Erosion Wear Behavior of Martensitic Stainless Steel Under the Hydro-Abrasive Condition of Hydropower Plants

被引:18
|
作者
Sharma, Shubham [1 ]
Gandhi, Bhupendra K. [1 ]
机构
[1] IIT Roorkee, Dept Mech & Ind Engn, Roorkee 247667, Uttar Pradesh, India
关键词
CA6NM; erosive wear; failure mechanism; hydro-abrasive condition; slurry pot tester; suspension loading; SLURRY-EROSION; VELOCITY; DESIGN; ANGLE;
D O I
10.1007/s11665-020-05238-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The erosive wear of a hydraulic turbine due to suspended solid particles reduces its performance and service life. Martensitic stainless steel CA6NM, used for turbine parts of a hydropower plant, gets eroded heavily every year, particularly in the monsoon period. A high-speed slurry pot tester is employed to investigate the erosion behavior of the material under different operating conditions of practical interest. Scanning electron microscopy (SEM), as well as spark emission spectrometer (SES) and micro-hardness tester measurements, is used to investigate the erosion wear behavior of CA6NM. The impingement velocity is varied from 13 to 32 m/s for the particle size of 90.5-362.5 mu m and solid concentration of 500-4000 ppm at different orientation angles ranging from 15 degrees to 90 degrees. The erosion rate for suspension loading is increased with the increase in the impact velocity and particle size but decreased with an increase in suspension concentration. The index value in power-law relationship with erosion rate is found as 2.77 and 3.19 for velocity, and 1.42 and 0.97 for particle size for impingement angle of 30 degrees and 90 degrees, respectively. The micrographic analysis of the eroded sample is performed through a scanning electron microscope (SEM). At shallow impingement angle, the material loss dominantly occurred by micro-cutting and plowing, but at high impact velocity, some spackle of brittle failure is also observed. At large impingement angles, deep craters and crack formation are found responsible for the material loss under the present operating conditions.
引用
收藏
页码:7544 / 7554
页数:11
相关论文
共 50 条
  • [31] Wear Behavior of Plasma-Nitrided 2Cr13 Martensitic Stainless Steel under Air and Vacuum
    Yang Jianqun
    Liu Yong
    Ye Zhuyu
    Yang Dezhuang
    He Shiyu
    [J]. ADVANCED TRIBOLOGY, 2009, : 285 - 286
  • [32] Erosion-corrosion of duplex stainless steel under Kuwait marine condition
    Hussain, E
    Husain, A
    [J]. DESALINATION, 2005, 183 (1-3) : 227 - 234
  • [33] Hydro-abrasive erosion and cavitation-silt erosion characteristics of HVOF sprayed WC-Ni cermet coatings under different flow velocities and sand concentrations
    Hong, Sheng
    Mei, Dongcheng
    Wu, Jianhua
    Lin, Jinran
    Wu, Yuping
    Li, Jiahui
    Zheng, Yuan
    [J]. CERAMICS INTERNATIONAL, 2023, 49 (01) : 74 - 83
  • [34] ABRASIVE WEAR BEHAVIOR OF AN AISI-5132 STEEL UNDER LOW STRESSES
    MODI, OP
    PRASAD, BK
    DAS, S
    JHA, AK
    YEGNESWARAN, AH
    [J]. MATERIALS TRANSACTIONS JIM, 1994, 35 (01): : 67 - 73
  • [35] Aging condition and trapped hydrogen effects on the mechanical behavior of a precipitation hardened martensitic stainless steel
    Snir, Y.
    Haroush, S.
    Dannon, A.
    Landau, A.
    Eliezer, D.
    Gelbstein, Y.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 805 : 509 - 516
  • [36] Modeling the Flow Curve Characteristics of 410 Martensitic Stainless Steel Under Hot Working Condition
    Momeni, Amir
    Dehghani, Kamran
    Ebrahimi, Golam Reza
    Keshmiri, Hamid
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (11): : 2898 - 2904
  • [37] Modeling the Flow Curve Characteristics of 410 Martensitic Stainless Steel Under Hot Working Condition
    Amir Momeni
    Kamran Dehghani
    Golam Reza Ebrahimi
    Hamid Keshmiri
    [J]. Metallurgical and Materials Transactions A, 2010, 41 : 2898 - 2904
  • [38] Abrasive slurry wear behavior of stainless steel surface produced by plasma transferred arc hardfacing process
    Balasubramanian, V.
    Varahamoorthy, R.
    Ramachandran, C. S.
    Babu, S.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2008, 202 (16): : 3903 - 3912
  • [39] CHARACTERISTIC BEHAVIOR OF PRECIPITATION HARDENING MARTENSITIC STAINLESS-STEEL UNDER SOLUTION TREATMENT
    IKEGAMI, Y
    [J]. TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1415 - 1415
  • [40] Effect of martensitic phase transformation on the behavior of 304 austenitic stainless steel under tension
    Wang, H.
    Jeong, Y.
    Clausen, B.
    Liu, Y.
    McCabe, R. J.
    Barlat, F.
    Tome, C. N.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 649 : 174 - 183