Effect of quasi-hydrostatic compression on the mechanical properties of ceramics in the ZrO2+3 mol.% Y2O3 system

被引:2
|
作者
Akimov, GY [1 ]
Prokhorov, IY [1 ]
Timehenko, VM [1 ]
机构
[1] Natl Acad Sci Ukraine, AA Galkin Donetsk Inst Engn Phys, Donetsk, Ukraine
关键词
Polymer; Japan; Mechanical Property; Martensite; Pressure Drop;
D O I
10.1023/A:1019651027479
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of quasi-hydrostatic compression on the strength of ZrO2 + 3 mol.% Y2O3 ceramic specimens of two series was studied. The series I ceramic was a powder commercially available from TOSOH Co. (Japan), with a density of 6.1g/cm(3), and the series 2 ceramic was a powder with a density of 5.9 g/cm(3) prepared under laboratory conditions at the IPM Research Institute (National Academy of Sciences, Ukraine). The pressure range was up to 1.2 GPa, and the pressure-transmitting medium was a coarse-grained corundum powder. In the series I specimens, the strength increases with pressure over the entire pressure range (from 670 MPa to 1098 MPa at 1.2 GPa); in the series 2 specimens, the strength increases only to a pressure of 0.8 GPa (from 695 MPa to 828 MPa) and then, with further increase in pressure drops sharply to nearly zero (30 MPa at 1.2 GPa). It Was proposed that the observed effect might be associated with a martensite transformation in the zone of structural imperfections (discontinuities). On reaching a critical value determined by the strength of the matrix, the martensite transformation becomes a cause of failure of the material.
引用
收藏
页码:100 / 102
页数:3
相关论文
共 50 条
  • [21] The Peculiarities of Crack Development in Chevron-Notched Specimens of ZrO2+3% Y2O3 Ceramics
    Deryugin, E. E.
    Panin, V. E.
    Lasko, G. V.
    Danilenko, I.
    Schmauder, S.
    PROCEEDINGS OF THE ADVANCED MATERIALS WITH HIERARCHICAL STRUCTURE FOR NEW TECHNOLOGIES AND RELIABLE STRUCTURES, 2018, 2051
  • [22] The characteristic frequencies for ionic conduction in 12 mol.% Y2O3 doped ZrO2
    Luo, J
    Hairetdinov, EF
    Almond, DP
    Stevens, R
    SOLID STATE IONICS, 1999, 122 (1-4) : 205 - 210
  • [23] The effect of prestressing on the fracture toughness of ZrO2-(3,4) mol % Y2O3 ceramics
    Akimov, GY
    Timchenko, VM
    TECHNICAL PHYSICS, 2001, 46 (01) : 125 - 126
  • [24] Growth kinetics of sintered NiO/ZrO2 (5 mol.% Y2O3) composites
    Chen, Shueiyuan
    Shen, Pouyan
    Gan, Dershin
    Materials Science and Engineering A, 1992, A158 (02) : 251 - 258
  • [25] Effect of Al2O3 on the properties of nanocrystalline ZrO2 + 3 mol % Y2O3 powder
    E. V. Dudnik
    A. V. Shevchenko
    A. K. Ruban
    V. P. Red’ko
    L. M. Lopato
    Inorganic Materials, 2010, 46 : 172 - 176
  • [26] High-frequency induction heating sintering of hydroxyapatite-(Zro2+3%Mol Y2o3) bioceramics
    Khalil, Khalil Abdel-razek
    Kim, Sug Won
    PROGRESS IN POWDER METALLURGY, PTS 1 AND 2, 2007, 534-536 : 1033 - +
  • [27] Evolution of the phase composition and physicomechanical properties of ZrO2+4 mol % Y2O3 ceramics
    Akimov, GY
    Marinin, GA
    Kameneva, VY
    PHYSICS OF THE SOLID STATE, 2004, 46 (02) : 254 - 257
  • [28] Evolution of the phase composition and physicomechanical properties of ZrO2 + 4 mol % Y2O3 ceramics
    G. Ya. Akimov
    G. A. Marinin
    V. Yu. Kameneva
    Physics of the Solid State, 2004, 46 : 254 - 257
  • [29] Effect of the loading rate on the mechanical properties of polycrystalline samples of a ZrO2-3 mol% Y2O3 solid solution
    Akimov, GY
    Timchenko, VM
    PHYSICS OF THE SOLID STATE, 1997, 39 (05) : 783 - 786
  • [30] Effect of Pore Size on the Mechanical Properties and Deformation Behavior of Porous ZrO2(Y2O3) Ceramics Under Axial Compression
    I. N. Sevostyanova
    V. V. Gorbatenko
    Russian Physics Journal, 2024, 67 (7) : 879 - 887