Wear resistance and wear mechanisms of WC-12%Co thermal sprayed coatings in three-body abrasion

被引:44
|
作者
Bozzi, AC [1 ]
de Mello, JDB [1 ]
机构
[1] Univ Fed Uberlandia, Lab Tribologia & Mat, Dept Ciencias Fis, BR-38400 Uberlandia, MG, Brazil
关键词
WC-12%Co; three-body abrasion; abrasive wear; AISI; 1020;
D O I
10.1016/S0043-1648(99)00206-9
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study, the three-body abrasion resistance of AISI 1020 annealed steel samples coated with WC-12%Co coatings produced by the Jet Kote(R) thermal spray process was evaluated. The tests were performed using SiO2, Al2O3 and SiC as abrasives and five levels of stress ranging from 0.10 to 0.60 MPa. By measuring the weight loss, the wear rate was evaluated after reaching the steady state of wear. Characterisation of the abrasives was performed using an image analyser and scanning electron microscopy. The microstructure and wear mechanisms of the coatings were characterised by scanning electron microscopy. The relationship between stress and wear rate was found to be dependant on abrasive type; this is due to different degrees of fragmentation of the abrasive. The effect of stress on the wear rate depended on the nature of the abrasive due to the fragmentation process of the abrasives. The results indicated that abrasion resistance and predominant wear mechanisms were strongly dependent on abrasive hardness. In tests using SiO2 abrasive a combination of micropolishing associated with gradual degradation of the lamellae was the predominant wear mechanism. Plastic deformation by microploughing and microcutting were the predominant wear mechanism in tests with Al2O3 abrasive. In tests with SiC abrasive, interlamellar brittle fracture was the predominant mechanism. (C) 1999 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:575 / 587
页数:13
相关论文
共 50 条
  • [41] Evaluation of erosive and abrasive wear resistance of the WC 12Co coatings applied HVOF thermal spray
    Xavier Belem, Maria Julia
    Camello Lima, Carlos Roberto
    Kuhl, Amanda
    Camargo, Flavio
    MATERIA-RIO DE JANEIRO, 2020, 25 (01):
  • [42] THE EFFECT OF CARBURIZATION OF ASTM A36 STEEL SUBSTRATE IN IMPROVING WEAR PROPERTIES OF PLASMA SPRAYED WC-12% Co COATING
    Karuppuswamy, P.
    Bhagyanathan, C.
    Narendhar, C.
    Kirupakaran, R. N.
    Kumar, S. D. Arun
    SURFACE REVIEW AND LETTERS, 2017, 24 (05)
  • [43] Wear resistance of thermal sprayed coatings on the base of recycled hardmetal
    Kulu, P
    Zimakov, S
    SURFACE & COATINGS TECHNOLOGY, 2000, 130 (01): : 46 - 51
  • [44] Effects of the dispersion time on the microstructure and wear resistance of WC/Co-CNTs HVOF sprayed coatings
    Rodriguez, M. A.
    Gil, L.
    Camero, S.
    Frety, N.
    Santana, Y.
    Caro, J.
    SURFACE & COATINGS TECHNOLOGY, 2014, 258 : 38 - 48
  • [45] The effect of spraying temperature on the corrosion and wear behavior of HVOF thermal sprayed WC-Co coatings
    Azizpour, M. Jalali
    Tolouei-Rad, M.
    CERAMICS INTERNATIONAL, 2019, 45 (11) : 13934 - 13941
  • [46] Effect of nanostructuring and Al alloying on friction and wear behaviour of thermal sprayed WC-Co coatings
    Basak, A. K.
    Celis, J. -P.
    Vardavoulias, M.
    Matteazzi, P.
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (16): : 3508 - 3516
  • [47] Wear behaviour of laser cladded and plasma sprayed WC-Co coatings
    Cadenas, M
    Vijande, R
    Montes, HJ
    Sierra, JM
    WEAR, 1997, 212 (02) : 244 - 253
  • [48] Sliding wear investigation of suspension sprayed WC-Co nanocomposite coatings
    Ahmed, R.
    Ali, O.
    Faisal, N. H.
    Al-Anazi, N. M.
    Al-Mutairi, S.
    Toma, F. -L.
    Berger, L. -M.
    Potthoff, A.
    Goosen, M. F. A.
    WEAR, 2015, 322 : 133 - 150
  • [49] Effect of WC particle size on the abrasive wear of thermally sprayed WC-Co coatings
    Li, CJ
    Ohmori, A
    Tani, K
    MATERIALS AND MANUFACTURING PROCESSES, 1999, 14 (02) : 175 - 184
  • [50] The parameters optimization and abrasion wear mechanism of liquid fuel HVOF sprayed bimodal WC-12Co coating
    Wang, Qun
    Chen, Zhenhua
    Li, Luoxing
    Yang, Guibing
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (8-9): : 2233 - 2241