Molten Salt Corrosion Behaviors and Mechanisms of Ytterbium Silicate Environmental Barrier Coating

被引:8
|
作者
Liu Pingping [1 ,2 ]
Zhong Xin [1 ]
Zhang Le [3 ]
Li Hong [2 ]
Niu Yaran [1 ]
Zhang Xiangyu [1 ]
Li Qilian [3 ]
Zheng Xuebin [1 ]
机构
[1] Chinese Acad Sci, Shanghai Inst Ceram, Shanghai 200050, Peoples R China
[2] Shanghai Univ, Res Ctr Composite Mat, Shanghai 200072, Peoples R China
[3] Av Mfg Technol Inst, Beijing 100024, Peoples R China
基金
上海市自然科学基金;
关键词
environmental barrier coating; ytterbium silicate; Na2SO4+25% NaCl molten salt; corrosion mechanism; PHYSICAL VAPOR-DEPOSITION; HOT CORROSION; THERMOMECHANICAL PROPERTIES; MICROSTRUCTURE EVOLUTION; THERMAL-PROPERTIES; CRYSTAL-STRUCTURE; WATER-VAPOR; RE2SIO5; RE; GAMMA-Y2SI2O7; COMPOSITE;
D O I
10.15541/jim20220265
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Environmental barrier coating (EBC) is essential for protection of ceramic matrix composite hot-sections in future gas turbine engines with high thrust-to-weight ratio. Rare-earth silicates, such as Yb2SiO5 and Yb2Si2O7, have been developed for potential application as EBC. However, the corrosion behaviors and mechanisms of EBC in molten salt environment such as Na2SO4 at high temperature are not clear. In this work, the Yb2SiO5/Yb2Si2O7/Si coating was prepared by vacuum plasma spraying (VPS). The molten salt (Na2SO4+25% NaCl, in mass) corrosion behaviors and mechanisms of the coating at 900 degrees C for 60-240 h were investigated. Results showed that the Yb2SiO5/Yb2Si2O7/Si coating exhibited dense structure with good bonding between the triple ceramic layers. The molten salt of Na2SO4+25% NaCl penetrated the Yb2SiO5 top layer and enriched in the Yb2Si2O7 interlayer, while the interfacial bonding between the coating and substrate still remained good after corrosion for 240 h. The Yb2SiO5 phase in the top layer exhibited good stability, while the second phase of the Yb2O3 reacted with molten salt. The content of the Yb2O3 decreased with the increase of corrosion time. The Yb2Si2O7 phase in the interlayer reacted with molten salt to form apatite phase of NaYb9Si6O26 and sodium silicate as well as volatile species such as Cl-2 and SO2, which might shorten the service life of the coating. Moreover, there was almost no molten salt in the silicon bond layer, which remained intact. The Yb2SiO5/Yb2Si2O7/Si coating exhibited good resistance to molten salt corrosion.
引用
收藏
页码:1267 / 1274
页数:8
相关论文
共 34 条
  • [11] Synthesis, structure, and polymorphism of A3LnSi2O7 (A=Na, K; Ln=Sm, Ho, Yb)
    Latshaw, Allison M.
    Yeon, Jeongho
    Smith, Mark D.
    zur Loye, Hans-Conrad
    [J]. JOURNAL OF SOLID STATE CHEMISTRY, 2016, 235 : 100 - 106
  • [12] Influence of rare earth cation size on the crystal structure in rare earth silicates, Na2RESiO4(OH) (RE = Sc, Yb) and NaRESiO4 (RE = La, Yb)
    Latshaw, Allison M.
    Wilkins, Branford O.
    Chance, W. Michael
    Smith, Mark D.
    zur Loye, Hans-Conrad
    [J]. SOLID STATE SCIENCES, 2016, 51 : 59 - 65
  • [13] LEE K N, 2022, ADV ENV BARRIER COAT
  • [14] Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics
    Lee, KN
    Fox, DS
    Bansal, NP
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2005, 25 (10) : 1705 - 1715
  • [15] Water vapor corrosion resistance and failure mechanism of SiCf/SiC composites completely coated with plasma sprayed tri-layer EBCs
    Li, Gui
    Qin, Lu
    Cao, Xueqiang
    Lu, Xiangrong
    Tu, Yunwei
    Zhang, Hao
    Jiang, Jianing
    Deng, Longhui
    Dong, Shujuan
    Liu, Li
    An, Wenran
    [J]. CERAMICS INTERNATIONAL, 2022, 48 (05) : 7082 - 7092
  • [16] AlxCoCrFeNi high entropy alloys with superior hot corrosion resistance to Na2SO4+25% NaCl at 900 °C
    Li, Ling
    Lu, Jie
    Liu, Xuanzhen
    Dong, Tao
    Zhao, Xiaofeng
    Yang, Fan
    Guo, Fangwei
    [J]. CORROSION SCIENCE, 2021, 187
  • [17] Calcium-magnesium-aluminosilicate corrosion behaviors of rare-earth disilicates at 1400 °C
    Liu, Jia
    Zhang, Litong
    Liu, Qiaomu
    Cheng, Laifei
    Wang, Yiguang
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (15-16) : 3419 - 3428
  • [18] LIU P P, 2022, CORROS SCI
  • [19] Advanced structural ceramics in aerospace propulsion
    Padture, Nitin P.
    [J]. NATURE MATERIALS, 2016, 15 (08) : 804 - 809
  • [20] Plasma spray deposition of tri-layer environmental barrier coatings
    Richards, Bradley T.
    Wadley, Haydn N. G.
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2014, 34 (12) : 3069 - 3083