Microstructure and mechanical properties of as-deposited and heat treated Ti-5Al-5Mo-5V-3Cr-1Zr (Ti-55531) alloy fabricated by laser melting deposition

被引:46
|
作者
Deng, Hao [1 ,2 ]
Chen, Longqing [1 ,2 ]
Qiu, Wenbin [2 ]
Zheng, Zhou [1 ]
Tang, Yi [2 ]
Hu, Zhendong [3 ]
Wei, Yongqiang [4 ]
Xia, Zuxi [4 ]
Le, Guomin [5 ]
Tang, Jun [2 ]
Cui, Xudong [1 ]
机构
[1] China Acad Engn Phys, Inst Chem Mat, Mianyang 621900, Sichuan, Peoples R China
[2] Sichuan Univ, Inst Nucl Sci & Technol, Key Lab Radiat Phys & Technol, Minist Educ, Chengdu 610064, Sichuan, Peoples R China
[3] Beijing Aeronaut Sci & Technol Res Inst COMAC, Beijing Key Lab Civil Aircraft Struct & Composite, Beijing 102211, Peoples R China
[4] CAAC, Res Inst 2, Chengdu 610064, Sichuan, Peoples R China
[5] China Acad Engn Phys, Inst Mat, Mianyang 621907, Sichuan, Peoples R China
关键词
Laser melting deposition; Ti-55531; Microstructure; Tensile properties; TENSILE PROPERTIES; TITANIUM; TI-6AL-4V; BEHAVIOR; COMPONENTS; MORPHOLOGY; TEXTURE; PHASE; EVOLUTION;
D O I
10.1016/j.jallcom.2019.151792
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this work, the first successful attempt of additive manufacturing (AM) Ti-55531 near-beta alloy fabricated by laser melting deposition (LMD) is reported. Optimized processing parameters of LMD were used to manufacture high relative density (99.8%) Ti-55531 alloy. It was found that the microstructure of as-deposited sample is mainly composed of beta phase with heterogeneous distribution of a phase. The heterogeneity of microstructure of as-deposited sample was caused by the ubiquitous temperature gradient during LMD process. Thus, the as-deposited samples have a significant anisotropic tensile property which may not meet the aeronautical criterion. To overcome the issue of inhomogeneous microstructure and minimize the anisotropy, the microstructure was tailored by two kinds of heat treatment, i.e., beta solution treatment subsequent aging (beta-STA) and triplex annealing (alpha/beta-STA). A transformed beta microstructure was obtained in beta-SAT condition, which resulted in the high ultimate tensile strength (UTS) (> 1350 MPa) and low ductility (<6.5%). Besides, the bimodal structure was formed in alpha/beta-STA condition and the associated sample shows an excellent balance of strength (UTS> 1200 MPa) and ductility (>8%). Furthermore, the formation mechanism of microstructure and the subsequent impact on mechanical properties was systematically discussed. This work demonstrates the potential of fabricating Ti-55531 alloy parts by LMD and paves the way for enhancing LMD processed near beta Ti-alloys through heat treatment. (C) 2019 Elsevier B.V. All rights reserved.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] The ageing response of direct laser deposited metastable β-Ti alloy, Ti-5Al-5Mo-5V-3Cr
    Sharma, Deepak
    Kada, Sitarama Raju
    Fabijanic, Daniel
    Parfitt, David
    Chen, Bo
    Roebuck, Bryan
    Fitzpatrick, Michael E.
    Barnett, Matthew Robert
    ADDITIVE MANUFACTURING, 2021, 48
  • [32] Influence of strain rates on high temperature deformation behaviors and mechanisms of Ti-5Al-5Mo-5V-3Cr-1Zr alloy
    Zhang, Hui
    Shao, Hui
    Shan, Di
    Wang, Kaixuan
    Cai, Lulu
    Yin, Enhuai
    Wang, Yanlin
    Zhuo, Longchao
    MATERIALS CHARACTERIZATION, 2021, 171
  • [33] Subtransus triplex heat treatment of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe near β titanium alloy
    Liu, C. M.
    Wang, H. M.
    Tian, X. J.
    Tang, H. B.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 590 : 30 - 36
  • [34] Microstructural characterization of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe near β titanium alloy
    Liu, C. M.
    Tian, X. J.
    Tang, H. B.
    Wang, H. M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 572 : 17 - 24
  • [35] Effect of microstructure on fatigue crack tip field of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy
    Wang, Kai
    Bao, Rui
    Ren, Siyuan
    Liu, Dong
    Yan, Chuliang
    12TH INTERNATIONAL FATIGUE CONGRESS (FATIGUE 2018), 2018, 165
  • [36] Evolution of Microstructure and mechanical properties of selective laser melted Ti-5Al-5V-5Mo-3Cr after heat treatments
    Carlton, Holly D.
    Klein, Kyle D.
    Elmer, John W.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2019, 24 (05) : 465 - 473
  • [37] Microstructure and mechanical properties evolution of Ti-5Al-5Mo-5V-1Cr-1Fe alloy under rapid heat treatment
    Qiu, Fucheng
    Cheng, Tuo
    Ivasishin, Orest M.
    Savvakin, Dmytro G.
    Ma, Guangyu
    Song, Yuchao
    Xu, Huiyan
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 24 : 4203 - 4217
  • [38] Microstructure, texture and mechanical properties of metastable beta titanium alloy Ti-5Al-5Mo-5V-3Cr
    Manda, Premkumar
    Saleem, Shaik
    Rao, K. Srinivasa
    Singh, A. K.
    ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, 2022, 8 (02) : 1916 - 1945
  • [39] Evaluation of microstructure and mechanical properties of additively manufactured Ti-5V-5Mo-5 Al-3 Cr alloy
    Casias, Zachary J.
    Kumar, Pankaj
    Pegues, Jonathan
    Buckner, Jessica
    Craig, Robert
    Carroll, Jay D.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 912
  • [40] Influence of heat treatment on mechanical properties of Ti-5Al-5V-5Mo-3Cr
    Otto Fuchs KG, Meinerzhagen, Germany
    不详
    不详
    不详
    VDI Ber., 2008, 2028 (183-193):