiranjit
    Barsoum, Imad
    [J]. HELIYON, 2024, 10 (03)
  • [49] Evaluating the fatigue initiation location in friction stir welded AA2024-T3 joints
    Lemmen, H. J. K.
    Alderliesten, R. C.
    Benedictus, R.
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2011, 33 (03) : 466 - 476
  • [50] Fatigue initiation behaviour throughout friction stir welded joints in AA2024-T3
    Lemmen, H. J. K.
    Alderliesten, R. C.
    Benedictus, R.
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2010, 32 (12) : 1928 - 1936