摘要
This data article reports a systematic fractographic analysis of SiC-based filaments aiming at stress intensity factors assessment. A total of 11 fiber types (as-received or chlorinated Nicalon (R) and Tyranno (R) of all three generations) where therefore repeatedly tensile tested to generate the fracture surfaces. The tensile strengths were found to be independent to defect location (surface or internal). The wellknown linear square root dependence of strength on mirror, mist or hackle outer radius was reaffirmed. These measurements reveal some residual tensile stresses on Nicalon (R) fibers, statement however questioned by the broad data scattering. Moreover, it is shown the surface etching treatment didn't affected (generating or releasing) such residual stress. A null y -intercept was consequently adopted to assess the characteristic stress intensity factors (K-IC, mirror, mist or hackle constants). The toughness (K-IC) estimated this way ranges from 1.0 to 1.9 MPa m(1/2) and shows a clear dependency to substrate composition: higher values were extracted on oxygen-free fibers. The A(m)/K-IC ratio, estimated to equal 1.8 and independent to substrate type, is a key parameter that would assist further fractographic investigations. (c) 2020 Published by Elsevier Inc. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/)
引用
收藏
页数:26
相关论文
共 50 条
  • [31] Fabrication of solid-phase-sintered SiC-based composites with short carbon fibers
    Xian-hui Li
    Qing-zhi Yan
    Yong-jun Han
    Mei-qi Cao
    Chang-chun Ge
    International Journal of Minerals, Metallurgy, and Materials, 2014, 21 : 1141 - 1145
  • [32] Sic-based ceramic fibers derived from polymer blend of polycarbosilane-polymethylsilane
    Narisawa, M
    Oura, T
    Shimoda, K
    Tsuda, H
    Nakatani, H
    Okamura, K
    Oka, K
    Dohmaru, T
    HIGH TEMPERATURE CERAMIC MATRIX COMPOSITES 5, 2005, : 17 - 22
  • [33] Fabrication of solid-phase-sintered SiC-based composites with short carbon fibers
    Li, Xian-hui
    Yan, Qing-zhi
    Han, Yong-jun
    Cao, Mei-qi
    Ge, Chang-chun
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2014, 21 (11) : 1141 - 1145
  • [34] Performance Analysis of Different SIC-Based Methods for Multipath Cancelation
    Aguilera, T.
    Alvarez, F. J.
    Paredes, Jose A.
    Morera, Jorge
    Moreno, Jose A.
    2015 INTERNATIONAL CONFERENCE ON INDOOR POSITIONING AND INDOOR NAVIGATION (IPIN), 2015,
  • [35] Generalized BER Performance Analysis for SIC-Based Uplink NOMA
    Alaaeldin, Mahmoud
    Alsusa, Emad
    Al-Jarrah, Mohammad
    Seddik, Karim G.
    Matthaiou, Michail
    IEEE OPEN JOURNAL OF THE COMMUNICATIONS SOCIETY, 2025, 6 : 1246 - 1265
  • [36] SiC-based gas sensor development
    Hunter, Gary W.
    Neudeck, Philip G.
    Gray, M.
    Androjna, D.
    Chen, Liang-Yu
    Hoffman Jr., Richard W.
    Liu, C.C.
    Wu, Q.H.
    Materials Science Forum, 2000, 338
  • [37] Fundamentals of SiC-based device processing
    Melloch, MR
    Cooper, JA
    MRS BULLETIN, 1997, 22 (03) : 42 - 47
  • [38] SiC-based current limiter devices
    Chante, JP
    Tournier, D
    Planson, D
    Raynaud, C
    Lazar, M
    Locatelli, ML
    Brosselard, P
    SILICON CARBIDE AND RELATED MATERIALS 2003, PTS 1 AND 2, 2004, 457-460 : 951 - 956
  • [39] Fundamentals of SiC-Based Device Processing
    M. R. Melloch
    J. A. Cooper
    MRS Bulletin, 1997, 22 : 42 - 49
  • [40] Nanoindentation characterization of SiC-based ceramics
    Guicciardi, Stefano
    Balbo, Andrea
    Sciti, Diletta
    Melandri, Cesare
    Pezzotti, Giuseppe
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (2-3) : 1399 - 1404