Effect of heat treatments on the microstructure and mechanical properties of a cast intermetallic Ti-44Al-4Nb-4Zr-0.2Si-0.3B alloy

被引:0
|
作者
Lapin, J.
Gabalcova, Z.
Bajana, O.
Daloz, D.
机构
[1] Slovak Acad Sci, Inst Mat & Machine Mech, Bratislava 83102, Slovakia
[2] Ecole Natl Super Mines, LSG2M, F-54042 Nancy, France
来源
KOVOVE MATERIALY-METALLIC MATERIALS | 2006年 / 44卷 / 06期
关键词
titanium aluminides; TiAl; heat treatment; microstructure; mechanical properties;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of two types of heat treatment, (i) cyclic heat treatment composed of annealing at temperatures ranging from 1523 to 1623 K combined with oil quenching and (ii) heat treatment consisting of annealing at a constant annealing temperature of 1623 K combined with cooling at constant rates ranging from 0.056 to 1.181 K(.)s(-1) on the microstructure and mechanical properties of a cast Ti-44Al-4Nb-4Zr-0.2Si-0.3B (at.%) alloy was studied. Grain size and Vickers hardness are decreased to final values after the first heat treatment cycle. Increasing number of the cycles has no statistical effect on these parameters. This heat treatment does not improve room-temperature tensile ductility. On the contrary, tensile tests at 1023 K showed clear yielding and plastic elongation before fracture ranging from 0.21 to 0.32 %. Increase of the cooling rate decreases mean interlamellar alpha(2)-alpha(2) spacing within lamellar alpha(2) + gamma grains and leads to formation of numerous equiaxed beta(B2), gamma and omega grains in the microstructure. Vickers hardness, room-temperature compressive yield stress, high-temperature tensile yield stress and high-temperature ultimate tensile stress increase with increasing cooling rate. Change of the cooling rate does not improve room-temperature ductility.
引用
收藏
页码:297 / 306
页数:10
相关论文
共 50 条
  • [1] Effect of thermal exposure on microstructure and mechanical properties of Ti-44Al-4Nb-4Zr-0.2Si-1B alloy
    Zhu, Xiao-Long
    Huang, Ze-Wen
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2011, 21 (12): : 3042 - 3049
  • [2] Effects of thermal exposure on the microstructure and properties of a γ-TiAl based alloy containing 44Al-4Nb-4Zr-0.2Si-0.3B
    Cheng, TT
    INTERMETALLICS, 1999, 7 (09) : 995 - 999
  • [3] Thermal stability of Ti-44Al-4Nb-4Zr-0.2Si-1B alloy
    Huang, Z. W.
    INTERMETALLICS, 2013, 42 : 170 - 179
  • [4] Effect of Vacuum Sintering Temperature on the Microstructure and Mechanical Properties of Ti-44Al-2Cr-4Nb-0.2W-0.2B Alloy
    Gong Siheng
    Dong Xianjuan
    Xu Yong
    Lu Shiqiang
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (08) : 2950 - 2956
  • [5] Effect of Vacuum Sintering Temperature on the Microstructure and Mechanical Properties of Ti-44Al-2Cr-4Nb-0.2W-0.2B Alloy
    Gong, Siheng
    Dong, Xianjuan
    Xu, Yong
    Lu, Shiqiang
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2021, 50 (08): : 2950 - 2956
  • [6] Microstructure and tensile properties of cast Ti-44Al-4Nb-4Hf-0.1Si-0.1B alloy with refined lamellar microstructures
    Hu, D.
    Jiang, H.
    Wu, X.
    INTERMETALLICS, 2009, 17 (09) : 744 - 748
  • [7] Thermal stability of Ti-44Al-4Nb-4Hf-0.2Si-1B alloy
    Huang, Z. W.
    INTERMETALLICS, 2013, 37 : 11 - 21
  • [8] The decomposition of the beta phase in Ti-44Al-8Nb and Ti-44Al-4Nb-4Zr-0.2Si alloys
    Cheng, TT
    Loretto, MH
    ACTA MATERIALIA, 1998, 46 (13) : 4801 - 4819
  • [9] Mechanical properties of the cast intermetallic alloy Ti-43Al-7(Nb,Mo)-0.2B (at %) after heat treatment
    V. M. Imayev
    R. M. Imayev
    T. G. Khismatullin
    The Physics of Metals and Metallography, 2008, 105
  • [10] Mechanical properties of the cast intermetallic alloy Ti-43Al-7(Nb,Mo)-0.2B (at %) after heat treatment
    Imayev, V. M.
    Imayev, R. M.
    Khismatullin, T. G.
    PHYSICS OF METALS AND METALLOGRAPHY, 2008, 105 (05): : 484 - 490