Helium-Implantation-Induced Damage in NHS Steel Investigated by Slow-Positron Annihilation Spectroscopy

被引:12
|
作者
Li Yuan-Fei [1 ,2 ,3 ]
Shen Tie-Long [1 ]
Gao Xing [1 ]
Gao Ning [1 ]
Yao Cun-Feng [1 ]
Sun Jian-Rong [1 ]
Wei Kong-Fang [1 ]
Li Bing-Sheng [1 ]
Zhang Peng [4 ]
Cao Xing-Zhong [4 ]
Zhu Ya-Bin [1 ]
Pang Li-Long [1 ]
Cui Ming-Huan [1 ]
Chang Hai-Long [1 ]
Wang Ji [1 ,2 ,3 ]
Zhu Hui-Ping [1 ,2 ]
Wang Dong [1 ,2 ]
Song Peng [1 ,2 ]
Sheng Yan-Bin [1 ]
Zhang Hong-Peng [1 ]
Hu Bi-Tao [3 ]
Wang Zhi-Guang [1 ]
机构
[1] Chinese Acad Sci, Inst Modern Phys, Lanzhou 730000, Peoples R China
[2] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
[3] Lanzhou Univ, Sch Nucl Sci & Technol, Lanzhou 730000, Peoples R China
[4] Chinese Acad Sci, Inst High Energy Phys, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
METALS; IRRADIATION; DEFECTS; ALLOYS;
D O I
10.1088/0256-307X/31/3/036101
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
Evolutions of defects and helium contained defects produced by atomic displacement and helium deposition with helium implantation at different temperatures in novel high silicon (NHS) steel are investigated by a slow positron beam. Differences of the defect information among samples implanted by helium to a fluence of 1 x 10(17) ions/cm(2) at room temperature, 300 degrees C, 450 degrees C and 750 degrees C are discussed. It is found that the mobility of vacancies and vacancy clusters, a recombination of vacancy-type defects and the formation of the He-V complex lead to the occurrence of these differences. At high temperature irradiations, a change of the diffusion mechanism of He atoms/He bubbles might be one of the reasons for the change of the S-parameter.
引用
收藏
页数:4
相关论文
共 37 条
  • [21] Slow positron implantation spectroscopy of high current ion nitrided austenitic stainless steel
    Anwand, W
    Parascandola, S
    Richter, E
    Brauer, G
    Coleman, PG
    Moller, W
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 1998, 136 : 768 - 772
  • [22] Hydrogen-damaged defects near the surface in heavily deformed iron and steels investigated by slow positron annihilation spectroscopy
    Wu, Y. C.
    Jean, Y. C.
    PHYSICA STATUS SOLIDI C - CURRENT TOPICS IN SOLID STATE PHYSICS, VOL 4, NO 10, 2007, 4 (10): : 3506 - +
  • [23] Vacancy defects in a stress-corrosion-cracked Type 304 stainless steel investigated by positron annihilation spectroscopy
    Yabuuchi, A.
    Maekawa, M.
    Kawasuso, A.
    JOURNAL OF NUCLEAR MATERIALS, 2011, 419 (1-3) : 9 - 14
  • [24] Neutron damage in reactor pressure-vessel steel examined with positron annihilation lifetime spectroscopy
    Cumblidge, SE
    Motta, AT
    Catchen, GL
    MICROSTRUCTURE EVOLUTION DURING IRRADIATION, 1997, 439 : 483 - 488
  • [25] Study of defect complexes and their evolution with temperature in hydrogen and helium irradiated RAFM steel using positron annihilation spectroscopy
    Ramachandran, Renjith
    David, C.
    Magudapathy, P.
    Rajaraman, R.
    Govindaraj, R.
    Amarendra, G.
    FUSION ENGINEERING AND DESIGN, 2019, 142 : 55 - 62
  • [26] Strain relaxation induced by He-implantation at the Si1-xGex/Si(100) interface investigated by positron annihilation
    Liszkay, L
    Kajcsos, Z
    Barthe, MF
    Desgardin, P
    Hackbarth, T
    Herzog, HJ
    Holländer, B
    Mantl, S
    APPLIED SURFACE SCIENCE, 2002, 194 (1-4) : 136 - 139
  • [27] Ion implantation induced defects in Fe-Cr alloys studied by conventional positron annihilation lifetime spectroscopy
    Krsjak, V.
    Sojak, S.
    Slugen, V.
    Petriska, M.
    INTERNATIONAL WORKSHOP ON POSITRON STUDIES OF DEFECTS (PSD 08), 2011, 265
  • [28] Raman spectroscopy study of damage and strain in (001) and (011) Si induced by hydrogen or helium implantation
    Villeneuve, C.
    Bourdelle, K. K.
    Paillard, V.
    Hebras, X.
    Kennard, M.
    JOURNAL OF APPLIED PHYSICS, 2007, 102 (09)
  • [29] Vacancy-type defects near Al surface studied by slow positron annihilation spectroscopy before and after He+ implantation
    Chen, C. A.
    Xiang, X.
    Sun, Y.
    Zhou, C. L.
    Ma, C. X.
    Wei, L.
    FUSION ENGINEERING AND DESIGN, 2010, 85 (05) : 734 - 738
  • [30] Vacancy-type defects and hardness of helium implanted CLAM steel studied by positron-annihilation spectroscopy and nano-indentation technique
    Xin, Yong
    Ju, Xin
    Qiu, Jie
    Guo, Liping
    Chen, Jihong
    Yang, Zheng
    Zhang, Peng
    Cao, Xinzhong
    Wang, Baoyi
    FUSION ENGINEERING AND DESIGN, 2012, 87 (5-6) : 432 - 436