Effect of Si content on the microstructure and properties of Al-Si alloys fabricated using hot extrusion

被引:39
|
作者
Ma, Pan [1 ]
Jia, Yandong [2 ]
Prashanth, Konda Gokuidoss [3 ,4 ]
Yu, Zhishui [1 ]
Li, Chonggui [1 ]
Zhao, Jian [1 ]
Yang, Shanglei [1 ]
Huang, Lixin [1 ]
机构
[1] Shanghai Univ Engn Sci, Sch Mat Engn, Shanghai 201620, Peoples R China
[2] Shanghai Univ, Inst Mat, Lab Microstruct, Shanghai 200444, Peoples R China
[3] Austrian Acad Sci, Erich Schmid Inst Mat Sci, A-8700 Leoben, Austria
[4] Norwegian Univ Sci & Technol, Gjovik, Norway
基金
中国国家自然科学基金; 上海市自然科学基金; 中国博士后科学基金;
关键词
Al-Si alloy; microstructure; mechanical properties; coefficient of thermal expansion; THERMAL-EXPANSION BEHAVIOR; TENSILE PROPERTIES; MECHANICAL-PROPERTIES; MATRIX COMPOSITES; MANAGEMENT APPLICATIONS; POWDER-METALLURGY; HEAT-TREATMENT; EUTECTIC SI; SILICON; PARTICLES;
D O I
10.1557/jmr.2017.97
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al-(12, 20, 35 wt%)Si alloys were fabricated using powder metallurgy process involving hot pressing followed by hot extrusion. The effect of Si content on the microstructure [by scanning electron microscopy], the mechanical properties (hardness and tensile tests), and the thermal expansion behavior were studied in detail, respectively. Due to the friction between the Si phase and the matrix, as well as the diffusion of the Si atoms, the Si phase becomes a particulate shape after hot extrusion, and the size increases with increasing Si content. The mechanical strength increases, whereas, the elongation decreases with increasing the Si content from 12 to 35 wt%, which lead to a variation of the fracture mechanism from ductile to brittle failure. The coefficient of thermal expansion (CTE) decreases with increasing Si content as a result of restriction of Si on the Al matrix, and the measured CTE value is in good agreement with the Turner model below 573 K.
引用
收藏
页码:2210 / 2217
页数:8
相关论文
共 50 条
  • [41] Effect of processing parameters on microstructure in brazing of Al-Si alloys
    Shutov, I. V.
    Kamaeva, L. V.
    Krivilyov, M. D.
    Yu, C-N.
    Mesarovic, S. Dj.
    Sekulic, D. P.
    JOURNAL OF CRYSTAL GROWTH, 2020, 530
  • [42] Effect of Zn on microstructure and properties of Al-Si alloy
    Zhao, Haofeng
    Wang, Ling
    Liu, Xuedong
    Te Zhong Zhu Zao Ji You Se He Jin/Journal of Special Casting & Nonferrous Alloys, 1994, (02): : 5 - 7
  • [43] Effect of Li on Al-Si Alloys Structure and Properties
    Zhao Zhongkui
    Qiao Zhen
    Li Chang-long
    Sun Qing-zhou
    Zhang Pu-qing
    Wang Gui-qing
    MULTI-FUNCTIONAL MATERIALS AND STRUCTURES II, PTS 1 AND 2, 2009, 79-82 : 119 - 122
  • [44] EFFECTS OF MICROSTRUCTURE ON THE EROSION OF AL-SI ALLOYS
    CONRAD, H
    SHIN, Y
    SARGENT, G
    JOURNAL OF METALS, 1983, 35 (12): : 81 - 81
  • [45] Evolution of microstructure in eutectic Al-Si alloys
    Kori, SA
    Murty, BS
    Chakraborty, M
    INTERNATIONAL CONFERENCE ON SOLIDIFICATION SCIENCE AND PROCESSING: OUTLOOK FOR THE 21ST CENTURY, 2001, : 109 - 121
  • [46] Effect of silicon content on wear resistance of Al-Si alloys
    Gu, Shuying
    Wang, Ruyao
    Lu, Weihua
    Journal of Dong Hua University (English Edition), 1998, 15 (03): : 88 - 91
  • [47] EFFECTS OF Si CONTENT ON THE PROPERTIES OF P/M Al-Si BINARY ALLOYS.
    Sano, Hideo
    Yamauchi, Shigenori
    Inumaru, Susumu
    Shibue, Kazuhisa
    1985, (26):
  • [48] Effect of Silicon Content on Wear Resistance of Al-Si Alloys
    顾书英
    王汝耀
    鲁薇华
    Journal of Donghua University(English Edition), 1998, (03) : 88 - 91
  • [49] Microstructure and mechanical properties of Al-Si-X alloys fabricated by gas atomization and extrusion process
    Lee, T. H.
    Hong, S. J.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 487 (1-2) : 218 - 224
  • [50] Microstructure and wear characteristics of spray formed and hot extruded Al-Si alloys
    Srivastava, VC
    Ojha, SN
    MATERIALS SCIENCE AND TECHNOLOGY, 2004, 20 (12) : 1632 - 1638