Calibrating Johnson's formula for applying DCPD method to an axial through-wall crack in a pipe

被引:4
|
作者
Sun, Dexin [1 ]
Li, He [2 ]
Feng, Hui [2 ]
Li, Yong [1 ]
Li, Qun [1 ]
机构
[1] Xi An Jiao Tong Univ, State Key Lab Strength & Vibrat Mech Struct, Sch Aerosp, Xian 710049, Peoples R China
[2] CNPC Tubular Goods Res Inst, Xian 710077, Peoples R China
基金
中国国家自然科学基金;
关键词
The calibrated Johnson's formula; Direct current potential drop method; Calibration curve; Pipe sample; Axial through-wall crack;
D O I
10.1016/j.engfracmech.2020.107461
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
Direct current potential drop (DCPD) method is widely employed in the determination of crack length in conductive materials. It is based on the change of structure potential drop caused by the variation of the electrical resistance under a steady direct current. The accuracy of DCPD method depends on the calibration curve which describes the relationship between crack length and potential drop. Generally, the calibration curve for the crack in a plate sample is given by Johnson's formula analytically. However, the traditional Johnson's formula is only applicable to a center-cracked plate but not to a cracked pipe. In this paper, Johnson's formula has to be calibrated to estimate the length of a through-the-thickness crack in a pipe. Considering the geometrical difference between a pipe sample and a plate sample, the calibrated Johnson's formula is established based on the existence of parallel circuit in a pipe and the proposed unique reference sample. The calibration curve between axial through-wall crack length and potential drop is carried out by the calibrated Johnson's formula. The calibrated formula has been verified for the axial through-wall crack in a pipe sample by numerical and experimental approaches. Compared with the traditional Johnson's formula, the results illustrate that the present calibrated formula is successful to estimate the crack length in a pipe. This paper extends the applicability of the original formulation of Johnson's formula to cracked pipes.
引用
收藏
页数:10
相关论文
共 50 条
  • [44] Research on Test and Theoretical Analysis Methods on Stability of LBB Circumferential Through-Wall Crack in Austenitic Stainless Steel Pipe under Dynamic Load
    He F.
    Yao D.
    Wang X.
    Li Y.
    Bai X.
    Xiong F.
    Hedongli Gongcheng/Nuclear Power Engineering, 2022, 43 (02): : 133 - 137
  • [45] Prediction of limit pressure in axial through-wall cracked X80 pipeline based on critical crack-tip opening angle
    Cao Y.
    Zhen Y.
    He Y.
    Zhang S.
    Sun Y.
    Yi H.
    Liu F.
    Zhongguo Shiyou Daxue Xuebao (Ziran Kexue Ban)/Journal of China University of Petroleum (Edition of Natural Science), 2017, 41 (02): : 139 - 146
  • [46] Elastic T-stress and I-II mixed mode stress intensity factors for a through-wall crack in an inner-pressured pipe
    Yu, Peishi
    Wang, Quan
    Zhang, Chaofeng
    Zhao, Junhua
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2018, 159 : 67 - 72
  • [47] A method of J testing based on crack opening displacement for circumferential through-wall cracked pipes under combined tension and bending
    Huh, NS
    Stumpfrock, L
    Roos, E
    Kim, YJ
    Kim, YJ
    ADVANCES IN SAFETY AND STRUCTURAL INTEGRITY 2005, 2006, 110 : 63 - 69
  • [50] A Method for Reducing Timing Jitter's Impact in Through-Wall Human Detection by Ultra-Wideband Impulse Radar
    Shi, Cheng
    Ni, Zhi-Kang
    Pan, Jun
    Zheng, Zhijie
    Ye, Shengbo
    Fang, Guangyou
    REMOTE SENSING, 2021, 13 (18)