Surface protection for AA8090 aluminum alloy by diffusion bonding

被引:25
|
作者
Wu, YW [1 ]
Lo, YL [1 ]
机构
[1] Natl Taiwan Univ Sci & Technol, Dept Mech Engn, Taipei 106, Taiwan
关键词
liquid film protection; AA8090 aluminum alloy; diffusion bonding; chemical etching; contact ratio;
D O I
10.1016/S0167-8442(02)00082-4
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The solid state diffusion bonding process is performed using a liquid film protection (LFP) method for AA8090 aluminum alloy in contrast to the more costly vacuum environment. After chemical etching and prior to bonding, aluminum sheets were immersed in dehydrated alcohol to isolate surface from air. Two sheets are then joined with a special clamp to form a specimen which is press-deformed and heated in a salt bath. Protecting liquid film completely volatilizes on heating to bonding temperature thus keeping bonding surface free from oxidation. Effectiveness of the LFP-method is demonstrated in various combinations of process parameters. The contact ratio, in particular, is an important index for bonding strength. (C) 2002 Published by Elsevier Science Ltd.
引用
收藏
页码:71 / 79
页数:9
相关论文
共 50 条
  • [21] INFLUENCE OF HIP PARAMETERS ON MECHANICAL-PROPERTIES OF AA8090
    HANADA, K
    TAN, MJ
    MURAKOSHI, Y
    NEGISHI, H
    SANO, T
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1995, 48 (1-4) : 399 - 405
  • [22] MECHANICAL-BEHAVIOR OF DOUBLE-AGED AA8090
    BLANKENSHIP, CP
    STARKE, EA
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1993, 24 (04): : 833 - 841
  • [23] Dispersoids in Al-Li AA8090 series alloys
    Waheed, A
    Lorimer, GW
    [J]. JOURNAL OF MATERIALS SCIENCE, 1997, 32 (12) : 3341 - 3347
  • [24] Effect of welding parameters on AA8090 Al-Li alloy FSW T-joints
    Lertora, Enrico
    Mandolfino, Chiara
    Gambaro, Carla
    [J]. CURRENT STATE-OF-THE-ART ON MATERIAL FORMING: NUMERICAL AND EXPERIMENTAL APPROACHES AT DIFFERENT LENGTH-SCALES, PTS 1-3, 2013, 554-557 : 985 - 995
  • [25] AA8090 Al-Li Alloy FSW parameters to minimize defects and increase fatigue life
    E. Lertora
    C. Gambaro
    [J]. International Journal of Material Forming, 2010, 3 : 1003 - 1006
  • [26] Wear behavior and mechanical properties of AA8090 aluminum alloy reinforced with B4C-Al2O3 hybrid nanoparticles
    Narasimmalu, Ramasubbu
    Sundaresan, Ramabalan
    [J]. INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2022, 74 (02) : 237 - 242
  • [27] Optimization of process parameters for friction stir processing (FSP) of AA8090/boron carbide surface composites
    Adiga, Karthik
    Herbert, Mervin A.
    Rao, Shrikantha S.
    Shettigar, Arun Kumar
    [J]. WELDING IN THE WORLD, 2024, 68 (10) : 2683 - 2700
  • [28] Thermal stability of ultrafine grained AA8090 Al-Li alloy processed by repetitive corrugation and straightening
    Raj, Jenix Rino John Xavier
    Shanmugavel, Balasivanandha Prabu
    [J]. JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (03): : 3251 - 3260
  • [29] Mechanical property and microstructural evaluation of friction stir welded AA8090 T87 aluminium alloy
    Shyamlal, Chandrasekaran
    Rajesh, Shanmugavel
    Sankar, Subramaniam Saravana
    Jappes, Jebas ThangiahWinowlin
    [J]. PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART E-JOURNAL OF PROCESS MECHANICAL ENGINEERING, 2023, 237 (06) : 2449 - 2456
  • [30] Severe plastic deformation of a commercial aluminium-lithium alloy (AA8090) by equal channel angular pressing
    Llorca-Isern, N
    Gonzalez, PA
    Luis, CJ
    Laborde, I
    [J]. NANOMATERIALS BY SEVERE PLASTIC DEFORMATION, 2006, 503-504 : 871 - 876