Electro discharge compaction of WC-Co composite material containing particles of diamond

被引:6
|
作者
Grigoriev, Eugene [1 ]
Rosliakov, Alexander [1 ]
机构
[1] Moscow Phys Engn Inst, Gen Phys Dept, Kashirskoe Sh 31, Moscow 115409, Russia
来源
关键词
powder; pressure; pulse; heating;
D O I
10.4028/www.scientific.net/MSF.534-536.1181
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present paper, the formation of high hardness and large strength structure of WC-Co composite material containing particles of diamond were investigated and optimal operating parameters were defined. Tungsten carbide - cobalt - diamond composite was produced by the method of high voltage electrical discharge together with applying mechanical pressure to powder compact. It was found that the density and hardness of composite material reach its maximum values at certain magnitudes of applied pressure and high voltage electrical discharge parameters. We found that there is [a maximum level -Comment: Don't you mean a maximum level?] for the discharge voltage and applied pressure beyond which the powder WC-Co-diamond composite material disintegrates like an exploding wire. Near this level, the cobalt particles are in a fused condition and are redistributed in the compact volume due to magnetic pressure of discharge current pulse. [The distribution of magnetic pressure is defined by the distribution of a current density in the powder compact. The magnetic pressure is more homogeneous in powder compact volume when the skin effect is strong. -Comment: Are these two statements of fact or conclusions made based on experimental observations? - Answer: The first statement is fact and the second statement is conclusion made based on experimental observations.]
引用
收藏
页码:1181 / +
页数:2
相关论文
共 50 条
  • [21] Nucleation rate of diamond films on WC-Co alloys
    Liu, S
    SURFACE REVIEW AND LETTERS, 2005, 12 (03) : 319 - 324
  • [22] WC-Co cutting tool inserts with diamond coatings
    Silva, S
    Mammana, VP
    Salvadori, MC
    Monteiro, OR
    Brown, IG
    DIAMOND AND RELATED MATERIALS, 1999, 8 (10) : 1913 - 1918
  • [23] High quality diamond films on WC-Co surfaces
    Guseva, MB
    Babaev, VG
    Khvostov, VV
    Ludena, GML
    Bregadze, AY
    Konyashin, IY
    Alexenko, AE
    DIAMOND AND RELATED MATERIALS, 1997, 6 (01) : 89 - 94
  • [24] Influence of boron on diamond growth on WC-Co hardmetals
    Kalss, W
    Bohr, S
    Haubner, R
    Lux, B
    Griesser, M
    Spicka, H
    Grasserbauer, M
    Wurzinger, P
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 1996, 14 (1-3): : 137 - 144
  • [25] High quality diamond films on WC-Co surfaces
    Physics Department, Moscow State University, Vorobjevy Gory, Moscow, 119899, Russia
    不详
    不详
    不详
    Diamond Relat. Mat., 1 (89-94):
  • [26] WC-Co cutting tool inserts with diamond coatings
    Univ of Sao Paulo, Sao Paulo, Brazil
    Diamond Relat Mater, 10 (1913-1918):
  • [27] Diamond-coated WC-Co cutting tools
    Inspektor, A
    Bauer, CE
    Gates, AS
    Oles, EJ
    ISRAEL JOURNAL OF CHEMISTRY, 1998, 38 (1-2) : 85 - 91
  • [28] Microstructure of WC in WC-Co cemented carbides consolidated by electric discharge
    Wu, X. Y.
    Zhang, W.
    Li, D. X.
    Guo, J. D.
    MATERIALS SCIENCE AND TECHNOLOGY, 2007, 23 (05) : 627 - 629
  • [29] SINTERING OF NANOCRYSTALLINE WC-Co COMPOSITE POWDER
    Shao, Gang-qin
    Duan, Xing-long
    Xie, Ji-ren
    Yu, Xiao-hua
    Zhang, Wei-feng
    Yuan, Run-zhang
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2003, 5 (04) : 281 - 286
  • [30] Sintering behavior of nanostructured WC-Co composite
    Kumar, Akshay
    Singh, K.
    Pandey, O. P.
    CERAMICS INTERNATIONAL, 2011, 37 (04) : 1415 - 1422