The effect of 0.5 wt.% Ca addition on the hot compressive characteristics and processing maps of the cast and extruded Mg-3Al-1Zn alloys

被引:26
|
作者
Kwak, T. Y. [1 ,2 ]
Lim, H. K. [1 ]
Kim, W. J. [2 ]
机构
[1] Korea Inst Ind Technol, Rare Met R&BD Grp, Inchon, South Korea
[2] Hongik Univ, Dept Mat Sci & Engn, Seoul 121791, South Korea
基金
新加坡国家研究基金会;
关键词
Metals and alloys; Liquid-solid reactions; Mechanical properties; Microstructure; Grain boundaries; AZ31 MAGNESIUM ALLOY; MICROSTRUCTURE EVOLUTION; MECHANICAL-PROPERTIES; DEFORMATION-BEHAVIOR; PLASTIC-DEFORMATION; HIGH-TEMPERATURE; RESISTANCE; STABILITY; IGNITION; WORKING;
D O I
10.1016/j.jallcom.2015.10.193
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The hot compressive characteristics and processing maps of the extruded 0.5 wt.% Ca-AZ31 (Ca-AZ31) alloy and the extruded AZ31 alloy were examined and compared in the temperature range between 473 and 673 K and in the strain rate range between 10(-3) and 10 s(-1). The extruded Ca-AZ31 alloy had a smaller grain size (10.64 vs. 23.44 mm) and a more homogeneous microstructure than the extruded AZ31 alloy due to the presence of thermally stable Al2Ca particles in the former. The addition of 0.5 wt.% Ca increased the ignition temperature of AZ31 by 270.5 K. While the added Ca did not affect the activation energy for plastic flow, it slightly decreased the stress exponent and increased the flow stress level. Dislocation climb creep associated with stress exponents of 5-7 dominated the plastic flow of the extruded AZ31 and extruded Ca-AZ31 alloys. The power-law breakdown did not appear in either alloy under the given testing conditions. In comparison with the extruded AZ31 alloy, the extruded Ca-AZ31 alloy exhibited a poor hot workability at low temperatures below 523 K. However, there was an improved hot workability at higher temperatures due to the presence of the Al2Ca particles that promoted dynamic recrystallization (DRX) and retarded coarsening of the DRXed grains. Compared with the extruded Ca-AZ31 alloy, the cast Ca-AZ31 alloy with a much larger grain size (86.2 mm) and a coarser secondary phase structure exhibited a poor hot workability at high strain rates (10(-1)-10(0) s(-1)) over the entire testing temperature range due to the occurrence of unstable flow. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:157 / 169
页数:13
相关论文
共 50 条
  • [21] Effect of Zn addition on hot tearing behaviour of Mg-0.5Ca-xZn alloys
    Song, Jiangfeng
    Wang, Zhi
    Huang, Yuanding
    Srinivasan, Arnirthalingam
    Beckmann, Felix
    Kainer, Karl Ulrich
    Hort, Norbert
    MATERIALS & DESIGN, 2015, 87 : 157 - 170
  • [22] The Effect of Extrusion Temperatures on Microstructure and Mechanical Properties of Mg-1.3Zn-0.5Ca (wt.%) Alloys
    Zhang, Honglin
    Xu, Zhigang
    Kecskes, Laszlo J.
    Yarmolenko, Sergey
    Sankar, Jagannathan
    CRYSTALS, 2021, 11 (10)
  • [23] Effect of 0.45 wt.% Nd Addition on the Corrosion Resistance of Extruded Mg-6Al-3Sn-2Zn Alloy
    Lv, Bin-Jiang
    Gao, Fu-Hao
    Lv, Jun-Jiang
    Peng, Jian
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (16) : 8262 - 8273
  • [24] Morphology and Mechanical, Corrosive, and Antibacterial Behaviors of Indirectly Extruded Zn-0.05 wt.%Mg-(0.5, 1 wt.%)Ag Alloys (pg 1, 2019)
    Xiao, C.
    Zhao, D. W.
    Sun, Q.
    Su, Y.
    Cui, D. P.
    Zhang, X. Z.
    Dong, X. L.
    Wang, H. X.
    Wang, F.
    Ren, Y. P.
    Qin, G. W.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (11) : 6873 - 6873
  • [25] Morphology and Mechanical, Corrosive, and Antibacterial Behaviors of Indirectly Extruded Zn-0.05wt.%Mg-(0.5, 1 wt.%)Ag Alloys
    C. Xiao
    D. W. Zhao
    Q. Sun
    Y. Su
    D. P. Cui
    X. Z. Zhang
    X. L. Dong
    H. X. Wang
    F. Wang
    Y. P. Ren
    G. W. Qin
    Journal of Materials Engineering and Performance, 2019, 28 : 6864 - 6872
  • [26] Hot deformation behavior and processing maps of as-cast Mg-8Zn-1Al-0.5Cu-0.5Mn alloy
    Zhu, Shao-zhen
    Luo, Tian-jiao
    Zhang, Ting-an
    Yang, Yuan-sheng
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (10) : 3232 - 3239
  • [27] Microstructure and texture studies on twin-roll cast AZ31 (Mg-3 wt.%Al-1 wt.%Zn) alloy and the effect of thermomechanical processing
    Masoumi, M.
    Zarandi, F.
    Pekguleryuz, M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (03): : 1268 - 1279
  • [28] Effect of Cu and Zn addition on the hot deformation behavior of Al-5.5wt.%Mg alloys
    Kang, SB
    Ko, HS
    Kim, HW
    Lee, ST
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 2000, 331-3 : 835 - 842
  • [29] Microstructure and mechanical properties of hot-extruded Mg-2Zn-xGa (x=1, 3, 5 and 7 wt.%) alloys
    Zhang, Ziyue
    He, Donglei
    Zheng, Yang
    Wu, Yan
    Li, Qiquan
    Gong, Hao
    Ma, Xiaolong
    Li, Yan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 859
  • [30] Geometrical compatibility factor analysis of paired extension twins in extruded Mg-3Al-1Zn alloys
    Xin, Renlong
    Liang, Yingchun
    Ding, Changhong
    Guo, Changfa
    Wang, Bingshu
    Liu, Qing
    MATERIALS & DESIGN, 2015, 86 : 656 - 663