摘要
Silicon nitride ceramics with different amounts and compositons of the grain boundary phases are produced by gas pressure sintering and the corrosion behaviour was analysed in acids, bases and under hydrothermal conditions. The investigation shows, that the corrosion is strongly affected by the SiO2 content in the grain boundary and the amount of the additives. The results indicate that the grains and the thin films between the grains are very stable in acids and bases but solves partially under hydrothermal conditions. The corrosion behaviour of the investigated materials with a relatively stable grain boundary phase in acids can be described by the same kinetic laws as those used to describe the corrosion of glasses. An interfacial reaction is assumed to be rate-controlling. The less stable material with Y2O3/Al2O3 additives can be described by the corrosion behaviour of oxide nitride glasses only at the beginning. For higher corrosion deaths, the formation of protective barriers consisting of a hydrated SiO2 network is assumed to occur. (C) 2003 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:585 / 594
页数:10
相关论文
共 50 条
  • [31] HYDROTHERMAL CORROSION RESISTANCE OF SILICON NITRIDE WITH O′-SIALON GRAIN BOUNDARY PHASE
    Vetrecin, Michal
    Lences, Zoltan
    Galuskova, Dagmar
    Sajgalik, Pavol
    CERAMICS-SILIKATY, 2018, 62 (04) : 382 - 388
  • [32] Aqueous corrosion of borosilicate glass under acidic conditions: A new corrosion mechanism
    Geisler, Thorsten
    Janssen, Arne
    Scheiter, Daniel
    Stephan, Thomas
    Berndt, Jasper
    Putnis, Andrew
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2010, 356 (28-30) : 1458 - 1465
  • [33] Silicon nanowires grown from silicon monoxide under hydrothermal conditions
    Pei, LZ
    Tang, YH
    Chen, YW
    Guo, C
    Zhang, W
    Zhang, Y
    JOURNAL OF CRYSTAL GROWTH, 2006, 289 (02) : 423 - 427
  • [34] Wear of silicon nitride ceramics under fretting conditions
    Novak, S.
    Drazic, G.
    Samardzija, Z.
    Kalin, M.
    Vizintin, J.
    Materials Science and Engineering A, 1996, A215 (1-2): : 125 - 133
  • [35] Wear of silicon nitride ceramics under fretting conditions
    Novak, S
    Drazic, G
    Samardzija, Z
    Kalin, M
    Vizintin, J
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 215 (1-2): : 125 - 133
  • [36] Acidic corrosion of aluminum under conditions of contact bismuth deposition
    V. V. Bartenev
    O. I. Barteneva
    Protection of Metals and Physical Chemistry of Surfaces, 2011, 47 : 86 - 92
  • [37] Corrosion of the International Simple Glass under acidic to hyperalkaline conditions
    Backhouse, Daniel J.
    Fisher, Adam J.
    Neeway, James J.
    Corkhill, Claire L.
    Hyatt, Neil C.
    Hand, Russell J.
    NPJ MATERIALS DEGRADATION, 2018, 2 (01)
  • [38] Corrosion of the International Simple Glass under acidic to hyperalkaline conditions
    Daniel J. Backhouse
    Adam J. Fisher
    James J. Neeway
    Claire L. Corkhill
    Neil C. Hyatt
    Russell J. Hand
    npj Materials Degradation, 2
  • [39] Acidic corrosion of aluminum under conditions of contact bismuth deposition
    Bartenev, V. V.
    Barteneva, O. I.
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2011, 47 (01) : 86 - 92
  • [40] Study on corrosion and destroy mechanism of concrete under acidic conditions
    Yu, Z.G.
    Chen, R.R.
    Mtei, B.
    Journal of Mechanical Engineering Research and Developments, 2016, 39 (01) : 142 - 148