LEACHING AND DECAY RESISTANCE OF ALDER AND PINE WOOD TREATED WITH COPPER BASED WOOD PRESERVATIVES

被引:30
|
作者
Temiz, Ali [1 ]
Alfredsen, Gry [2 ]
Yildiz, Umit C. [1 ]
Gezer, Engin D. [1 ]
Kose, Gaye [1 ]
Akbas, Selcuk [3 ]
Yildiz, Sibel [1 ]
机构
[1] Karadeniz Tech Univ, Fac Forestry, TR-61080 Trabzon, Turkey
[2] Norwegian Forest & Landscape Inst, As, Norway
[3] Artvin Coruh Univ, Fac Forestry, TR-08000 Artvin, Turkey
来源
MADERAS-CIENCIA Y TECNOLOGIA | 2014年 / 16卷 / 01期
关键词
Copper based wood preservatives; wood protection; Alder; Scots pine; leaching of copper; YELLOW PINE; CCA; CHROMIUM; TOXICITY; FIXATION;
D O I
10.4067/S0718-221X2014005000006
中图分类号
TB3 [工程材料学]; TS [轻工业、手工业、生活服务业];
学科分类号
0805 ; 080502 ; 0822 ;
摘要
The objective of this study was to determine the leaching and decay resistance of Alder (Alnus glutinosa subsp. barbata) and Scots pine (Pinus sylvestris) wood samples treated with copper based preservatives. Samples were treated with CCA, ACQ, Tanalith E and Wolmanit with different concentrations. Scots pine samples were exposed the mini-block test against brown rot fungi (Poria placenta) and Coniophora puteana while alder wood samples were tested against brown rot fungi (Coniophora puteana) and white rot fungi (Coriolus versicolor). Regarding to leaching test, treated samples were impregnated with 300 ml of distilled water and after 6, 24, 48 and thereafter at 48-hour intervals, the leachate was removed and replaced with fresh distilled water according to AWPA E11. Samples of each leachate were collected and retained for copper analysis. Amount of copper released from treated wood during the leaching test was chemically analyzed with Atomic Absorption spectroscopy. Perchloric acid procedure for the digestion of wood was used according to AWPA A7-97. The amount of copper component (Qd), the cumulative quantities leached (Qc) and the average daily fluxes (FLUX) were calculated. Results shows that CCA treated samples release less copper compared to other copper based preservatives used in this study. Highest mass losses were obtained from the leached samples treated with 1% of ACQ-2200 against decay fungi.
引用
收藏
页码:63 / 76
页数:14
相关论文
共 50 条
  • [1] Leaching of copper from wood treated with copper based wood preservatives
    Humar, M
    Petric, M
    Pohleven, F
    [J]. WOOD IN CONSTRUCTION INDUSTRY - TRADITION AND FUTURE, 2001, : 39 - 47
  • [2] Combustion and Decay Resistance Performance of Scots Pine Treated with Boron and Copper Based Wood Preservatives
    Surdem, Sedat
    Eseroglu, Cihan
    Yildiz, Serhat
    Sogutlu, Cevdet
    Yorukoglu, Abdulkerim
    [J]. DRVNA INDUSTRIJA, 2022, 73 (04) : 397 - 404
  • [3] The effect of soil type on copper leaching from wood treated with three copper-based wood preservatives
    Baskal, Kadir Sahin
    Yalcin, Mesut
    Akcay, Caglar
    Sarginci, Murat
    [J]. WOOD MATERIAL SCIENCE & ENGINEERING, 2024, 19 (05) : 997 - 1003
  • [4] Resistance of bioincised wood treated with wood preservatives to blue-stain and wood-decay fungi
    Schubert, M.
    Volkmer, T.
    Lehringer, C.
    Schwarze, F. W. M. R.
    [J]. INTERNATIONAL BIODETERIORATION & BIODEGRADATION, 2011, 65 (01) : 108 - 115
  • [5] Influence of water properties on leaching of copper-based preservatives from treated wood
    Humar, M.
    Pohleven, F.
    Zlindra, D.
    [J]. WOOD RESEARCH, 2006, 51 (03) : 69 - 76
  • [6] Leaching of chromated copper arsenate wood preservatives: a review
    Hingston, JA
    Collins, CD
    Murphy, RJ
    Lester, JN
    [J]. ENVIRONMENTAL POLLUTION, 2001, 111 (01) : 53 - 66
  • [7] Analyses of Impregnation Quality and Mechanical Properties of Radiata Pine Wood Treated with Copper Nanoparticle- and Micronized-Copper-Based Wood Preservatives
    Graciela Aguayo, Maria
    Erazo, Oswaldo
    Montero, Claudio
    Reyes, Laura
    Gacitua, William
    Gomez, Liset
    Torres, Hugo
    [J]. FORESTS, 2022, 13 (10):
  • [8] Evaluation of mold, decay and termite resistance of pine wood treated with zinc- and copper-based nanocompounds
    Mantanis, George
    Terzi, Evren
    Kartal, S. Nami
    Papadopoulos, A. N.
    [J]. INTERNATIONAL BIODETERIORATION & BIODEGRADATION, 2014, 90 : 140 - 144
  • [9] Toxicity, tolerance and bioremediation of wood treated with copper based preservatives
    Humar, M
    Pohleven, F
    [J]. WOOD IN CONSTRUCTION INDUSTRY - PROSPECTIVES OF RECONSTRUCTION, 2002, : 17 - 24
  • [10] LEACHING OF WOOD PRESERVATIVES IN PRACTICE
    WILLEITNER, H
    ILLNER, HM
    [J]. HOLZ ALS ROH-UND WERKSTOFF, 1986, 44 (09) : 347 - 350