Reactive synthesis for porous Ti3AlC2 ceramics through TiH2, Al and graphite powders

被引:30
|
作者
Yang, Junsheng [1 ]
Liao, Cuijiao [1 ]
Wang, Jiefeng [1 ]
Jiang, Yao [1 ]
He, Yuehui [1 ]
机构
[1] Cent S Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
关键词
Solid state reaction; Sintering; Porosity; Carbides; Pore forming Mechanism; MICROSTRUCTURE; FABRICATION; COMPOSITES; MEMBRANE; BEHAVIOR; CARBIDE;
D O I
10.1016/j.ceramint.2013.11.136
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Porous Ti3AlC2 ceramics were fabricated by reactive synthesis. The process of fabrication involved five steps: (i) the pyrolysis of stearic acid at 450 degrees C; (ii) the decomposition of TiH2 at 700 degrees C, which leads to the conversion of TiH2 to Ti; (iii) the solid liquid chemical reaction of solid Ti and molten Al at 800-1000 degrees C, which converts the mixture to Ti-Al compounds; (iv) the newly synthesized Ti-Al compounds that react with surplus Ti and graphite to form ternary carbides and TiC at 1100-1200 degrees C; and (v) reactive synthesized ternary carbides and TiC that yield porous Ti3AlC2 at 1300 degrees C. The effects of sintering temperature and Al contents on porosity, pore size and permeability of porous Ti3AlC2 ceramics were examined. The results revealed that the porosity and permeability tended to increase with reactive sintering temperature. The pore forming mechanism accompanying phase transformation was explored in this study. (C) 2013 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:6739 / 6745
页数:7
相关论文
共 50 条
  • [21] Effects of carbon addition on combustion synthesis of Ti3AlC2 powders
    Guo, JM
    Chen, KX
    Ge, ZB
    Liu, GH
    Zhou, HP
    Ning, XS
    ACTA METALLURGICA SINICA, 2003, 39 (04) : 409 - 413
  • [22] Effects of TiAl additions on combustion synthesis of Ti3AlC2 powders
    Guo, JM
    Chen, KX
    Liu, GH
    Ge, ZB
    Zhou, HP
    Ning, XS
    RARE METAL MATERIALS AND ENGINEERING, 2004, 33 (01) : 59 - 62
  • [23] Diffusion bonding of Al2O3 with Ti through Ti + TiH2 interfaces
    Wlosinski, Wladyslaw K.
    International Journal of Materials and Product Technology, 1995, 10 (1-2): : 152 - 160
  • [24] INFLUENCE OF PRECURSORS STOICHIOMETRY ON SHS SYNTHESIS OF Ti3AlC2 POWDERS
    Chlubny, L.
    Lis, J.
    PROCESSING AND PROPERTIES OF ADVANCED CERAMICS AND COMPOSITES V, 2013, 240 : 79 - 85
  • [25] Synthesis and characterization of Ti3AlC2
    Tzenov, NV
    Barsoum, MW
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (04) : 825 - 832
  • [26] Preparation of Ti3AlC2–Al Cermets by Combined Use of SHS of Ti3AlC2 Porous Skeleton and Spontaneous Infiltration with Al and Al-Based Melts
    E. I. Latukhin
    E. R. Umerov
    A. P. Amosov
    International Journal of Self-Propagating High-Temperature Synthesis, 2023, 32 : 23 - 29
  • [27] Mechanochemical synthesis mechanism of Ti3AlC2 MAX phase from elemental powders of Ti, Al and C
    Shahin, N.
    Kazemi, Sh.
    Heidarpour, A.
    ADVANCED POWDER TECHNOLOGY, 2016, 27 (04) : 1775 - 1780
  • [28] Synthesis and Properties of Large-scale Ti3AlC2 Ceramics
    Qian Ying
    Li Chong
    Zhu Jia
    Zhu Chuncheng
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 : 241 - 243
  • [29] Fabrication of Ti3SiC2 powders using TiH2 as the source of Ti
    Yang, Jinshan
    Zhang, Xiangyu
    Wang, Zhen
    He, Ping
    Gao, Le
    Dong, Shaoming
    CERAMICS INTERNATIONAL, 2012, 38 (04) : 3509 - 3512
  • [30] The reaction between Ti3AlC2 and Cu in the synthesis process of Cu/Ti3AlC2 composites
    Peng, Chunqing
    Wang, Chang-An
    Song, Yang
    Huang, Yong
    HIGH-PERFORMANCE CERAMICS IV, PTS 1-3, 2007, 336-338 : 1374 - 1376