The microstructure and mechanical properties of permanent-mould cast Mg-5 wt%Sn-(0-2.6) wt%Di alloys

被引:73
|
作者
Liu, Hongmei
Chen, Yungui [1 ]
Tang, Yongbai
Huang, Deming
Niu, Gao
机构
[1] Sichuan Univ, Sch Mat Sci & Engn, Chengdu 610065, Peoples R China
[2] Taiyuan Univ Technol, Taiyuan 030024, Shanxi, Peoples R China
关键词
magnesium alloys; tin; neodymium; praseodymium; rare earth elements;
D O I
10.1016/j.msea.2006.07.149
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The didymium (neodymium-praseodymium mixed metal, neodymium:praseodymium = 3:1) addition to the Mg-5 wt%Sn alloy results in the formation of a feather-shaped Sn-x(Nd,Pr)(y), phase mainly on the grain boundaries, and gives rise to grain refinement when the addition is below 2 wt%. The tensile strength and elongation of the alloys are improved with the addition of didymium, and optimum mechanical results are attained at an addition of 2.0 wt% didymium, where the UTS increased by 26.9% and the elongation by 7.7%. The feather-shaped Sn-x(Nd,Pr)(y) phase changes to a stick-shaped Sn-x,(Nd,Pr)(y) phase when the didymium addition is over 2 wt%. As a consequence, the tensile strength and especially the elongation show an obvious decline. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:348 / 355
页数:8
相关论文
共 50 条
  • [41] Corrosion behavior of as-cast Mg-5Sn based alloys with In additions in 3.5 wt% NaCl solution
    Wang, Xuejian
    Chen, Zongning
    Ren, Jing
    Kang, Huijun
    Guo, Enyu
    Li, Jiehua
    Wang, Tongmin
    CORROSION SCIENCE, 2020, 164 (164)
  • [42] Microstructure and mechanical properties of Mg-5Sn-5Zn-xCa alloys
    Qiu Ke-qiang
    Liu Bin
    You Jun-hua
    Ren Ying-lei
    MAGNESIUM TECHNOLOGY 2012, 2012, : 537 - 541
  • [43] Microstructures and Mechanical Properties of As-Cast AZ91+0-2.0wt.%La Magnesium Alloys
    Zhao Yuanhua
    Chen Yungui
    Tang Yongbai
    Xiao Sufen
    Wei Shanghai
    Zhang Xiaoping
    Wang Qing
    Tu Mingjing
    RARE METAL MATERIALS AND ENGINEERING, 2010, 39 (05) : 843 - 847
  • [44] Microstructure characterization and mechanical properties of the as-cast and as-extruded Mg-xLi-5Zn-0.5Er (x=8, 10 and 12 wt%) alloys
    Ji, Hao
    Wu, Guohua
    Liu, Wencai
    Liang, Xinli
    Liao, Guanglan
    Ding, Dehua
    MATERIALS CHARACTERIZATION, 2020, 159 (159)
  • [45] Effects of minor Sr addition on as-cast microstructure and mechanical properties of a Mg-3Sn-2Ca(wt.%) magnesium alloy
    Yang Mingbo
    Li Hongliang
    Duan Chengyu
    China Foundry, 2014, (02) : 108 - 114
  • [46] Effects of minor Sr addition on as-cast microstructure and mechanical properties of a Mg-3Sn-2Ca(wt.%) magnesium alloy
    Yang Mingbo
    Li Hongliang
    Duan Chengyu
    China Foundry, 2014, 11 (02) : 108 - 114
  • [47] Effects of minor Ti addition on as-cast microstructure and mechanical properties of Mg-3Sn-2Sr (wt.%) magnesium alloy
    Yang, Mingbo
    Li, Hongliang
    Duan, Chengyu
    Zhang, Jia
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 579 : 92 - 99
  • [48] Effects of minor Sr addition on as-cast microstructure and mechanical properties of a Mg-3Sn-2Ca (wt.%) magnesium alloy
    Yang Mingbo
    Li Hongliang
    Duan Chengyu
    CHINA FOUNDRY, 2014, 11 (02) : 108 - 114
  • [49] The effect of iron on the microstructure and mechanical properties of a cast Cu-12Sn-1.5Ni (wt. %) alloy
    Chen, Kaixuan
    Zhang, Jiawei
    Chen, Xiaohua
    Wang, Zidong
    Shi, Rongjian
    Zhang, Aijun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 785 (785):
  • [50] Influence of phase composition on microstructure and properties of Mg-5Al-0.4Mn-xRE (x=0, 3 and 5 wt.%) alloys
    Braszczynska-Malik, K. N.
    Grzybowska, A.
    MATERIALS CHARACTERIZATION, 2016, 115 : 14 - 22