Influence of crystallographic texture on susceptibility to stress corrosion cracking mechanism of API 5L X52 steel for sour service

被引:5
|
作者
Blanco, A. [1 ]
Hallen, J. M. [1 ]
Tang Son Nguyen [2 ,4 ]
Tu Le Manh [3 ,4 ]
机构
[1] IPN ESIQIE, Dept Ingn Met & Mat, Ciudad De Mexico 07738, Mexico
[2] PHENIKAA Univ, Fac Biotechnol Chem & Environm Engn, Hanoi 10000, Vietnam
[3] Phenikaa Univ, Fac Mat Sci & Engn, Phenikaa Inst Adv Study PIAS, Hanoi 100000, Vietnam
[4] A&A Green Phoenix Grp, Phenikaa Res & Technol Inst PRATI, 167 Hoang Ngan, Hanoi 10000, Vietnam
关键词
Near-neutral SCC; Crack initiation; API 5L steel; EBSD; Crystallographic orientation; Anisotrophy of Young's modulus; X80 PIPELINE STEEL; LOW-CARBON STEELS; BEHAVIOR; ANISOTROPY; INITIATION; HYDROGEN;
D O I
10.1016/j.engfailanal.2020.105002
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This work studies the relationship between the early stage of stress corrosion cracking (SCC) mechanism and the crystallographic texture of API 5L X52 steel for sour service in a near-neutral pH solution. Experimental evidence of the SCC initiation of X52 steel for sour service was obtained using SEM and EBSD techniques. The results show that the crack initiation mechanism behaves like a synergistic combination of chemical attack and stress concentration at pits, being the last one the driving force to crack transition. In addition, it was found from both X-ray macrotexture and EBSD microtexture measurements that the cracks initiation process depends strongly on the material's texture characteristics and the presence of the texture fiber {0 0 1}// ND in X52 steel for sour service can increase its susceptibility to SCC. In a quantitative manner, the influence of the crystallographic texture in the SCC mechanism was explained through the relationship between the initiation of SCC cracks and the predictions of the anisotropy of Young's modulus using EBSD measurements.
引用
下载
收藏
页数:15
相关论文
共 50 条
  • [41] Hydrogen induced cracking susceptibility of API 5L X70 pipeline steel in relation to microstructure and crystallographic texture developed after different thermomechanical treatments
    Ohaeri, Enyinnaya
    Szpunar, Jerzy
    Fazeli, Fateh
    Arafin, Muhammad
    MATERIALS CHARACTERIZATION, 2018, 145 : 142 - 156
  • [42] Corrosion Inhibition of Compounds Derived from Dihydropyrimidines (DMPH) in API 5L X52 Steel Immerse in 1M HCl
    Espinoza-Vazquez, A.
    Rodriguez Gomez, F. J.
    Lopez Alvares, I. G.
    Angeles Beltran, D.
    Negron Silva, G. E.
    Palomar Pardave, M.
    XXXII NATIONAL CONGRESS OF THE MEXICAN SOCIETY OF ELECTROCHEMISTRY/10TH MEETING OF THE ECS MEXICAN SECTION, 2018, 84 (01): : 189 - 194
  • [43] STUDY OF THE SUSCEPTIBILITY OF API 5L X80 GIRTH WELDS TO SULFIDE STRESS CORROSION CRACKING AND HYDROGEN EMBRITTLEMENT
    Ballesteros, Adriana Forero
    da Cunha Ponciano, Jose A.
    Bott, Ivani de S.
    PROCEEDINGS OF THE ASME INTERNATIONAL PIPELINE CONFERENCE 2010, VOL 1, 2010, : 375 - 380
  • [44] Charpy impact toughness in all directions with respect to the rolling direction of API 5L X52 pipeline steel
    Teran, G.
    Capula-Colindres, S.
    Chavez, F.
    Velazquez, J. C.
    Torres-Santillan, E.
    Angeles-Herrera, D.
    Goiz, O.
    MRS ADVANCES, 2022, 7 (33) : 1022 - 1027
  • [45] Electrochemical behaviour of API 5L X52 Steel Samples Immersed in Sulphate Aqueous Solutions with Different pH
    Morales Gil, Perla
    Julien, Baptiste
    Palomar-Pardave, Manuel
    Montes de Oca-Yemha, Maria Guadalupe
    Teresa Ramirez-Silva, Maria
    Romero-Romo, Mario
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2018, 13 (04): : 3297 - 3308
  • [46] Charpy Impact Toughness and Transition Temperature for API 5L X52 Seamless Pipeline
    Capula-Colindres, S.
    Teran, G.
    Velazquez, J. C.
    Angeles-Herrera, D.
    Torres-Santillan, E.
    STRENGTH OF MATERIALS, 2024, 56 (01) : 136 - 143
  • [47] Charpy impact toughness in all directions with respect to the rolling direction of API 5L X52 pipeline steel
    G. Terán
    S. Capula-Colindres
    F. Chávez
    J. C. Velázquez
    E. Torres-Santillan
    D. Angeles-Herrera
    O. Goiz
    MRS Advances, 2022, 7 : 1022 - 1027
  • [48] Evaluation of the Mode I Stress Intensity Factor calculated by the Finite Element Method for CT Specimen of API 5L X52 Steel
    Ousfya, S.
    Taouil, R.
    Moustabchir, H.
    Touzani, M.
    ICCWCS'17: PROCEEDINGS OF THE 2ND INTERNATIONAL CONFERENCE ON COMPUTING AND WIRELESS COMMUNICATION SYSTEMS, 2017,
  • [49] Assessment of the effects of acetic acid and turbulent flow conditions on the corrosion of API 5L X52 steel in aqueous CO2 solutions
    Elena Olvera-Martinez, Maria
    Mendoza-Flores, Juan
    Javier Rodriguez-Gomez, Francisco
    Duran-Romero, Ruben
    Genesca, Juan
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (03): : 376 - 385
  • [50] Influence of Thermomechanically Controlled Processing on Microstructure and HydrogenInduced Cracking Susceptibility of API 5L X70 Pipeline Steel
    Ohaeri, Enyinnaya
    Omale, Joseph
    Tiamiyu, Ahmed
    Rahman, K. M. Mostafijur
    Szpunar, Jerzy
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (09) : 4533 - 4547