摘要
Porous silicon carbide (SiC) ceramics were prepared by an in situ reaction bonding process. Their thermal shock resistance to cooling was evaluated as a function of the quenching temperature, quenching cycles and specimen thickness by the water-quenching technique. It is shown that the residual strength of the quenched specimens decreases with increasing the quenching temperature and specimen thickness, but the residual strength is hardly affected by the quenching cycles. Moreover, the thermal shock resistance to heating was investigated by the instantaneous heating method. It was found that the residual strength of the heated specimens decreases gradually with increasing the heating temperature. The thermal shock damage was proposed to originate from the propagation of cracks at the necks (the bonded parts between SiC particles). However, the pores may arrest the propagating cracks and then impair this damage. Therefore, the in situ reaction bonded porous SiC ceramics exhibit excellent thermal shock resistance. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:326 / 329
页数:4
相关论文
共 50 条
  • [21] Gas permeability behavior of mullite-bonded porous silicon carbide ceramics
    Ding, Shuqiang
    Zeng, Yu-Ping
    Jiang, Dongliang
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (17) : 7171 - 7175
  • [22] Reaction mechanism of preparing porous silicon nitride/silicon carbide composite ceramics
    Zhang, W
    Wang, HJ
    Jin, ZH
    Bai, Y
    JOURNAL OF INORGANIC MATERIALS, 2005, 20 (05) : 1215 - 1221
  • [23] Novel reaction-formed joint technology for reaction bonded silicon carbide ceramics
    Zhang, Ge
    Zhao, Ru-Cheng
    Zhao, Wen-Xing
    Guangxue Jingmi Gongcheng/Optics and Precision Engineering, 2008, 16 (06): : 1037 - 1041
  • [24] THERMAL-SHOCK RESISTANCE OF POROUS SIC CERAMICS
    KOUMOTO, K
    SHIMIZU, H
    SEO, WS
    PAI, CH
    YANAGIDA, H
    BRITISH CERAMIC TRANSACTIONS AND JOURNAL, 1991, 90 (01): : 32 - 33
  • [25] Thermal shock and chemical corrosion resistance of oxide bonded porous SiC ceramics prepared by infiltration technique
    Baitalik, Sanchita
    Kayal, Nijhuma
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 781 : 289 - 301
  • [26] Oxidation resistance of reaction-formed silicon carbide ceramics
    Ogbuji, Linus U.J.T.
    Singh, M.
    Ceramic Engineering and Science Proceedings, 1995, 16 (05): : 1121 - 1126
  • [27] Electrical, thermal, and mechanical properties of porous silicon carbide ceramics with a boron carbide additive
    Kultayeva, Shynar
    Kim, Young-Wook
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2023, 20 (02) : 1114 - 1128
  • [28] Effect of oxide filler on the preparation and properties of reaction bonded silicon carbide ceramics
    Ji, XL
    Guo, BJ
    Yan, YG
    Wu, QD
    RARE METAL MATERIALS AND ENGINEERING, 2004, 33 (06) : 35 - 39
  • [29] Effect of solid loading on properties of reaction bonded silicon carbide ceramics by gelcasting
    Yuan, Zhiyong
    Zhang, Yumin
    Zhou, Yufeng
    Dong, Shanliang
    RSC ADVANCES, 2014, 4 (92) : 50386 - 50392
  • [30] Effect of carbon black addition on reaction-bonded silicon carbide ceramics
    Kim, J
    Jun, HW
    Song, H
    Lee, JH
    Lee, HW
    ADVANCED SI-BASED CERAMICS AND COMPOSITES, 2005, 287 : 189 - 193