Deformation and fracture, during cooling, of the alumina scale developed on Fe3Al

被引:4
|
作者
Griffin, D [1 ]
Daadbin, A [1 ]
Datta, PK [1 ]
机构
[1] Northumbria Univ, Sch Engn, Surface Engn Res Ctr, Newcastle Upon Tyne NE1 8ST, Tyne & Wear, England
来源
SURFACE & COATINGS TECHNOLOGY | 2000年 / 126卷 / 2-3期
关键词
spallation; finite element analysis; scale fracture; deformation;
D O I
10.1016/S0257-8972(00)00528-4
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The deformation and fracture, during cooling, of oxide scales developed on Fe3Al has been modelled using finite element analysis (FEA). Embedded defects were introduced at the oxide surface and at the oxide/substrate interface; the propagation of these defects and the influence of such propagation on scale spallation was analysed under both elastic and elastic plastic conditions. Stress relaxation associated with the plastic deformation of the substrate delayed scale spallation as indicated by the greater temperature drop required to cause spallation. In this situation, the presence of the oxide surface crack influenced scale spallation in a complex manner. The oxide surface crack did not influence the scale spallation process for the linear elastic analysis, which was solely controlled by the interfacial defect. (C) 2000 Published by Elsevier Science S.A. All rights reserved.
引用
收藏
页码:142 / 151
页数:10
相关论文
共 50 条
  • [41] The Microstructure Evolution of a Fe3Al Alloy during the LENS Process
    Karczewski, Krzysztof
    Durejko, Tomasz
    Czujko, Tomasz
    MATERIALS, 2018, 11 (03):
  • [42] INTERNAL OXIDATION OF Fe3Al DURING HIGH TEMPERATURE OXIDATION
    Wang Yonggang1
    TransactionsofNonferrousMetalsSocietyofChina, 1998, (01) : 53 - 56
  • [43] TRANSITION FROM HYDROGEN INDUCED CLEAVAGE FRACTURE TO HYDROGEN INDUCED INTERGRANULAR FRACTURE IN FE3AL
    LIN, JP
    CHU, WY
    ZHANG, DZ
    HSIAO, CM
    SCRIPTA METALLURGICA ET MATERIALIA, 1992, 27 (10): : 1295 - 1299
  • [44] Internal oxidation of Fe3Al during high temperature oxidation
    Wang, YG
    He, YD
    Zhu, RH
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 1998, 8 (01) : 52 - 55
  • [45] Fine surface microstructure of Fe3Al alloy after severe plastic deformation
    Ren, Jiangwei
    Li, Dong
    MATERIALS LETTERS, 2016, 171 : 133 - 136
  • [46] Magnetic observation of deformation substructure in cyclically deformed Fe3Al single crystals
    Yasuda, HY
    Hatta, T
    Umakoshi, Y
    SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS, 2004, 5 (1-2) : 3 - 9
  • [47] Transgranular cleavage fracture of Fe3Al intermetallics induced by moisture and aqueous environments
    Mao, SX
    Qiao, L
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 258 (1-2): : 187 - 195
  • [48] Fracture behaviour of Fe3Al alloy with additions of Zr and C at different temperatures
    Prahl, J
    Hausild, P
    Karlík, M
    Crenn, JF
    KOVOVE MATERIALY-METALLIC MATERIALS, 2005, 43 (02): : 134 - 144
  • [49] Internal stresses and textures of nanostructured alumina scales growing on polycrystalline Fe3Al alloy
    Brito, Pedro
    Pinto, Haroldo
    Klaus, Manuela
    Genzel, Christoph
    Kaysser-Pyzalla, Anke
    POWDER DIFFRACTION, 2010, 25 (02) : 114 - 118
  • [50] Transgranular cleavage fracture of Fe3Al intermetallics induced by moisture and aqueous environments
    Mao, Scott X.
    Qiao, L.
    Materials Science and Engineering A, 1998, 258 (1-2): : 187 - 195